daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Hydrophobic PEGylation of Chitosan: A Graft Copolymer Approach toward Developing Nontoxic Antimicrobial Chitosan AITranslate

Indian Institute of Technology Patna; National Institute of Technology Durgapur; Indian Institute of Technology Patna; National Institute of Technology Durgapur; National Institute of Technology Durgapur; Indian Institute of Technology Patna
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Though chitosan-based antimicrobial polymers have been well-known for a long time, selectivity of such derivatives remains always an issue, especially selective bacteria killing using chitosan-derived antimicrobials are far less addressed to the best of our knowledge. In this context, a series of graft copolymers were prepared via chemoselective grafting of acrylate telechelic hydrophobic PEGs onto a chitosan backbone at the C2–NH2 position. The graft copolymers show superior and selective antimicrobial efficacy (with respect to both types of bacteria and RBC) with low toxicity. Based on grafting density, selective bacteria killing was noted between Escherichia coli and Staphylococcus aureus. In the current study, MIC (S. aureus)/ MIC (E. coli) for graft copolymers with a lesser grafting density (CHT-g-OPEG10) is calculated as 1.68, and for graft copolymers with a higher grafting density (CHT-g-OPEG30) MIC (E. coli)/MIC (S. aureus) is reported as 2.14, indicating that CHT-g-OPEG10 may be used preferentially for killing E. coli (with a much lesser effect for S. aureus); whereas CHT-g-OPEG30 may be utilized for the preferential killing of S. aureus (with a much lesser effect on E. coli).

KeyWords AITranslate

graft copolymers antimicrobial polymers chitosan polyethylene glycols (PEG) azaMichael reactions
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01351

Chinese Library Classification Number:

Citation Information:

Though chitosan-based antimicrobial polymers have been well-known for a long time, selectivity of such derivatives remains always an issue, especially selective bacteria killing using chitosan-derived antimicrobials are far less addressed to the best of our knowledge. In this context, a series of graft copolymers were prepared via chemoselective grafting of acrylate telechelic hydrophobic PEGs onto a chitosan backbone at the C2–NH2 position. The graft copolymers show superior and selective antimicrobial efficacy (with respect to both types of bacteria and RBC) with low toxicity. Based on grafting density, selective bacteria killing was noted between Escherichia coli and Staphylococcus aureus. In the current study, MIC (S. aureus)/ MIC (E. coli) for graft copolymers with a lesser grafting density (CHT-g-OPEG10) is calculated as 1.68, and for graft copolymers with a higher grafting density (CHT-g-OPEG30) MIC (E. coli)/MIC (S. aureus) is reported as 2.14, indicating that CHT-g-OPEG10 may be used preferentially for killing E. coli (with a much lesser effect for S. aureus); whereas CHT-g-OPEG30 may be utilized for the preferential killing of S. aureus (with a much lesser effect on E. coli).

quote

GB/T 7714-2015 [1] Jyoti Devi Katiyar, Arpita Halder, Mohd. Avais, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01351.
MLA [1] Jyoti Devi Katiyar, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01351.
APA [1] Jyoti Devi Katiyar, Arpita Halder, Mohd. Avais, Hiya Aidasani, Oindrilla Mukherjee, & Subrata Chattopadhyay. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01351
IEEE [1] Jyoti Devi Katiyar, Arpita Halder, Mohd. Avais, Hiya Aidasani, Oindrilla Mukherjee, and Subrata Chattopadhyay, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01351. keywords: {graft copolymers;antimicrobial polymers;chitosan;polyethylene glycols (PEG);azaMichael reactions}