Microstructure and Macrohardness of Ti2AlNb-Based Alloy with Different Cooling Modes AITranslate

1.Western Titanium Technologies Co.,Ltd.,Xi'an 710201,China
2.High Temperature Materials Research Institute,Central Iron and Steel Research Institute,Beijing 100081,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

With the rapid advancement of aerospace propulsion systems, the demand for high-performance materials capable of enduring extreme thermal and mechanical stresses in aeroengine components has reached unprecedented levels. Ti-22Al-25Nb (atom fraction) alloy, an orthorhombic titanium aluminide (Ti2AlNb-based system), has emerged as a leading candidate for next-generation high-temperature structural applications due to its exceptional combination of low density, high specific strength, superior creep resistance, and remarkable stability under prolonged thermal exposure. This alloy system primarily consists of three distinct phases:the ordered body-centered cubic (B2) phase, the hexagonal close-packed α2 phase (derived from Ti3Al), and the orthorhombic (O) phase. However, the intricate interplay between phase transformations and microstructural evolution during thermal processing poses significant challenges in optimizing its mechanical performance. To address this, the present study systematically investigated the phase transformation and microstructure evolution of Ti-22Al-25Nb alloy under varying cooling conditions, with a focus on elucidating the nucleation mechanisms, growth behavior, and crystallographic orientation relationships of O phase with the parent phase. Specimens were subjected to controlled heat treatments at two critical temperatures (1060 and 980 ℃) followed by cooling at rates ranging from rapid quenching (water and oil) to slow furnace cooling. Phase identification and structural characterization were performed using X-ray diffraction (XRD) with Cu-Kα radiation. Microstructural features were analyzed via optical microscope (OM) and scanning electron microscope (SEM). Crystallographic orientation relationships between the precipitated O phase and the parent phase (B2 matrix or α2 particles) during the cooling process were resolved using electron backscatter diffraction (EBSD). Macrohardness of the alloys were tested by using a macrohardness tester. The results indicated that the morphology of the precipitated O phase was significantly influenced by the cooling mode. When the alloy was cooled from a higher temperature (1060 ℃), numerous acicular O phase precipitated formed in B2 matrix, along B2 grain boundaries, and around α2 particles. The specimen cooled at higher rates, such as water quenching and oil quenching, showed retention of the high-temperature B2 phase, in which B2 phase was an ordered cubic phase, due to the window for phase transformation to form new α2 phase was narrow and rapid cooling suppressed elemental diffusion, particularly of Nb elements. Moreover, the high niobium content in Ti-22Al-25Nb alloy decelerated diffusion processes and led to sluggish phase transformations. With the decrease of the cooling rate, such as air cooling and forced air cooling, the flocculent O phases consisting of numerous fine needle-like O plates gradually became the lamellar O phase. During furnace cooling, the grain boundary O phase became continuous and well-defined and the thickness and the length of acicular O phase changed greatly as well. The growth of lamellar O-phase structures developed a typical Widmanstätten structure in B2 grain. The formation of this microstructure was due to the fact that O phase had sufficient time for nucleation and growth at a slow cooling mode. In addition, Widmanstätten O phase precipitated directly from B2 phase maintained specific orientation relationships with B2 matrix, i.e., {001}O//{110}B2 and <110>O//<111>B2. When cooled from a lower temperature (980 ℃), the increase of the phase boundary due to the presence of α2 particles provided favorable nucleation sites for O phase, and the acicular O-phase initially precipitated aroundα2 particles. The volume fraction and size of α2 particles during water quenching and oil quenching were similar with the particles in as-received Ti-22Al-25Nb alloy slab since the solution temperature was lower than the forging temperature. Compared with rapid cooling following heated at 1060 ℃, B2 grain size was smaller at 980 ℃ due to the combination of low heating temperature and pinning effect of α2 particle. During air cooling and forced air cooling, the acicular O lamellae were precipitated from B2 matrix, B2 grain boundaries and around α2 particles. Similar to 1060 ℃ cooled samples, the fine needle-like O lamellae precipitated into flocculent clusters. As the cooling rate further decreased (furnace cooling), the volume fraction of the floccular O phase precipitated in B2 grains and around α2 particles greatly increased. Meanwhile, α2 particles appeared to be decomposed and the precipitated rim-O phaseappeared in the periphery of α2 particles. The rim O phase formed through a decomposition reaction of α2→α2 (Nb-lean) + O (Nb-rich) was controlled by a diffusional mechanism and maintain specific orientation relationship, i.e., {001}O//{0001}α2 and <110>O//<11 2 ¯ 0>α2, with the parent α2 particles. Rapid cooling (water-quenching and oil-quenching) led to the lowest macrohardness values for both 1060 and 980 ℃ cooling conditions, attributed to the low strength of B2 phase. Aircooling and forcedair cooling enhanced alloy macrohardness due to extensive precipitation of acicular O-phase. However, partial dissolution of α2 particles at higher temperatures (1060 ℃) reduced nucleation sites for O phase, resulting in lower macrohardness compared to 980 ℃ cooled samples. Furnace cooling drastically reduced macrohardness owing to the increased volume fraction and coarsening of lamellar O phase. In summary, macrohardness under different cooling modes primarily correlated with Ophase precipitation strengthening, and the alloy macrohardness reached a maximum value under aircooling.

