Preparation of Aqueous Solutions with Information on Solids (ASIS) of a Mechanochromic Luminescent Tetraphenylethylene Derivative by Complexation with Polysaccharides AITranslate

Hiroshima University; Hiroshima University; Hiroshima University; Shinshu University; Hiroshima University; Hiroshima University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The emission wavelengths of mechanochromic luminescent (ML) materials differ in the solid state based on molecular packing, whereas they exhibit one homogenized emission wavelength when dispersed in a solvent. Using a top-down approach, we developed a method that can maintain the solid state properties of ML materials in aqueous solutions. We confirmed that the crystallographic information on a tetraphenylethylene derivative with mechanochromic luminescence in the solid state was preserved in aqueous solutions via complexation with polysaccharides. The aqueous solutions of the complexes were stable for over 1 week.

KeyWords AITranslate

aggregationinduced emission mechanochromic luminescence polysaccharides aqueous solution supramolecular chemistry Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00646

Chinese Library Classification Number:

Citation Information:

The emission wavelengths of mechanochromic luminescent (ML) materials differ in the solid state based on molecular packing, whereas they exhibit one homogenized emission wavelength when dispersed in a solvent. Using a top-down approach, we developed a method that can maintain the solid state properties of ML materials in aqueous solutions. We confirmed that the crystallographic information on a tetraphenylethylene derivative with mechanochromic luminescence in the solid state was preserved in aqueous solutions via complexation with polysaccharides. The aqueous solutions of the complexes were stable for over 1 week.

quote

GB/T 7714-2015 [1] Riku Omokawa, Riku Kawasaki, Kouta Sugikawa, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00646.
MLA [1] Riku Omokawa, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00646.
APA [1] Riku Omokawa, Riku Kawasaki, Kouta Sugikawa, Tomoki Nishimura, Toshimi Nakaya, & Atsushi Ikeda. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00646
IEEE [1] Riku Omokawa, Riku Kawasaki, Kouta Sugikawa, Tomoki Nishimura, Toshimi Nakaya, and Atsushi Ikeda, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00646. keywords: {aggregationinduced emission;mechanochromic luminescence;polysaccharides;aqueous solution;supramolecular chemistry;Show More}