Dual Redox-Responsive Os/Ru-Based Alternated Heterobimetallic Supramolecular Polymer as a Multicolor Electrochromic Material for Camouflage Devices Dual Redox-Responsive Os/Ru-Based Alternated Heterobimetallic Supramolecular Polymer as a Multicolor Electrochromic Material for Camouflage Devices AITranslate

CSIR-Indian Institute of Chemical Technology (CSIR-IICT); CSIR-Indian Institute of Chemical Technology (CSIR-IICT); CSIR-Indian Institute of Chemical Technology (CSIR-IICT)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Materials that show multicolor electrochromism, including yellow and green, are highly applicable for various smart applications including voltage-tunable multicolor electrochromic (EC) displays and camouflage devices. Although metallo-supramolecular polymers (MSPs) show excellent EC color variability with attractive EC properties, the generation of multicolor electrochromism from one MSP is still difficult. Moreover, an MSP-based multicolor EC device (ECD) that also exhibits yellow and green EC colors has not been realized to date. Herein, we report the synthesis of a dual redox-responsive heterobimetallic supramolecular polymer (PolyOsRu) as a multicolor EC material that can also be used for camouflage applications. PolyOsRu was synthesized by stepwise homoleptic complexation of Os2+ and Ru2+ ions using a 2,2′:6′,2″-terpyridine-based ligand and characterized by various analytical and spectroscopic techniques. The polymer shows broad absorption (312–671 nm) and well-separated dual redox potentials of Os2+/Os3+ (E1/2 = 0.59 V) and Ru2+/Ru3+ (E1/2 = 0.93 V) pairs. A thin film of PolyOsRu on ITO displays reversible multicolor (brown–red ↔ yellow ↔ green) electrochromism with a maximum optical contrast of ∼58%, fast EC color switching (<1 s), a good coloration efficiency of 404.39 cm2/C, and a more than 2400 EC cycling stability. Finally, the fabrication of a solid-state ECD and a prototype EC camouflage display with the polymer film is demonstrated to represent its potentiality as a multicolor EC material for display and camouflage applications.

KeyWords AITranslate

heterobimetallic supramolecular polymer osmium ruthenium multicolor electrochromism electrochromic deviceShow More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01765

Chinese Library Classification Number:

Citation Information:

Materials that show multicolor electrochromism, including yellow and green, are highly applicable for various smart applications including voltage-tunable multicolor electrochromic (EC) displays and camouflage devices. Although metallo-supramolecular polymers (MSPs) show excellent EC color variability with attractive EC properties, the generation of multicolor electrochromism from one MSP is still difficult. Moreover, an MSP-based multicolor EC device (ECD) that also exhibits yellow and green EC colors has not been realized to date. Herein, we report the synthesis of a dual redox-responsive heterobimetallic supramolecular polymer (PolyOsRu) as a multicolor EC material that can also be used for camouflage applications. PolyOsRu was synthesized by stepwise homoleptic complexation of Os2+ and Ru2+ ions using a 2,2′:6′,2″-terpyridine-based ligand and characterized by various analytical and spectroscopic techniques. The polymer shows broad absorption (312–671 nm) and well-separated dual redox potentials of Os2+/Os3+ (E1/2 = 0.59 V) and Ru2+/Ru3+ (E1/2 = 0.93 V) pairs. A thin film of PolyOsRu on ITO displays reversible multicolor (brown–red ↔ yellow ↔ green) electrochromism with a maximum optical contrast of ∼58%, fast EC color switching (<1 s), a good coloration efficiency of 404.39 cm2/C, and a more than 2400 EC cycling stability. Finally, the fabrication of a solid-state ECD and a prototype EC camouflage display with the polymer film is demonstrated to represent its potentiality as a multicolor EC material for display and camouflage applications.

quote

GB/T 7714-2015 [1] Sanjib Sarmah, Siddhartha Shankar Kashyap, Manas Kumar Bera. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01765.
MLA [1] Sanjib Sarmah, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01765.