KeyWords AITranslate

Ti-22Al-25Nb alloy cooling modes microstructure evolution orientation relationship macrohardness

[1]Banerjee D,Gogia A K,Nandy T K,Joshi V A. A new ordered orthorhombic phase in a Ti3AlNb alloy [J]. Acta Metallurgica,1988,36(4):871.

[2]Boehlert C J,Cowen C J,Jaeger C R,Niinomi M,Akahori T. Tensile and fatigue evaluation of Ti-15Al-33Nb (at.%) and Ti-21Al-29Nb (at.%) alloys for biomedical applications [J]. Materials Science and Engineering:C,2005,25(3):263.

[3](尹续臣,陈志勇,王清江,刘建荣,李文辉,邓浩,罗恒军. 退火处理对粉末冶金Ti2AlNb合金电子束焊接接头显微组织和拉伸性能的影响 [J]. 稀有金属材料与工程,2024,53(8):2293.)

X C Yin,Z Y Chen,Q J Wang,J R Liu,W H Li,H Deng,H J Luo. Influence of annealing on microstructure and tensile properties of electron beamweldment of powder metallurgy Ti2AlNb alloy [J]. Rare Metal Materials and Engineering,2024,53(8):2293.

[4]Nandy T K,Banerjee D. Creep of the orthorhombic phase base on the intermetallic Ti2AlNb [J]. Intermetallics,2000,8(1):915.

[5](冯艾寒,李渤渤,沈军. Ti2AlNb基合金的研究进展 [J]. 材料与冶金学报,2011,10(1):30.)

A H Feng,B B Li,J Shen. Recent advances on Ti2AlNb-based alloys [J]. Journal of Materials and Metallurgy,2011,10(1):30.

[6](李萍,丁瑞东,张勇强,石成峰,郅强,薛克敏. O相对Ti2AlNb合金B2基体相拉伸性能影响的分子动力学模拟 [J]. 稀有金属材料与工程,2024,53(6):1701.)

P Li,R D Ding,Y Q Zhang,C F Shi,Q Zhi,K M Xue. Molecular dynamics simulation of effect of O phase on tensile properties of B2 matrix phase in Ti2AlNb alloy [J]. Rare Metal Materials and Engineering,2024,53(6):1701.

[7](裴会平,刘冬,姚利盼,邵天敏,刘巧沐,刘亮亮,陈乾明. Ti2AlNb合金研究进展及在航空发动机上应用可行性分析 [J]. 材料工程,2025,53(1):28.)

H P Pei,D Liu,L P Yao,T M Shao,Q M Liu,L L Liu,Q M Chen. Research progress of Ti2AlNb alloy and feasibility analysis of its application in aero engines [J]. Journal of Materials Engineering,2025,53(1):28.

[8]Wang W,Zeng W D,Xue C,Liang X B,Zhang J W. Microstructural evolution,creep,and tensile behavior of a Ti-22Al-25Nb (at%) orthorhombic alloy [J]. Materials Science and Engineering:A,2014,603(1):176.

[9](马雄,张晓越,师俊东,曾卫东,梁晓波,张建伟. Ti-22Al-25Nb合金盘件B2/β锻工艺优化 [J]. 热加工工艺,2023,52(23):83.)

