Progress and Analysis of Preparation Process of Nuclear Grade Zirconium Sponge AITranslate

Xi′an Western Energy Material Technologies Co.,Ltd.;Xi′an Western Energy Material Technologies Co.,Ltd.;Xi′an Western Energy Material Technologies Co.,Ltd.;Xi′an Western Energy Material Technologies Co.,Ltd.;Xi′an Western Energy Material Technologies Co.,Ltd.;Xi′an Western Energy Material Technologies Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

With the restart of domestic nuclear power in recent years,nuclear grade zirconium sponge has been widely emphasized as the primary raw material for nuclear grade zirconium alloy in the industry,accelerating the development of the domestic nuclear grade zirconium sponge industry.This study briefly reviews the research progress of the nuclear grade zirconium sponge in China,discusses the common industrial preparation processes of the nuclear grade zirconium sponge,summarizes the advantages,disadvantages,and applications of the main production processes,and analyzes the development trend of the nuclear grade zirconium sponge preparation process in the future from a technical perspective.Some suggestions on cost reduction,efficiency increase,and environmental protection are also put forward.

KeyWords AITranslate

nuclear grade zirconium sponge zirconium tetrachloride purification magnesium thermal reduction vacuum distillation development trend

1逯冉.我国锆工业发展浅析[J].中国金属通报,2019,0(12):3-3. 被引量:1

2李献军.海绵锆的生产工艺技术及技术标准的发展[J].钛工业进展,2009,26(3):17-21. 被引量:8

3魏占海,王力军,熊炳昆.核电发展为我国锆铪产业带来发展机遇[J].稀有金属快报,2007,26(1):10-13. 被引量:15

4贾豫婕,林希衡,邹小伟,韩卫忠.锆合金的研发历史、现状及发展趋势[J].中国材料进展,2022,41(5):354-370. 被引量:6

5袁改焕,李恒羽,王德华.锆材在核电站的应用及前景[J].稀有金属快报,2007,26(1):14-16. 被引量:39

6解西京,柳松,王敬欣.溶剂萃取分离锆和铪研究进展[J].稀有金属,2009(3):426-433. 被引量:16

7刘敏娉,丁燕,张泽光,蔡挺.锆与铪分离技术的研究现状及应用前景[J].广东有色金属学报,2001,11(2):115-119. 被引量:15

8李攀红,徐志高,池汝安,赵骏,王力军,徐源来.湿法分离锆铪的研究进展[J].稀有金属,2016,40(5):499-508. 被引量:8

9罗方承,陈忠锡,孙小龙,谌美玲.MIBK双溶剂萃取法制备原子能级氧化锆和氧化铪的工艺设计[J].稀有金属快报,2007,26(1):89-92. 被引量:13

10林振汉.用甲基异丁基酮萃取分离锆铪的工艺评价[J].稀有金属快报,2007,26(1):93-96. 被引量:15

1陈泽宇,刘亮,刘兰波,柴艳红,李源.太赫兹极化栅网制造工艺进展探讨[J].中国科技纵横,2023(7):66-68.

2张云生.污油泥处理工艺现状及进展[J].中文科技期刊数据库(全文版)工程技术,2021(2):0166-0166.

3管先才,来海林.银杏叶中有效成分的提取工艺进展[J].中国科技期刊数据库 医药,2023(5):0167-0170.

4李吉帆,盛卓,李开华,孙浩山,张小辉,李冬勤,李亮,周杰,陈秀敏.镁热法生产海绵钛过程反应器温度场模拟研究[J].钢铁钒钛,2023,44(2):20-27.

5夏浩涛,石宇,赖文劲,罗文,黄金.锂离子电池微米级三维多孔硅负极材料合成及性能研究[J].材料研究与应用,2023,17(3):567-571.

6阮晶晶,刘福园,李珅珅,高桂红,刘艳侠.碳还原法制备棒状硅基材料及其在锂浆料电池中的应用[J].储能科学与技术,2023,12(4):1051-1058.

7叶朝侯,傅华伟.异氰酸酯的清洁生产工艺进展[J].天津化工,2023,37(2):59-61.

8于剑昆,陈仁树.国内CHPPO工业化技术进展(待续)[J].化学推进剂与高分子材料,2023,21(1):7-24.

9杨浩,王方军,李采,吴畏.镍基高温合金的熔炼工艺研究进展[J].特殊钢,2023,44(3):1-9. 被引量:2

10史石磊.甜菊糖苷提取工艺进展[J].食品工业,2023,44(6):157-159.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.4[冶金工程—有色金属冶金]

Citation Information:

With the restart of domestic nuclear power in recent years,nuclear grade zirconium sponge has been widely emphasized as the primary raw material for nuclear grade zirconium alloy in the industry,accelerating the development of the domestic nuclear grade zirconium sponge industry.This study briefly reviews the research progress of the nuclear grade zirconium sponge in China,discusses the common industrial preparation processes of the nuclear grade zirconium sponge,summarizes the advantages,disadvantages,and applications of the main production processes,and analyzes the development trend of the nuclear grade zirconium sponge preparation process in the future from a technical perspective.Some suggestions on cost reduction,efficiency increase,and environmental protection are also put forward.

quote

GB/T 7714-2015 [1] YAN Bao-hui, CUI Chun-juan, XIAO Ying, et al. Progress and Analysis of Preparation Process of Nuclear Grade Zirconium Sponge[J]. Rare Metals and Cemented Carbides, 2023(3): 23-29.
MLA [1] YAN Bao-hui, et al., "Progress and Analysis of Preparation Process of Nuclear Grade Zirconium Sponge." Rare Metals and Cemented Carbides, no. 3, 2023, pp. 23-29.
APA [1] YAN Bao-hui, CUI Chun-juan, XIAO Ying, TIAN Feng, LIU Hai-ming, & ZHOU Jun. (2023). Progress and Analysis of Preparation Process of Nuclear Grade Zirconium Sponge. Rare Metals and Cemented Carbides(3), 23-29.
IEEE [1] YAN Bao-hui, CUI Chun-juan, XIAO Ying, TIAN Feng, LIU Hai-ming, and ZHOU Jun, "Progress and Analysis of Preparation Process of Nuclear Grade Zirconium Sponge," Rare Metals and Cemented Carbides, no. 3, pp. 23-29, 2023. keywords: {nuclear grade zirconium sponge;zirconium tetrachloride;purification;magnesium thermal reduction;vacuum distillation;development trend}