Université catholique de Louvain; Institute of Physical Chemistry; Institute of Physical Chemistry; Institute of Physical Chemistry; Institute of Physical Chemistry Polish Academy of Sciences; University of Warsaw; University of Warsaw; University of Warsaw;Institute of Applied Physics “Nello Carrara”─National Research Council (IFAC-CNR); Cardinal Stefan Wyszynski University in Warsaw; Institute of Physical Chemistry
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The present research reports on in-water, site-specific photodeposition of glyphosate (GLP)-containing polyacrylamide (PAA-GLP) nanometer-thick films (nanofilms) on an inner surface of fused silica (fused quartz) microcapillaries presilanized with trimethoxy(octen-7-yl)silane (TMOS). TMOS was chosen because of the vinyl group presence in its structure, enabling its participation in the (UV light)-activated free-radical polymerization (UV-FRP) after its immobilization on a fused silica surface. The photodeposition was conducted in an aqueous (H2O/ACN; 3:1, v/v) solution, using UV-FRP (λ = 365 nm) of the acrylamide (AA) functional monomer, the N,N′-methylenebis(acrylamide) (BAA) cross-linking monomer, GLP, and the azobisisobutyronitrile (AIBN) UV-FRP initiator. Acetonitrile (ACN) was used as the porogen and the solvent to dissolve monomers and GLP. Because of the micrometric diameters of microcapillaries, the silanization and photodeposition procedures were first optimized on fused silica slides. The introduction of TMOS, as well as the formation of PAA and PAA-GLP nanofilms, was determined using atomic force microscopy (AFM), scanning electron microscopy with energy-dispersive X-ray (SEM–EDX) spectroscopy, and confocal micro-Raman spectroscopy. Particularly, AFM and SEM–EDX measurements determined nanofilms’ thickness and GLP content, respectively, whereas in-depth confocal (micro-Raman spectroscopy)-assisted imaging of PAA- and PAA-GLP-coated microcapillary inner surfaces confirmed the successful photodeposition. Moreover, we examined the GLP impact on polymer gelation by monitoring hydration in a hydrogel and a dried powder PAA-GLP. Our study demonstrated the usefulness of the in-capillary micro-Raman spectroscopy imaging and in-depth profiling of GLP-encapsulated PAA nanofilms. In the future, our simple and inexpensive procedure will enable the fabrication of polymer-based microfluidic chemosensors or adsorptive-separating devices for GLP detection, determination, and degradation.

KeyWords AITranslate

confocal microRaman spectroscopy glyphosate fused silica microcapillary microfluidics nanofilm photopolymerization Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01461

Chinese Library Classification Number:

Citation Information:

The present research reports on in-water, site-specific photodeposition of glyphosate (GLP)-containing polyacrylamide (PAA-GLP) nanometer-thick films (nanofilms) on an inner surface of fused silica (fused quartz) microcapillaries presilanized with trimethoxy(octen-7-yl)silane (TMOS). TMOS was chosen because of the vinyl group presence in its structure, enabling its participation in the (UV light)-activated free-radical polymerization (UV-FRP) after its immobilization on a fused silica surface. The photodeposition was conducted in an aqueous (H2O/ACN; 3:1, v/v) solution, using UV-FRP (λ = 365 nm) of the acrylamide (AA) functional monomer, the N,N′-methylenebis(acrylamide) (BAA) cross-linking monomer, GLP, and the azobisisobutyronitrile (AIBN) UV-FRP initiator. Acetonitrile (ACN) was used as the porogen and the solvent to dissolve monomers and GLP. Because of the micrometric diameters of microcapillaries, the silanization and photodeposition procedures were first optimized on fused silica slides. The introduction of TMOS, as well as the formation of PAA and PAA-GLP nanofilms, was determined using atomic force microscopy (AFM), scanning electron microscopy with energy-dispersive X-ray (SEM–EDX) spectroscopy, and confocal micro-Raman spectroscopy. Particularly, AFM and SEM–EDX measurements determined nanofilms’ thickness and GLP content, respectively, whereas in-depth confocal (micro-Raman spectroscopy)-assisted imaging of PAA- and PAA-GLP-coated microcapillary inner surfaces confirmed the successful photodeposition. Moreover, we examined the GLP impact on polymer gelation by monitoring hydration in a hydrogel and a dried powder PAA-GLP. Our study demonstrated the usefulness of the in-capillary micro-Raman spectroscopy imaging and in-depth profiling of GLP-encapsulated PAA nanofilms. In the future, our simple and inexpensive procedure will enable the fabrication of polymer-based microfluidic chemosensors or adsorptive-separating devices for GLP detection, determination, and degradation.

quote

GB/T 7714-2015 [1] Jaroslaw Mazuryk, Katarzyna Klepacka, Joanna Piechowska, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01461.
MLA [1] Jaroslaw Mazuryk, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01461.
APA [1] Jaroslaw Mazuryk, Katarzyna Klepacka, Joanna Piechowska, Jakub Kalecki, Ladislav Derzsi, Piotr Piotrowski, Piotr Paszke, Dorota A. Pawlak, Simone Berneschi, Wlodzimierz Kutner, & Piyush Sindhu Sharma. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01461
IEEE [1] Jaroslaw Mazuryk, Katarzyna Klepacka, Joanna Piechowska, Jakub Kalecki, Ladislav Derzsi, Piotr Piotrowski, Piotr Paszke, Dorota A. Pawlak, Simone Berneschi, Wlodzimierz Kutner, and Piyush Sindhu Sharma, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01461. keywords: {confocal microRaman spectroscopy;glyphosate;fused silica microcapillary;microfluidics;nanofilm;photopolymerization;Show More}