X Ma,X Y Zhang,J D Shi,W D Zeng,X B Liang,J W Zhang. Optimization of B2/β forging process for Ti-22Al-25Nb alloy disk [J]. Hot Working Technology,2023,52(23):83.

[10]Li D,Zeng W D,Ma H Y,Xu J W,Liang X B. Evolution of lamellar O phase during hot compression in Ti2AlNb-based alloy [J]. Science of Advanced Materials,2022,14(4):682.

[11]Zheng Y P,Zeng W D,Li D,Zhao Q Y,Liang X B,Zhang J W. Fracture toughness of the bimodal size lamellar O phase microstructures in Ti-22Al-25Nb (at.%) orthorhombic alloy [J]. Journal of Alloys Compounds,2017,709(1):511.

[12](李宗泽,卫俊鑫,高志荣. 热处理中双尺寸O相的变体选择和析出行为 [J]. 塑性工程学报,2025,32(1):218.)

Z Z Li,J X Wei,Z R Gao. Variant selection and precipitation behavior of double-size O phases in heat treatment [J]. Journal of Plasticity Engineering,2025,32(1):218.

[13](徐建伟,纪晓宇,田胜利,吴望月,曾卫东. TC17钛合金在连续冷却过程中的组织析出特征 [J]. 稀有金属,2024,48(3):317.)

J W Xu,X Y Ji,S L Tian,W Y Wu,W D Zeng. Microstructure precipitation characteristics of TC17 titanium alloy during continuous cooling [J]. Chinese Journal of Rare Metals,2024,48(3):317.

[14](姜森宝,王宇盛,陈瑶. Ti2AlNb轧板激光弯曲工艺及微观组织研究 [J]. 锻压技术,2024,49(5):61.)

S B Jiang,Y S Wang,Y Chen. Research on laser bending process and microstructure for Ti2AlNb rolled sheet [J]. Forging & Stamping Technology,2024,49(5):61.

[15](周平,熊淑秋,周林. 时效温度对钛合金微观组织和力学性能的影响 [J]. 锻压技术,2025,50(6):180.)

P Zhou,S Q Xiong,L Zhou. Influence of aging temperature on microstructure and mechanical properties for titanium alloys [J]. Forging & Stamping Technology,2025,50(6):180.

[16]Muraleedharan K,Banerjee D,Banerjee S,Lele S. The α2-to-O transformation in Ti-Al-Nb alloys [J]. Philosophical Magazine A,1995,71(8):101.

[17]Wu Y,Yang D Z,Song G M. The formation mechanism of the O phase in a Ti3Al-Nb alloy [J]. Intermetallics,2000,8(5):629.

[18]Sadi F A,Servant C. On the B2→O phase transformation in Ti-Al-Nb alloys [J]. Materials Science and Engineering:A,2003,346(2):19.

[19]Muraleedharan K,Nandy T K,Banerjee D,Lele S. Phase stability and ordering behaviour of the O phase in Ti-Al-Nb alloys [J]. Intermetallics,1995,3(1):187.

[20]Muraleedharan K,Gogia A K,Nandy T K,Banerjee D,Lele S. Transformations in a Ti-24Al-15Nb alloy:Part I. Phase equilibria and microstructure [J]. Metallurgical Transactions A,1992,23(1):401.

[21]Boehlert C J,Majumdar B S,Seetharaman V,Miracle D B. Part I. the microstructural evolution in Ti-Al-Nb O+bcc orthorhombic alloys [J]. Metallurgical and Materials Transaction A,1999,30(1):2305.

[22]Zheng Y P,Zeng W D,Zhang P H,Ma H Y,Li D,Xu J W,Ma X. Anti-correlation between solution strengthening and precipitation strengthening in lamellar O microstructures of a Ti2AlNb based alloy [J]. Journal of Alloys Compounds,2020,847(1):1.

[23]Huang Y,Liu Y C,Li C,Ma Z Q,Yu L M,Li H J. Microstructure evolution and phase transformations in Ti-22Al-25Nb alloys tailored by super-transus solution treatment [J]. Vacuum,2019,161(1):209.

[24]Raghavan V. Al-Nb-Ti (aluminum-niobium-titanium) [J]. Journal of Phase Equilibria and Diffusion,2010,31(1):47.

[25]Kumpfert J,Kaysser W A. Orthorhombic titanium aluminides:phases,phase transformation and microstructure evolution [J]. Materials Research and Advanced Techniques,2001,92(2):128.

