Synthesis and Consolidation of Ball-milled Nanocomposite WC-Co Powders Compaction AITranslate

Northwest Nonferrous Metal Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This paper presents the results of synthesis of nanocomposite WC-Co powders at room temperature-by high-energy ball milling.Discussion is made on the powder property.

KeyWords AITranslate

nanocomposite material mechanical alloying ball-milling compaction

1Mahday A A,et al.Mechanically induced solid state carburization for fabrication of nanocristwline ZrC refractory material powders[].Journal of Alloys and Compounds.2000

2Sherif M,et al.Solid-state amorphization reaction in mechanically deformeod AlxHf100- x multilayered composite powders and the effect of annealing[].Joarnal of Alloys and Compounds.1999

3Sherif M,et al.Mechanical solid state mixing for synthesizing of sicp/Al nanocomposite[].Journal of Alloys and Compounds.1998

1张建兵,李小强,龙雁,陈维平,李元元.WC-6Co-1.5Al合金高能球磨-电场活化烧结工艺的研究[J].粉末冶金工业,2005,15(6):13-17.

2张春华,郭亨群,宋志华,吴冲浒,吴其山.纳米碳化钨粉体的粒度表征[J].华侨大学学报:自然科学版,2010,31(4):388-391. 被引量:4

3吴翔,廖军,刘方舟.不同工艺条件对WC-20%Co硬质合金性能的影响[J].湖南有色金属,2013,29(1):44-46. 被引量:1

4唐玉霜.离子色谱柱切换法测定工业硫酸锰中的氯离子[J].湖南有色金属,2013,29(1):76-78. 被引量:1

5李少香,王兆丰,李文倩,周贵忠,刘光兆.硬质合金再生料的表征及影响因素研究[J].稀有金属与硬质合金,2014,42(4):63-67. 被引量:1

1朱诗秀.纳米钨粉生产工艺研究[J].有色金属科学与工程,2012,3(3):36-39. 被引量:6

2江荆,伍斯静,周花珑,覃建友.电感耦合等离子体原子发射光谱法测定硫酸锰中钙镁[J].冶金分析,2014,34(1):71-74. 被引量:5

3李广生.准纳米WC粉的试制[J].硬质合金,2015,32(3):175-181.

4李广生,李飞.纳米碳化钨粉的生产[J].中国钨业,2015,30(4):68-72. 被引量:2

5周新华,王力民,彭英健.我国硬质合金再生产业现状与发展[J].硬质合金,2016,33(5):356-364. 被引量:19

6蔡园园,房怀英,余文,黄文景,林伟端,杨建红.采用数字图像处理的机制砂粒度级配检测方法[J].华侨大学学报:自然科学版,2019,40(5):567-573. 被引量:8

7易长宾,金星,吴翔.添加W粉对YG20C硬质合金组织及性能的影响[J].稀有金属与硬质合金,2019,47(2):68-73. 被引量:2

1雷景轩,马学鸣,余海峰,朱丽慧.机械合金化制备电触头材料进展[J].材料科学与工程,2002,20(3):457-460. 被引量:11

2刘维平.制备细铜粉的新方法[J].粉末冶金技术,2008,26(5):360-364. 被引量:1

3王迎,王尔德,于洋.两种球磨方法对Nd_2Fe_(14)B/-αFe形成非晶和纳米晶效率的研究[J].粉末冶金技术,2006,24(3):213-217.

4王德军,刘润茹.机械球磨方法合成稀土过渡族氧化物[J].长春大学学报,2003,13(1):31-33. 被引量:1

5沈元勋,肖志瑜,温利平,潘国如,李元元.粉末冶金高速压制技术的原理、特点及其研究进展[J].粉末冶金工业,2006,16(3):19-23. 被引量:33

6党新安,张政.选择性激光烧结制备多孔金属的工艺研究[J].陕西科技大学学报:自然科学版,2007,25(3):28-31. 被引量:3

7张寅,李小强,叶永权,李元元.高能球磨工艺对Cu-10Cr-0.5Al_2O_3组织与性能的影响[J].中国有色金属学报,2011,21(6):1328-1334. 被引量:3

8张伟,付俊凯,王辉,田铁磊,邢宏伟.高磷赤铁矿气化脱磷反应活化能研究[J].烧结球团,2015,40(4):12-15. 被引量:2

9张伟,王辉,邢宏伟,田铁磊,李杰.高磷鲕状赤铁矿气化脱磷动力学研究[J].矿冶工程,2015,35(3):79-82. 被引量:1

10陈立甲,查五生,吴开霞,吕先竞.机械球磨方法在表面薄膜涂层制备中的应用[J].粉末冶金技术,2014,32(1):64-67. 被引量:9

Basic Information:

DOI:

Chinese Library Classification Number:TF123.74[冶金工程—粉末冶金]

Citation Information:

This paper presents the results of synthesis of nanocomposite WC-Co powders at room temperature-by high-energy ball milling.Discussion is made on the powder property.

quote

GB/T 7714-2015 [1] NING Yang. Synthesis and Consolidation of Ball-milled Nanocomposite WC-Co Powders Compaction[J]. Rare Metals and Cemented Carbides, 2003(1): 53-56.
MLA [1] NING Yang. "Synthesis and Consolidation of Ball-milled Nanocomposite WC-Co Powders Compaction." Rare Metals and Cemented Carbides, no. 1, 2003, pp. 53-56.
APA [1] NING Yang. (2003). Synthesis and Consolidation of Ball-milled Nanocomposite WC-Co Powders Compaction. Rare Metals and Cemented Carbides(1), 53-56.
IEEE [1] NING Yang, "Synthesis and Consolidation of Ball-milled Nanocomposite WC-Co Powders Compaction," Rare Metals and Cemented Carbides, no. 1, pp. 53-56, 2003. keywords: {nanocomposite material;mechanical alloying;ball-milling compaction}