Performance Comparison of P204/P507 for Extraction Separation of Vanadium and Iron in Sulfuric Acid System AITranslate
Abstract AITranslate
Iron ions and other impurities existing in the leaching solution of vanadium-containing minerals seriously affect the separation and enrichment of vanadium.In this paper,P204 and P507 were used as extractants to extract vanadium from the simulated leaching solution containing V(Ⅳ)and Fe(Ⅱ)by solvent extraction.The effects of pH value,vanadium concentration and iron concentration on the vanadium extraction effect and vanadium-iron separation effect were investigated.At the same time,the structural changes of the organic phase before and after extraction were also analyzed.The results show that the effect of pH on vanadium extraction and vanadium-iron separation is significant.P204 is more suitable for the vanadium-iron separation under strongly acidic conditions(pH1),while P507 is more appropriate under sub-strongly acidic conditions(pH=2).When the pH value is 2,the concentration of V4+is 0.07 g/L,the concentration of Fe2+is 14 g/L,the O/A ratio is 1.5,the temperature is 25°C,and the stirring time is 10 min,the extraction rate of vanadium by P507 reaches above 99%,and the extraction rate of iron is below 5%,showing a good separation effect of vanadium and iron.The infrared spectrum shows that the extraction of vanadium by P204 and P507 is a cation exchange process,which is presented by the replacement of H~+with VO2+in P—OH functional group of the extractant.
KeyWords AITranslate
1徐正震,梁精龙,李慧,郭佳明.含钒废弃物中钒的回收研究现状及展望[J].矿产综合利用,2020(3):8-13. 被引量:13
2刘月菊,孟昭阳,阎成友.无盐焙烧-稀酸浸出提钒工艺研究[J].化工管理,2022(5):138-140. 被引量:1
3张立萍,吕灵灵,孔慧,叶红,祝汉国.控制萃取平衡时间选择性分离回收FCC废催化剂酸浸液中的钒[J].石油炼制与化工,2021,52(8):96-101. 被引量:2
4彭雪枫,张洋,郑诗礼,范兵强,王晓健,乔珊,刘丰强.溶液中钒铬分离方法的研究进展[J].中国有色金属学报,2019,29(11):2620-2634. 被引量:4
5张一敏,包申旭.含钒浸出液净化富集技术现状及前景[J].金属矿山,2016,45(7):64-70. 被引量:9
6贾蓝波,王玲,郭紫璇,熊雨婷,夏亮亮,王龙,聂轶苗,刘淑贤.含钒溶液萃取分离富集钒的研究进展[J].中国有色金属学报,2022,32(11):3489-3504. 被引量:1
7熊璞,张一敏,黄晶,包申旭,杨晓,谌纯.P507-N235混合萃取剂分离石煤酸浸液中钒与铁[J].有色金属:冶炼部分,2016(10):36-39. 被引量:6
8冯雪茹,吕国志,张延安,张莹,赵秋月,刘述平.P204萃取硫酸体系中V(Ⅳ)、Fe(Ⅲ)的分离性能研究[J].钢铁钒钛,2017,38(2):23-29. 被引量:13
9李金辉,徐志峰,高岩,剧智华,陈志峰,李德顺.优先络合-水解沉淀法分离铬铁机理[J].中国有色金属学报,2019,29(7):1528-1535. 被引量:6
10张莹,张廷安,吕国志,刘卓林.钒渣无焙烧浸出液中钒铁萃取分离[J].东北大学学报:自然科学版,2015,36(10):1445-1448. 被引量:7
1邓永贵.硫酸体系压力浸出反应釜衬里层材料的选择[J].科学技术创新,2023(18):39-42.
2王韶川,高艳芳.硫酸体系中反萃取Ni(Ⅱ)的动力学研究[J].湿法冶金,2023,42(3):247-251.
3侯静,徐众,吴恩辉,李军,蒋燕,黄平.双碳背景下提钒弃渣制备集热涂层及其性能[J].攀枝花科技与信息,2023,48(2):37-41.
