Molecularly Imprinted Polymer with High Capacity and Selectivity for Separation of Bovine Serum Albumin AITranslate
Abstract AITranslate
A cost-effective but simple method for the separation of bovine serum albumin (BSA) from complex biological fluids is still lacking. Here using N-isopropylacrylamide as the main monomer and dimethylaminoethyl methacrylate, methacrylic acid, and acrylamide as functional monomers, a BSA-imprinted polymer was synthesized. To overcome the two major obstacles of common protein-imprinted polymers, i.e., difficult template removal and low imprinting efficiency, an oligo(glutamic acid)-based peptide cross-linker with the same vinyl group on both ends was designed and used as cross-linker in the synthesis of the polymers. The introduction of the peptide segments, which are capable of undergoing a pH-triggered reversible and precise helix–coil transition, into the polymers makes the imprint cavities shape-memorable. Therefore, complete removal of the template BSA under mild conditions, that is, at physiological pH, ionic strength, and temperature, was achieved. More importantly, an adsorption capacity of 607 mg/g and an imprinting factor of 6.0, both of which are not only higher than the molecularly imprinted polymer (MIP) cross-linked with the commonly used cross-linker N,N′-methylenebis(acrylamide), but also higher than most BSA MIPs reported previously in the literature, were obtained, indicating a high affinity of the MIP to the template BSA. The BSA MIP also showed a high selectivity and could be used repeatedly. Using the BSA MIP as the adsorbent, BSA was extracted from fetal bovine serum selectively and efficiently.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01370
Chinese Library Classification Number:
Citation Information:
A cost-effective but simple method for the separation of bovine serum albumin (BSA) from complex biological fluids is still lacking. Here using N-isopropylacrylamide as the main monomer and dimethylaminoethyl methacrylate, methacrylic acid, and acrylamide as functional monomers, a BSA-imprinted polymer was synthesized. To overcome the two major obstacles of common protein-imprinted polymers, i.e., difficult template removal and low imprinting efficiency, an oligo(glutamic acid)-based peptide cross-linker with the same vinyl group on both ends was designed and used as cross-linker in the synthesis of the polymers. The introduction of the peptide segments, which are capable of undergoing a pH-triggered reversible and precise helix–coil transition, into the polymers makes the imprint cavities shape-memorable. Therefore, complete removal of the template BSA under mild conditions, that is, at physiological pH, ionic strength, and temperature, was achieved. More importantly, an adsorption capacity of 607 mg/g and an imprinting factor of 6.0, both of which are not only higher than the molecularly imprinted polymer (MIP) cross-linked with the commonly used cross-linker N,N′-methylenebis(acrylamide), but also higher than most BSA MIPs reported previously in the literature, were obtained, indicating a high affinity of the MIP to the template BSA. The BSA MIP also showed a high selectivity and could be used repeatedly. Using the BSA MIP as the adsorbent, BSA was extracted from fetal bovine serum selectively and efficiently.
quote
| GB/T 7714-2015 | [1] Meiyu Zhang, Yafei Wang, Keling Hu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01370. |
| MLA | [1] Meiyu Zhang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01370. |
| APA | [1] Meiyu Zhang, Yafei Wang, Keling Hu, Yaojing Zhang, Shun Liu, Zhuo Zhao, Lei Zou, & Yongjun Zhang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01370 |
| IEEE | [1] Meiyu Zhang, Yafei Wang, Keling Hu, Yaojing Zhang, Shun Liu, Zhuo Zhao, Lei Zou, and Yongjun Zhang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01370. keywords: {molecularly imprinted polymers;peptide;helix−coil transition;separation;bovine serum albumin} |