daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Functionally Graded Multilayer Composites Based on Poly(D,L lactide)/Bioactive Fillers Fabricated by a 3D Direct Pellet Printing Multi-Extrusion Process AITranslate

France|Université de Lyon;Université de Lyon; Université Jean Monnet; Université Jean Monnet
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The aim of the present work was to investigate a 3D manufacturing process dealing with 3D Direct Pellet multi-Extrusion (DPPmE). Throughout this paper, various functionally graded materials (FGM) were obtained with tailored properties for bone regeneration. Therefore, an experimental investigation was performed to gain a better understanding of the structure-processing-properties relationships. A poly(D,l-lactic acid) (PDLLA) matrix and bioglass (BG) or hydroxyapatite (HA) bioactive fillers were chosen to obtain hybrid FGM in comparison to composite references. Different compositions and shape factors (from microspheres to fibers) of these bioactive fillers were used to control the PDLLA matrix degradation. Then, different strategies of DPPmE were used to tailor and tune the desired gradient of properties. Interestingly, good interfaces and adhesion properties were obtained. Subsequently, rheological, size-exclusion chromatography, and porosity measurements corroborated the present findings. Besides, tensile as well as thermomechanical properties showed the advantages of the DPPmE process to fabricate FGM composites with tailored architectures.

KeyWords AITranslate

3D printing multifunctional composites biocomposite microstructural analysis bioglass rheology
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01475

Chinese Library Classification Number:

Citation Information:

The aim of the present work was to investigate a 3D manufacturing process dealing with 3D Direct Pellet multi-Extrusion (DPPmE). Throughout this paper, various functionally graded materials (FGM) were obtained with tailored properties for bone regeneration. Therefore, an experimental investigation was performed to gain a better understanding of the structure-processing-properties relationships. A poly(D,l-lactic acid) (PDLLA) matrix and bioglass (BG) or hydroxyapatite (HA) bioactive fillers were chosen to obtain hybrid FGM in comparison to composite references. Different compositions and shape factors (from microspheres to fibers) of these bioactive fillers were used to control the PDLLA matrix degradation. Then, different strategies of DPPmE were used to tailor and tune the desired gradient of properties. Interestingly, good interfaces and adhesion properties were obtained. Subsequently, rheological, size-exclusion chromatography, and porosity measurements corroborated the present findings. Besides, tensile as well as thermomechanical properties showed the advantages of the DPPmE process to fabricate FGM composites with tailored architectures.

quote

GB/T 7714-2015 [1] Xavier Lacambra Andreu, JeanMarc Chenal, Abderrahim Maazouz, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01475.
MLA [1] Xavier Lacambra Andreu, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01475.
APA [1] Xavier Lacambra Andreu, JeanMarc Chenal, Abderrahim Maazouz, & Khalid Lamnawar. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01475
IEEE [1] Xavier Lacambra Andreu, JeanMarc Chenal, Abderrahim Maazouz, and Khalid Lamnawar, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01475. keywords: {3D printing;multifunctional composites;biocomposite;microstructural analysis;bioglass;rheology}