4付玉洁,于海龙.纤维素酶的低共熔溶剂双水相萃取研究[J].青岛科技大学学报:自然科学版,2023,44(3):23-29.
5赖永传,杨鑫龙,孙建之,尚鹤,莫晓兰,温建康.石煤含氟酸浸液中V(Ⅴ)-Fe(Ⅲ)-F-H_(2)O系钒铁分离热力学研究[J].中南大学学报:自然科学版,2023,54(5):1703-1712.
6陶媛媛,叶国华,胡渝杰,唐悦.叔胺萃取剂提钒的现状与趋势展望[J].矿产综合利用,2023(3):57-62.
7刘洋,高建树,李静静,邵磊山,曾昕.溶剂萃取后处理方法制备汽车用低气味改性聚丙烯[J].塑料工业,2023,51(6):52-57.
8林颖悦,张玉,陈家畅.司法毒物鉴定中SPME技术的应用[J].法制博览(名家讲坛、经典杂文),2022(31):100-102.
9王吉,向滢,彭强,杨光茜.重量法测定烧结焊剂中石英[J].冶金分析,2023,43(6):55-61.
10王亚,肖霞霞,杨云,黄博闻,陈小龙,孙星,程金金,葛静,宋立晓,余向阳.溶剂萃取-气相色谱-三重四极杆串联质谱法测定水体和土壤中6种邻苯二甲酸酯[J].分析科学学报,2023,39(3):287-294.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]
Citation Information:
Iron ions and other impurities existing in the leaching solution of vanadium-containing minerals seriously affect the separation and enrichment of vanadium.In this paper,P204 and P507 were used as extractants to extract vanadium from the simulated leaching solution containing V(Ⅳ)and Fe(Ⅱ)by solvent extraction.The effects of pH value,vanadium concentration and iron concentration on the vanadium extraction effect and vanadium-iron separation effect were investigated.At the same time,the structural changes of the organic phase before and after extraction were also analyzed.The results show that the effect of pH on vanadium extraction and vanadium-iron separation is significant.P204 is more suitable for the vanadium-iron separation under strongly acidic conditions(pH1),while P507 is more appropriate under sub-strongly acidic conditions(pH=2).When the pH value is 2,the concentration of V4+is 0.07 g/L,the concentration of Fe2+is 14 g/L,the O/A ratio is 1.5,the temperature is 25°C,and the stirring time is 10 min,the extraction rate of vanadium by P507 reaches above 99%,and the extraction rate of iron is below 5%,showing a good separation effect of vanadium and iron.The infrared spectrum shows that the extraction of vanadium by P204 and P507 is a cation exchange process,which is presented by the replacement of H~+with VO2+in P—OH functional group of the extractant.
quote
| GB/T 7714-2015 | [1] MA Chen, ZHU Xiao-bo, LI Wang, et al. Performance Comparison of P204/P507 for Extraction Separation of Vanadium and Iron in Sulfuric Acid System[J]. Rare Metals and Cemented Carbides, 2023(3): 18-22. |
| MLA | [1] MA Chen, et al., "Performance Comparison of P204/P507 for Extraction Separation of Vanadium and Iron in Sulfuric Acid System." Rare Metals and Cemented Carbides, no. 3, 2023, pp. 18-22. |
| APA | [1] MA Chen, ZHU Xiao-bo, LI Wang, & LIU Yue. (2023). Performance Comparison of P204/P507 for Extraction Separation of Vanadium and Iron in Sulfuric Acid System. Rare Metals and Cemented Carbides(3), 18-22. |
| IEEE | [1] MA Chen, ZHU Xiao-bo, LI Wang, and LIU Yue, "Performance Comparison of P204/P507 for Extraction Separation of Vanadium and Iron in Sulfuric Acid System," Rare Metals and Cemented Carbides, no. 3, pp. 18-22, 2023. keywords: {vanadium-iron separation;solvent extraction;P204;P507;sulfuric acid system;extraction mechanism;infrared spectrum} |