Antifungal Polymer Containing Menthoxy Triazine AITranslate

Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Tsinghua University; Tsinghua University; Beijing University of Chemical Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

An antifungal polymer containing menthoxy triazine was synthesized by a polycondensation of 2,4-dichloro-6-menthoxy-1,3,5-triazine (DMT) with 4,4-oxidianiline (ODA) and named as P(MT-alt-ODA). To emphasize the antifungal performance of the menthoxy group, series of similar triazine polymers derived correspondingly with hydrogen, ethoxy, and decoxy groups were prepared and served as controls. The spores of Aspergillus niger were used for an antifungal evaluation. Only P(MT-alt-ODA) can effectively inhibit the growth and spread of spores. A further in-depth analysis combined with an inhibition zone and water contact angle illustrated that the surface menthoxy stereochemistry is crucial for the antifungal mechanism.

KeyWords AITranslate

antifungal polymer menthoxy triazine stereochemical antifungal strategy managing and controlling microorganisms fungal Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00506

Chinese Library Classification Number:

Citation Information:

An antifungal polymer containing menthoxy triazine was synthesized by a polycondensation of 2,4-dichloro-6-menthoxy-1,3,5-triazine (DMT) with 4,4-oxidianiline (ODA) and named as P(MT-alt-ODA). To emphasize the antifungal performance of the menthoxy group, series of similar triazine polymers derived correspondingly with hydrogen, ethoxy, and decoxy groups were prepared and served as controls. The spores of Aspergillus niger were used for an antifungal evaluation. Only P(MT-alt-ODA) can effectively inhibit the growth and spread of spores. A further in-depth analysis combined with an inhibition zone and water contact angle illustrated that the surface menthoxy stereochemistry is crucial for the antifungal mechanism.

quote

GB/T 7714-2015 [1] Xuefei Li, Zixu Xie, Guofeng Li, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00506.
MLA [1] Xuefei Li, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00506.
APA [1] Xuefei Li, Zixu Xie, Guofeng Li, Lei Tao, Yen Wei, & Xing Wang. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00506
IEEE [1] Xuefei Li, Zixu Xie, Guofeng Li, Lei Tao, Yen Wei, and Xing Wang, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00506. keywords: {antifungal polymer;menthoxy triazine;stereochemical antifungal strategy;managing and controlling microorganisms;fungal;Show More}