ZnO@Ti3C2Tx MXene Hybrid Composite-Based Schottky-Barrier-Coated SAW Sensor for Effective Detection of Sub-ppb-Level NH3 at Room Temperature under UV Illumination AITranslate

Chungnam National University; Chungnam National University; Kyungpook National University; National Nanofab Center at Korea Advanced Institute of Science and Technology (KAIST); Chungnam National University; Chungnam National University; Joongbu University; Chungnam National University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Smart sensors capable of detecting NH3 at sub-ppb levels are important for human health in our daily life. Here, we demonstrate a surface acoustic wave (SAW) sensor based on ZnO@MXene hybrid heterostructure for ultrahigh NH3 gas detection under UV illumination at room temperature (RT). Under UV illumination, the ZnO@MXene SAW sensor not only significantly enhances the frequency response (Δf ≈ 32.24 kHz/20 ppm) but also effectively improves the selectivity with a low detection limit (89.41 ppb), short response/recovery times (92/104 s), long-term stability, and robust sensitivity under various relative humidity conditions (dark) to NH3 at RT. These unique NH3 sensing properties might be attributed to the enriched functional groups, oxygen vacancies, and excellent charge transfer at the Schottky barrier via band bending, which is explained using an energy band theory sensing mechanism. Overall, the current study offers strategic insights for designing light-activated high-performance SAW-based RT NH3 sensors in safety assurance and environmental monitoring.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00698

Chinese Library Classification Number:

Citation Information:

Smart sensors capable of detecting NH3 at sub-ppb levels are important for human health in our daily life. Here, we demonstrate a surface acoustic wave (SAW) sensor based on ZnO@MXene hybrid heterostructure for ultrahigh NH3 gas detection under UV illumination at room temperature (RT). Under UV illumination, the ZnO@MXene SAW sensor not only significantly enhances the frequency response (Δf ≈ 32.24 kHz/20 ppm) but also effectively improves the selectivity with a low detection limit (89.41 ppb), short response/recovery times (92/104 s), long-term stability, and robust sensitivity under various relative humidity conditions (dark) to NH3 at RT. These unique NH3 sensing properties might be attributed to the enriched functional groups, oxygen vacancies, and excellent charge transfer at the Schottky barrier via band bending, which is explained using an energy band theory sensing mechanism. Overall, the current study offers strategic insights for designing light-activated high-performance SAW-based RT NH3 sensors in safety assurance and environmental monitoring.

quote

GB/T 7714-2015 [1] Kedhareswara Sairam Pasupuleti, Alphi Maria Thomas, Devthade Vidyasagar, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00698.
MLA [1] Kedhareswara Sairam Pasupuleti, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00698.
APA [1] Kedhareswara Sairam Pasupuleti, Alphi Maria Thomas, Devthade Vidyasagar, Vempuluru Navakoteswara Rao, SoonGil Yoon, YoungHeon Kim, SongGang Kim, & MoonDeock Kim. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00698
IEEE [1] Kedhareswara Sairam Pasupuleti, Alphi Maria Thomas, Devthade Vidyasagar, Vempuluru Navakoteswara Rao, SoonGil Yoon, YoungHeon Kim, SongGang Kim, and MoonDeock Kim, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00698.