Highly Conductive Liquid Metal-Based Shape Memory Material with an Ultrasensitive Fire Warning Response AITranslate

Hunan University of Technology; Harbin Institute of Technology; Harbin Institute of Technology; Harbin Institute of Technology; Hunan University of Technology; Hunan University of Technology; Harbin Institute of Technology; Harbin Institute of Technology; Harbin Institute of Technology; Harbin Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Fire warning materials always play an important role in safeguarding people’s lives and property. In general, existing approaches to realize supersensitive fire warning responses are typically focused on how to reduce response times. However, most strategies to effectively achieve fire warning require a high trigger temperature of over 180 °C that is unsuitable for fire warning of materials with a low flash point. Herein, a liquid metal-based shape memory material (LM-SMM) is fabricated by integrating liquid metal (LM), polydimethylsiloxane (PDMS), and polyurethane foam. The phase transition function of the LM contributes to better shape fixation properties. Meanwhile, the flexibility of PDMS assures good shape recovery performance. In particular, the LM-SMM still owns favorable electrical conductivity that could facilitate its application in advanced electronics. The combination of switchable structure and excellent electrical conductivity makes this LM-SMM appropriate for an ultrasensitive fire warning response. With the help of such performance, the LM-SMM can achieve the lowest fire-warning response temperature in a fast response time, which displays promising application in the safe storage of flammable materials. More importantly, this work could not only achieve the fabrication of highly conductive LM-SMM but also expand applications, thus providing possibilities for the next-generation supersensitive fire-warning response materials.

KeyWords AITranslate

shape memory material liquid metal high conductivity deformable structure ultrasensitive fire warning response
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00912

Chinese Library Classification Number:

Citation Information:

Fire warning materials always play an important role in safeguarding people’s lives and property. In general, existing approaches to realize supersensitive fire warning responses are typically focused on how to reduce response times. However, most strategies to effectively achieve fire warning require a high trigger temperature of over 180 °C that is unsuitable for fire warning of materials with a low flash point. Herein, a liquid metal-based shape memory material (LM-SMM) is fabricated by integrating liquid metal (LM), polydimethylsiloxane (PDMS), and polyurethane foam. The phase transition function of the LM contributes to better shape fixation properties. Meanwhile, the flexibility of PDMS assures good shape recovery performance. In particular, the LM-SMM still owns favorable electrical conductivity that could facilitate its application in advanced electronics. The combination of switchable structure and excellent electrical conductivity makes this LM-SMM appropriate for an ultrasensitive fire warning response. With the help of such performance, the LM-SMM can achieve the lowest fire-warning response temperature in a fast response time, which displays promising application in the safe storage of flammable materials. More importantly, this work could not only achieve the fabrication of highly conductive LM-SMM but also expand applications, thus providing possibilities for the next-generation supersensitive fire-warning response materials.

quote

GB/T 7714-2015 [1] Wu Wang, Zhimin Fan, Jingfeng Wang, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00912.
MLA [1] Wu Wang, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00912.
APA [1] Wu Wang, Zhimin Fan, Jingfeng Wang, Chao Wu, Jianxin Tang, Li Tang, Dongjie Zhang, Zhimin Xie, Zhongjun Cheng, & Yuyan Liu. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00912
IEEE [1] Wu Wang, Zhimin Fan, Jingfeng Wang, Chao Wu, Jianxin Tang, Li Tang, Dongjie Zhang, Zhimin Xie, Zhongjun Cheng, and Yuyan Liu, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00912. keywords: {shape memory material;liquid metal;high conductivity;deformable structure;ultrasensitive fire warning response}