Application of Microwave in Sintering Wolframite Soda Mixture AITranslate
Abstract AITranslate
Applications of microwave in hard metal production and its raw materials treatment was briefly presented with emphasis placed on the microwave sintering of wolframite soda mixture.Optimal conditions for microwave treating of wolframite-soda mixture are soda content 30%,temperature 800-850℃,treatment time 20-30minutes.Water leaching gives a tungsten recovery of 99% in sodium tungstate solution.
KeyWords AITranslate
1[1]Meek TT,et al.Microwave sintering of Al2O3 - SiC whisker composites[C].US:Ceram Eng Sci Proc, 1987.861.
2[2]Das S,et al.Microwave sintering of cerarnics:can we save energy[J].Am Ceram Soc Bull, 1987,66(7) :1 093.
1艾光华,刘炯天.钨矿选矿药剂和工艺的研究现状及展望[J].矿山机械,2011,39(4):1-7. 被引量:32
2刘书祯,李杰,程艳明.微波加热在钨工业中的应用现状[J].稀有金属与硬质合金,2012,40(1):51-54. 被引量:3
3刘长军,吴昕.微波能工业应用研究进展[J].信息与电子工程,2012,10(4):451-455. 被引量:13
4曾青云,张勇,帅庚未.微波及超声波在钨冶金中的研究进展[J].有色金属科学与工程,2014,5(2):15-19. 被引量:2
5宋增凯,陈菓,彭金辉,赵巍,赵云飞,王占奎.微波加热技术在典型冶金工艺中的应用研究进展[J].矿冶,2014,23(3):57-63. 被引量:24
6韩战旗,熊亚东,李轩,张晓强,李红明,范建忠.微波干燥机在铜阳极泥烘干工艺上的应用实践[J].中国有色冶金,2020,49(6):49-52. 被引量:3
1廖崇蔚,陈潇杰,余泽,陈倩,刘长军.S波段大功率注入锁频磁控管的输出特性[J].太赫兹科学与电子信息学报,2021,19(4):688-691. 被引量:3
2艾光华,李晓波.微细粒黑钨矿选矿研究现状及展望[J].矿山机械,2011,39(10):89-96. 被引量:15
3辛亚淘,邓双丽.低品位白钨矿的浮选实践[J].矿山机械,2012,40(2):88-90. 被引量:6
4李英霞,王国生.广东某白钨矿选矿的试验研究[J].矿产保护与利用,2012,32(2):20-22. 被引量:2
5李英霞,王国生.某白钨矿回收工艺的试验研究[J].中国钨业,2012,27(4):23-25. 被引量:10
6曹占芳,钟宏,刘广义,王帅.我国矿产资源的特点及其加工技术与专业教学现状[J].稀有金属与硬质合金,2012,40(5):18-22. 被引量:2
7任传成,杨建国.浮选过程精矿品位软测量技术的研究进展[J].矿山机械,2013,41(8):8-12. 被引量:4
8谭鑫,范志鸿,陈定洲,刘龙利.钨矿螯合捕收剂的研究现状及展望[J].现代矿业,2013(9):1-5. 被引量:2
9章晓波,孙文,陈永明,沈崇.粉末轧制-叠层烧结法制备较厚93W-4.9Ni-2.1Fe高密度钨合金片材的研究[J].稀有金属与硬质合金,2013,41(5):28-31. 被引量:3
10黄万抚,张小冬.钨矿细泥选矿工艺发展[J].有色金属科学与工程,2013,4(5):54-57. 被引量:4
1株洲硬质合金厂APT的回收率达世界先进水平[J].中国钨业,1993,0(3):36-36.
2闫丽,王海北,曲志平.苏打烧结-酸浸法富集回收铂族金属[J].中国资源综合利用,2011,29(1):27-29. 被引量:6
3张启修,龚柏凡.我国钨湿法冶金技术进步概述[J].中国钨业,1992(2):17-21. 被引量:2
4李政.株洲硬质合金厂钨湿法冶炼技术改造取得迅速进展[J].中国钨业,1990(3):33-34.
Basic Information:
DOI:
Chinese Library Classification Number:TF046[冶金工程—冶金物理化学]
Citation Information:
Applications of microwave in hard metal production and its raw materials treatment was briefly presented with emphasis placed on the microwave sintering of wolframite soda mixture.Optimal conditions for microwave treating of wolframite-soda mixture are soda content 30%,temperature 800-850℃,treatment time 20-30minutes.Water leaching gives a tungsten recovery of 99% in sodium tungstate solution.
quote
| GB/T 7714-2015 | [1] ZHAO Qin-sheng. Application of Microwave in Sintering Wolframite Soda Mixture[J]. Rare Metals and Cemented Carbides, 2003(1): 51-52. |
| MLA | [1] ZHAO Qin-sheng. "Application of Microwave in Sintering Wolframite Soda Mixture." Rare Metals and Cemented Carbides, no. 1, 2003, pp. 51-52. |
| APA | [1] ZHAO Qin-sheng. (2003). Application of Microwave in Sintering Wolframite Soda Mixture. Rare Metals and Cemented Carbides(1), 51-52. |
| IEEE | [1] ZHAO Qin-sheng, "Application of Microwave in Sintering Wolframite Soda Mixture," Rare Metals and Cemented Carbides, no. 1, pp. 51-52, 2003. keywords: {microwave;sintering;wolframite} |