Study on Preparation of Ti2AlNb by Spark Plasma Sintering and Its Room Temperature Mechanical Properties AITranslate

School of Materials Engineering,Xi an Polytechnic University;School of Materials Engineering,Xi an Polytechnic University;School of Materials Engineering,Xi an Polytechnic University;School of Materials Engineering,Xi an Polytechnic University;School of Materials Engineering,Xi an Polytechnic University;School of Materials Engineering,Xi an Polytechnic University;School of Materials Engineering,Xi an Polytechnic University;School of Materials Engineering,Xi an Polytechnic University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ti2AlNb alloy was prepared using elemental powders of Ti,Al and Nb through spark plasma sintering(SPS).The microstructure and phase composition of the alloy were characterized using scanning electron microscope(SEM)and X-ray diffractometer(XRD),and the room temperature mechanical properties of the Ti2AlNb alloy were also tested.The results show that the Ti2AlNb alloy prepared by spark plasma sintering has uniform grain distribution and superior room temperature mechanical properties,with a tensile strength of 254 MPa.Compared with traditional sintering methods,spark plasma sintering offers advantages such as rapid heating and high densification of sintered samples.

KeyWords AITranslate

Ti2AlNb spark plasma sintering room temperature mechanical property tensile strength

1罗媛媛,张菁丽,赵圣泽,郭荻子,苏航标,毛小南.Ti-25Al-15Nb-1Mo合金的高温变形行为研究[J].稀有金属与硬质合金,2019,47(6):59-63. 被引量:3

2徐磊,姚利盼,卢正冠,吴杰,杨锐.粉末冶金Ti2AlNb合金研究进展[J].航空制造技术,2019,62(22):14-20. 被引量:3

3李博,王俊勃,刘江南,窦博,黄晟,王振楠,梅金娜.V元素掺杂对粉末冶金Ti_(2)AlNb合金显微组织的影响[J].钛工业进展,2022,39(2):24-28. 被引量:1

1张光磊,杜亚琼,胡美华,胡前库,周爱国.新型MAX相陶瓷Mo_(2)Ga_(2)C的放电等离子烧结[J].现代技术陶瓷,2023,44(5):481-489.

2蔡森,王晓巍,焦清洋,王漪琼,姜洪淼.不锈钢铸件热等静压工艺研究[J].铸造,2023,72(10):1288-1290.

3刘坤定,杨斌,王爱琴,信要龙.烧结温度对放电等离子烧结(SPS)制备氧化石墨烯/2024Al复合材料的微观组织和性能影响[J].粉末冶金工业,2023,33(5):25-30.

4郭克星.钛合金的制备和应用[J].热处理,2023,38(5):8-12.

5刘胜,刘文进,满延进,周国相,杨治华,贾德昌.氮化硅陶瓷材料高温抗热震性能及其衰减规律研究[J].现代技术陶瓷,2023,44(5):451-460.

6谭永生.电厂旋风分离器受热面管泄漏原因分析[J].失效分析与预防,2023,18(5):346-350.

7赵志朋,胡浩,宋克兴,程浩艳,代明伟,郁宁宁,卢伟伟,冯庆,杨祥魁.PEG和MPS对电解铜箔结构和力学性能的影响[J].电镀与涂饰,2023,42(21):54-64.

8曹宇,胡继林,陈占军,刘哲皓,陈都,彭秧锡.不同粘结剂与烧结温度对Al_(2)O_(3)陶瓷力学性能和显微结构的影响[J].粉末冶金工业,2023,33(5):119-124.

9王垂磊,侯立敏,郇宇.(1-x)KNNS-xBFANZ无铅压电陶瓷的结构与性能的研究[J].现代技术陶瓷,2023,44(5):490-496.

10宋奎晶,季雨凯,韦勇,丁子恒,张铭雨,刘鑫泉,钟志宏,方坤.焊接温度对5A06铝合金SPS钎焊接头组织和性能的影响[J].稀有金属材料与工程,2023,52(10):3461-3469.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料]

Citation Information:

Ti2AlNb alloy was prepared using elemental powders of Ti,Al and Nb through spark plasma sintering(SPS).The microstructure and phase composition of the alloy were characterized using scanning electron microscope(SEM)and X-ray diffractometer(XRD),and the room temperature mechanical properties of the Ti2AlNb alloy were also tested.The results show that the Ti2AlNb alloy prepared by spark plasma sintering has uniform grain distribution and superior room temperature mechanical properties,with a tensile strength of 254 MPa.Compared with traditional sintering methods,spark plasma sintering offers advantages such as rapid heating and high densification of sintered samples.

quote

GB/T 7714-2015 [1] DOU Bo, LIU Song-tao, JIANG Feng-yang, et al. Study on Preparation of Ti2AlNb by Spark Plasma Sintering and Its Room Temperature Mechanical Properties[J]. Rare Metals and Cemented Carbides, 2023(5): 73-77.
MLA [1] DOU Bo, et al., "Study on Preparation of Ti2AlNb by Spark Plasma Sintering and Its Room Temperature Mechanical Properties." Rare Metals and Cemented Carbides, no. 5, 2023, pp. 73-77.
APA [1] DOU Bo, LIU Song-tao, JIANG Feng-yang, SI Fang, WU Tian-dong, WANG Jun-bo, LIU Jiang-nan, & DONG Xi. (2023). Study on Preparation of Ti2AlNb by Spark Plasma Sintering and Its Room Temperature Mechanical Properties. Rare Metals and Cemented Carbides(5), 73-77.
IEEE [1] DOU Bo, LIU Song-tao, JIANG Feng-yang, SI Fang, WU Tian-dong, WANG Jun-bo, LIU Jiang-nan, and DONG Xi, "Study on Preparation of Ti2AlNb by Spark Plasma Sintering and Its Room Temperature Mechanical Properties," Rare Metals and Cemented Carbides, no. 5, pp. 73-77, 2023. keywords: {TiAlNb;spark plasma sintering;room temperature mechanical property;tensile strength}