Finite element modeling and experimental study on bending and vibration of laminated stiffened glass fiber/polyester composite plates AITranslate
Abstract AITranslate
In this paper, free vibration and bending failure of laminated stiffened glass fiber/polyester composite plates with laminated open section (rectangular or T-shaped) and closed section (hat shaped) of stiffeners have been studied by finite element method and experiment. A 9-noded isoparametric element with 9 degrees of freedom per node is developed for the plates. The stiffener element is a 3-noded isoparametric beam element with 5 degrees of freedom per node and the stiffeners can be positioned anywhere within the plate element. The natural frequencies of the laminated stiffened plates are determined experimentally by Dewebook device and DasyLab 7.0 software. The results calculated by computational model for above plates under different boundary conditions are in good agreement with experiments. The failure problems of these stiffened glass fiber/polyester composite plates are also investigated.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.commatsci.2010.05.011
Chinese Library Classification Number:
Citation Information:
In this paper, free vibration and bending failure of laminated stiffened glass fiber/polyester composite plates with laminated open section (rectangular or T-shaped) and closed section (hat shaped) of stiffeners have been studied by finite element method and experiment. A 9-noded isoparametric element with 9 degrees of freedom per node is developed for the plates. The stiffener element is a 3-noded isoparametric beam element with 5 degrees of freedom per node and the stiffeners can be positioned anywhere within the plate element. The natural frequencies of the laminated stiffened plates are determined experimentally by Dewebook device and DasyLab 7.0 software. The results calculated by computational model for above plates under different boundary conditions are in good agreement with experiments. The failure problems of these stiffened glass fiber/polyester composite plates are also investigated.
quote
| GB/T 7714-2015 | [1] Tran Ich Thinh, Tran Huu Quoc. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.05.011. |
| MLA | [1] Tran Ich Thinh, and Tran Huu Quoc. Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.05.011. |
| APA | [1] Tran Ich Thinh, & Tran Huu Quoc. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.05.011 |
| IEEE | [1] Tran Ich Thinh and Tran Huu Quoc, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.05.011. |