daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A Bilayered Carbon with High Sunlight-Absorption Coefficient Designed by Flat-Band-Guided Strategy AITranslate

Jilin University; Jilin University; Jilin University; Jilin University; Changchun University of Science and Technology; Jilin University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The electronic band structure of a material determines its photovoltaic performance. In this work, we developed a methodology to explore desired semiconducting materials with a specialized designed fitness function for characterizing flat electronic bands via the generalization of our in-house-developed CALYPSO method. An intriguing bilayered carbon with sp3- and sp2-hybridized bonds, related to a bilayered reconstruction of (111) diamond or twisted graphene, was proposed and termed as two-dimensional diaphite. Two-dimensional diaphite has a direct electronic bandgap of 1.20 eV, with a high density of states near the band edges caused by the nearby flat bands, affording an extremely high sunlight-absorption coefficient. The type-II van der Waals heterojunctions composed of 2D diaphite and InSe monolayers yielded extraordinary performance for solar-to-electricity conversion with a theoretical power conversion efficiency of up to a record-breaking value of 24.1%, making it a potential candidate for high-efficiency and ultrathin photovoltaic devices. Our results show that the approach proposed herein is a feasible way of searching for functional semiconducting materials with specialized characteristic energy-band structures.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00690

Chinese Library Classification Number:

Citation Information:

The electronic band structure of a material determines its photovoltaic performance. In this work, we developed a methodology to explore desired semiconducting materials with a specialized designed fitness function for characterizing flat electronic bands via the generalization of our in-house-developed CALYPSO method. An intriguing bilayered carbon with sp3- and sp2-hybridized bonds, related to a bilayered reconstruction of (111) diamond or twisted graphene, was proposed and termed as two-dimensional diaphite. Two-dimensional diaphite has a direct electronic bandgap of 1.20 eV, with a high density of states near the band edges caused by the nearby flat bands, affording an extremely high sunlight-absorption coefficient. The type-II van der Waals heterojunctions composed of 2D diaphite and InSe monolayers yielded extraordinary performance for solar-to-electricity conversion with a theoretical power conversion efficiency of up to a record-breaking value of 24.1%, making it a potential candidate for high-efficiency and ultrathin photovoltaic devices. Our results show that the approach proposed herein is a feasible way of searching for functional semiconducting materials with specialized characteristic energy-band structures.

quote

GB/T 7714-2015 [1] Rui Xu, Hang Zhai, Di Wang, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00690.
MLA [1] Rui Xu, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00690.
APA [1] Rui Xu, Hang Zhai, Di Wang, Xianqi Song, Dan Zhou, & Quan Li. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00690
IEEE [1] Rui Xu, Hang Zhai, Di Wang, Xianqi Song, Dan Zhou, and Quan Li, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00690.