[26]Popov A A,Illarionov A G,Grib S V,Demakov S L,Karabanalov M S,Elkina O A. Phase and structural transformations in the alloy on the basis of the orthorhombic titanium aluminide [J]. The Physics of Metals and Metallography,2008,106(4):399.

[27]Wang W,Zeng W D,Li D,Zhu B,Zheng Y P,Liang X B. Microstructural evolution and tensile behavior of Ti2AlNb alloys based α2-phase decomposition [J]. Materials Science and Engineering:A,2016,662(1):120.

[28]Wu Y,Zhen L,Yang D Z,Mao J F. TEM observation of the α2/O interface in a Ti3A1-Nb alloy [J]. Materials Letters,1997,32(5):319.

[29]Banerjee D. Deformation of the O and α2 phases in the Ti-Al-Nb system [J]. Philosophical Magazine A,1995,72(6):1559.

[30](王伟,曾卫东,薛晨,梁晓波,张建伟. 热处理对Ti-22Al-25Nb合金显微组织演变及显微硬度的影响 [J]. 中国有色金属学报,2013,23(1):456.)

W Wang,W D Zeng,C Xue,X B Liang,J W Zhang. Effect of heat treatment on microstructural evolution and micro-hardness of Ti-22Al-25Nb orthorhombic alloy [J]. The Chinese Journal of Nonferrous Metals,2013,23(1):456.

[31]Boehlert C. Part Ⅲ. the tensile behavior of Ti-Al-Nb O+bcc orthorhombic alloys [J]. Metallurgical and Materials Transactions A,2001,32:1977.

[32]Wei B B,Tang B,Chen X F,Xu Q,Zhang S J,Kou H C,Li J S. Precipitation behavior of orthorhombic phase in Ti-22Al-25Nb alloy during slow cooling aging treatment and its effect on tensile properties [J]. Metals,2020,10(11):1515.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY24120006

Chinese Library Classification Number:TK91

Citation Information:

