Abstract AITranslate
With the development of spintronics, the search for heterostructures with Curie temperatures higher than room temperature has become a top priority for all researchers. We calculated the electronic and magnetic properties of heterostructures constructed by VN with ferromagnetic half-metallic properties and Ga2O2 with nonmagnetic semiconducting properties using first-principles calculations. Our results show that the VN/Ga2O2 heterostructure not only has a Curie temperature well above room temperature but also has a 100% spin filtering effect. In addition, the ability to maintain perpendicular magnetic anisotropy (PMA) at −5 to 5% biaxial strain is an essential point for achieving high-density information storage. The spin-valve structure constructed by combining a monolayer VN and a monolayer Ga2O2 according to the ferromagnetic/nonmagnetic/ferromagnetic structure not only has the same 100% spin filtering effect and a Curie temperature well above room temperature but also the easy magnetization axis direction still points perfectly in the out-of-plane direction. Our study shows that the VN/Ga2O2 heterostructure and the VN/Ga2O2/VN spin-valve heterostructure are promising materials for low-dimensional spintronic devices.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c01465
Chinese Library Classification Number:
Citation Information:
With the development of spintronics, the search for heterostructures with Curie temperatures higher than room temperature has become a top priority for all researchers. We calculated the electronic and magnetic properties of heterostructures constructed by VN with ferromagnetic half-metallic properties and Ga2O2 with nonmagnetic semiconducting properties using first-principles calculations. Our results show that the VN/Ga2O2 heterostructure not only has a Curie temperature well above room temperature but also has a 100% spin filtering effect. In addition, the ability to maintain perpendicular magnetic anisotropy (PMA) at −5 to 5% biaxial strain is an essential point for achieving high-density information storage. The spin-valve structure constructed by combining a monolayer VN and a monolayer Ga2O2 according to the ferromagnetic/nonmagnetic/ferromagnetic structure not only has the same 100% spin filtering effect and a Curie temperature well above room temperature but also the easy magnetization axis direction still points perfectly in the out-of-plane direction. Our study shows that the VN/Ga2O2 heterostructure and the VN/Ga2O2/VN spin-valve heterostructure are promising materials for low-dimensional spintronic devices.
quote
| GB/T 7714-2015 | [1] Qianqian Wu, Jin Wang, Ting Zhi, et al. ACS Applied Electronic Materials, 2024(6). DOI:10.1021/acsaelm.3c01465. |
| MLA | [1] Qianqian Wu, et al., ACS Applied Electronic Materials, no. 6, 2024, https://doi.org/10.1021/acsaelm.3c01465. |
| APA | [1] Qianqian Wu, Jin Wang, Ting Zhi, Zhikuo Tao, Pengfei Shao, Qing Cai, Guofeng Yang, Junjun Xue, Dunjun Chen, & Rong Zhang. (2024). ACS Applied Electronic Materials(6). https://doi.org/10.1021/acsaelm.3c01465 |
| IEEE | [1] Qianqian Wu, Jin Wang, Ting Zhi, Zhikuo Tao, Pengfei Shao, Qing Cai, Guofeng Yang, Junjun Xue, Dunjun Chen, and Rong Zhang, ACS Applied Electronic Materials, no. 6, 2024, doi: 10.1021/acsaelm.3c01465. keywords: {spin valve spin polarization efficiency magnetic anisotropy energy van der Waals heterostructures Curie temperature} |