Preparation of Ce-Zr-O Compound Oxide Under Strong Base AITranslate
Abstract AITranslate
In the environment of strong base,ultrafine Ce-Zr-O powders were prepared.At the same time,the properties of the ultrafine powders were studied with aids of XRD,TG,laser particle sizer,specific surface measuring and testing instruments etc.The experiment showed that Zr-Ce-O particle size tends to become bigger with the increase of the zirconium content.Ethanol absolute is a good cleaning compound,the efficiency under the dry ball milling is better than that under the wet method milling.As a kind of reaction raw material,nitric salt is more suitable than chloride salt under the strong base.
KeyWords AITranslate
1北京师范大学无机化学教研室.无机化学(第三版)[M].北京:高等教育出版社,1992.117-118.
2吴君毅,高玮,张凡,古宏晨.小颗粒氧化铈制备过程中的团聚控制[J].稀土,2001,22(1):5-8. 被引量:22
3武金有.金属基复合材料及其应用[J].金属成形工艺,1992,10(6):265-269. 被引量:5
4Gerhardt- Anderson R, et al. Ionic conductivity of CeO2 with trivalent dopant of different ionic radii[J]. Solid State Ionics,1981,5:67.
5Maffei N, et al. Solid oxide fuel cells for ceria doped with gadolinium and praseodymium[ J ]. Solid State Ionics, 1998,107:547.
6Zedas M S,et al. High - temperature discontinuously reinfored aluminum[ J ]. JOM, 1991,8 : 28.
7Jloyd D.Particle reinforced aluminum and magnesium marie composties[ J]. International Materials, 1994.39( 1 ) : 1.
1阎忠君,王京刚,文明芬,陈靖,顾永万.不同沉淀剂对铈锆复合稀土氧化物性能的影响[J].北京化工大学学报:自然科学版,2005,32(3):9-12. 被引量:5
1谬文浩,赵明,余全伟,蔡黎,龚茂初,陈耀强.不同沉淀剂对Ce_(0.65)Zr_(0.35)O_2复合氧化物性能的影响[J].化学研究与应用,2007,19(6):657-659. 被引量:5
2申思,宋月清,汪礼敏,张景怀.沉淀剂对共沉淀法制备FeCo预合金粉末粒度与形貌的影响[J].稀有金属,2008,32(2):171-175. 被引量:5
3古映莹,冯圣生,李金林,顾向奎,王曼娟.Preparation of Mesoporous Ce_(0.5)Zr_(0.5)O_2 Mixed Oxide by Hydrothermal Templating Method[J].稀土学报:英文版,2007,25(6):710-714. 被引量:1
4李岩峰,李梅,柳召刚,胡艳宏,付海.铈锆固溶体掺杂改性的研究进展[J].稀土,2009,30(5):78-83. 被引量:9
5黄海凤,陈晓,顾蕾,徐琴琪,占林军,卢晗锋.柴油车DOC催化剂Pt/CeZrO_2载体的制备及影响[J].化工学报,2017,68(4):1390-1397. 被引量:6
1王会娟.瓦斯灰中氧化锌的强碱浸取及测定[J].冶金分析,2005,25(1):89-90. 被引量:1
2陈金清,朱志全,陈传林.W/O微乳液对强碱体系中钒的萃取[J].有色金属:冶炼部分,2010(4):29-32. 被引量:6
3王德全.强碱分离氟盐置换纯铜滴定法测定铁矿石中Al_2O_3[J].理化检验:化学分册,2003,39(5):301-301. 被引量:1
4王世伟,李瑛,王林山.土壤中侵蚀性离子对X70钢的侵蚀作用研究[J].腐蚀科学与防护技术,2005,17(2):98-100. 被引量:9
5刘海飞,许根国,方淑媛.用氯化盐和硫酸盐电解液制备电解镍粉[J].有色金属:冶炼部分,1999(4):36-38. 被引量:4
6赵坚,丁成芳,胡海南,赵秦生.萃取法从铜阳极泥制备的碲化铜中回收碲[J].稀有金属与硬质合金,2012,40(4):1-3. 被引量:9
7黄海辉,王云.提金渣氯化焙烧提取金银的试验[J].有色金属:冶炼部分,2009(6):46-48. 被引量:13
8张溅波,吴轩,缪辉俊,周丽.熔盐氯化废渣回收氯化盐及其促进钛铁矿盐酸浸出研究[J].钢铁钒钛,2015,36(4):48-52. 被引量:3
9李明建.洗涤剂用 4A 沸石合成的晶化导向剂制备及应用研究[J].广东工业大学学报,1997,0(3):34-37. 被引量:4
10岳梅,张娜,崔梅生,龙志奇,黄小卫.H_2O_2氧化对铈锆复合氧化物性能的影响研究[J].稀有金属材料与工程,2014,43(12):3109-3113. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TF123.25[冶金工程—粉末冶金]
Citation Information:
In the environment of strong base,ultrafine Ce-Zr-O powders were prepared.At the same time,the properties of the ultrafine powders were studied with aids of XRD,TG,laser particle sizer,specific surface measuring and testing instruments etc.The experiment showed that Zr-Ce-O particle size tends to become bigger with the increase of the zirconium content.Ethanol absolute is a good cleaning compound,the efficiency under the dry ball milling is better than that under the wet method milling.As a kind of reaction raw material,nitric salt is more suitable than chloride salt under the strong base.
quote
| GB/T 7714-2015 | [1] HAO Shi-you, LI Jin, ZHOU Xue-zhen, et al. Preparation of Ce-Zr-O Compound Oxide Under Strong Base[J]. Rare Metals and Cemented Carbides, 2003(2): 1-4. |
| MLA | [1] HAO Shi-you, et al., "Preparation of Ce-Zr-O Compound Oxide Under Strong Base." Rare Metals and Cemented Carbides, no. 2, 2003, pp. 1-4. |
| APA | [1] HAO Shi-you, LI Jin, ZHOU Xue-zhen, & LI Yong-xiu. (2003). Preparation of Ce-Zr-O Compound Oxide Under Strong Base. Rare Metals and Cemented Carbides(2), 1-4. |
| IEEE | [1] HAO Shi-you, LI Jin, ZHOU Xue-zhen, and LI Yong-xiu, "Preparation of Ce-Zr-O Compound Oxide Under Strong Base," Rare Metals and Cemented Carbides, no. 2, pp. 1-4, 2003. keywords: {strong base;ultrafine Zr-Ce-O powder;property} |