With the rapid advancement of aerospace propulsion systems, the demand for high-performance materials capable of enduring extreme thermal and mechanical stresses in aeroengine components has reached unprecedented levels. Ti-22Al-25Nb (atom fraction) alloy, an orthorhombic titanium aluminide (Ti2AlNb-based system), has emerged as a leading candidate for next-generation high-temperature structural applications due to its exceptional combination of low density, high specific strength, superior creep resistance, and remarkable stability under prolonged thermal exposure. This alloy system primarily consists of three distinct phases:the ordered body-centered cubic (B2) phase, the hexagonal close-packed α2 phase (derived from Ti3Al), and the orthorhombic (O) phase. However, the intricate interplay between phase transformations and microstructural evolution during thermal processing poses significant challenges in optimizing its mechanical performance. To address this, the present study systematically investigated the phase transformation and microstructure evolution of Ti-22Al-25Nb alloy under varying cooling conditions, with a focus on elucidating the nucleation mechanisms, growth behavior, and crystallographic orientation relationships of O phase with the parent phase. Specimens were subjected to controlled heat treatments at two critical temperatures (1060 and 980 ℃) followed by cooling at rates ranging from rapid quenching (water and oil) to slow furnace cooling. Phase identification and structural characterization were performed using X-ray diffraction (XRD) with Cu-Kα radiation. Microstructural features were analyzed via optical microscope (OM) and scanning electron microscope (SEM). Crystallographic orientation relationships between the precipitated O phase and the parent phase (B2 matrix or α2 particles) during the cooling process were resolved using electron backscatter diffraction (EBSD). Macrohardness of the alloys were tested by using a macrohardness tester. The results indicated that the morphology of the precipitated O phase was significantly influenced by the cooling mode. When the alloy was cooled from a higher temperature (1060 ℃), numerous acicular O phase precipitated formed in B2 matrix, along B2 grain boundaries, and around α2 particles. The specimen cooled at higher rates, such as water quenching and oil quenching, showed retention of the high-temperature B2 phase, in which B2 phase was an ordered cubic phase, due to the window for phase transformation to form new α2 phase was narrow and rapid cooling suppressed elemental diffusion, particularly of Nb elements. Moreover, the high niobium content in Ti-22Al-25Nb alloy decelerated diffusion processes and led to sluggish phase transformations. With the decrease of the cooling rate, such as air cooling and forced air cooling, the flocculent O phases consisting of numerous fine needle-like O plates gradually became the lamellar O phase. During furnace cooling, the grain boundary O phase became continuous and well-defined and the thickness and the length of acicular O phase changed greatly as well. The growth of lamellar O-phase structures developed a typical Widmanstätten structure in B2 grain. The formation of this microstructure was due to the fact that O phase had sufficient time for nucleation and growth at a slow cooling mode. In addition, Widmanstätten O phase precipitated directly from B2 phase maintained specific orientation relationships with B2 matrix, i.e., {001}O//{110}B2 and <110>O//<111>B2. When cooled from a lower temperature (980 ℃), the increase of the phase boundary due to the presence of α2 particles provided favorable nucleation sites for O phase, and the acicular O-phase initially precipitated aroundα2 particles. The volume fraction and size of α2 particles during water quenching and oil quenching were similar with the particles in as-received Ti-22Al-25Nb alloy slab since the solution temperature was lower than the forging temperature. Compared with rapid cooling following heated at 1060 ℃, B2 grain size was smaller at 980 ℃ due to the combination of low heating temperature and pinning effect of α2 particle. During air cooling and forced air cooling, the acicular O lamellae were precipitated from B2 matrix, B2 grain boundaries and around α2 particles. Similar to 1060 ℃ cooled samples, the fine needle-like O lamellae precipitated into flocculent clusters. As the cooling rate further decreased (furnace cooling), the volume fraction of the floccular O phase precipitated in B2 grains and around α2 particles greatly increased. Meanwhile, α2 particles appeared to be decomposed and the precipitated rim-O phaseappeared in the periphery of α2 particles. The rim O phase formed through a decomposition reaction of α2→α2 (Nb-lean) + O (Nb-rich) was controlled by a diffusional mechanism and maintain specific orientation relationship, i.e., {001}O//{0001}α2 and <110>O//<11 2 ¯ 0>α2, with the parent α2 particles. Rapid cooling (water-quenching and oil-quenching) led to the lowest macrohardness values for both 1060 and 980 ℃ cooling conditions, attributed to the low strength of B2 phase. Aircooling and forcedair cooling enhanced alloy macrohardness due to extensive precipitation of acicular O-phase. However, partial dissolution of α2 particles at higher temperatures (1060 ℃) reduced nucleation sites for O phase, resulting in lower macrohardness compared to 980 ℃ cooled samples. Furnace cooling drastically reduced macrohardness owing to the increased volume fraction and coarsening of lamellar O phase. In summary, macrohardness under different cooling modes primarily correlated with Ophase precipitation strengthening, and the alloy macrohardness reached a maximum value under aircooling.

quote

GB/T 7714-2015 [1] Dong Li, Yi Dai, Yingjie Xie, et al. Microstructure and Macrohardness of Ti2AlNb-Based Alloy with Different Cooling Modes[J]. Chinese Journal of Rare Metals, 2026, 50(8): 1385-1392. DOI:10.13373/j.cnki.cjrm.XY24120006.
MLA [1] Dong Li, et al., "Microstructure and Macrohardness of Ti2AlNb-Based Alloy with Different Cooling Modes." Chinese Journal of Rare Metals, vol. 50, no. 8, 2026, pp. 1385-1392, https://doi.org/10.13373/j.cnki.cjrm.XY24120006.
APA [1] Dong Li, Yi Dai, Yingjie Xie, Wenjie Fu, Peng Li, Zhimin Hou, & Xiong Ma. (2026). Microstructure and Macrohardness of Ti2AlNb-Based Alloy with Different Cooling Modes. Chinese Journal of Rare Metals, 50(8), 1385-1392. https://doi.org/10.13373/j.cnki.cjrm.XY24120006
IEEE [1] Dong Li, Yi Dai, Yingjie Xie, Wenjie Fu, Peng Li, Zhimin Hou, and Xiong Ma, "Microstructure and Macrohardness of Ti2AlNb-Based Alloy with Different Cooling Modes," Chinese Journal of Rare Metals, vol. 50, no. 8, pp. 1385-1392, 2026, doi: 10.13373/j.cnki.cjrm.XY24120006. keywords: {Ti-22Al-25Nb alloy;cooling modes;microstructure evolution;orientation relationship;macrohardness}