Study of thermodynamic properties of cerium dioxide under high pressures AITranslate

Hanoi National University of Education;Hanoi National University of Education;Tokyo Institute of Technology
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The statistical moment method (SMM) is used to study the thermodynamic quantities of the cubic fluorite cerium dioxide talking into account the anharmonicity effects of the lattice vibrations and hydrostatic pressures. The thermodynamic quantities of CeO 2 are calculated as a function of the pressure. The SMM calculations are performed by using the Buckingham potential for the cerium dioxide. The effects of the three different potential parameter sets of the Buckingham potential on some thermodynamic properties for CeO 2 are also investigated.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2010.03.003

Chinese Library Classification Number:

Citation Information:

The statistical moment method (SMM) is used to study the thermodynamic quantities of the cubic fluorite cerium dioxide talking into account the anharmonicity effects of the lattice vibrations and hydrostatic pressures. The thermodynamic quantities of CeO 2 are calculated as a function of the pressure. The SMM calculations are performed by using the Buckingham potential for the cerium dioxide. The effects of the three different potential parameter sets of the Buckingham potential on some thermodynamic properties for CeO 2 are also investigated.

quote

GB/T 7714-2015 [1] Vu Van Hung, Le Thi Mai Thanh, K. MasudaJindo. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.03.003.
MLA [1] Vu Van Hung, et al., Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.03.003.
APA [1] Vu Van Hung, Le Thi Mai Thanh, & K. MasudaJindo. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.03.003
IEEE [1] Vu Van Hung, Le Thi Mai Thanh, and K. MasudaJindo, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.03.003.