Vanadium Extraction from Carbonaceous Shale by Blank Roasting-Pressurized High Temperature Alkali Leaching AITranslate
Abstract AITranslate
Vanadium was extracted from carbonaceous shale by blank roasting-pressurized high temperature alkali leaching.The effects of calcine grain size,liquid to solid ratio,leaching time and temperature,and alkali dosage on vanadium leaching rate were investigated.The results show that when the process of blank roasting-pressurized high temperature alkali leaching is applied in treating with carbonaceous shale,the vanadium leaching rate is satisfactory under the conditions of 3% NaOH dosage,195 ℃ leaching temperature and 2 h leaching time.Compared with blank roasting-atmospheric alkali leaching,the applied process has the advantages of less alkali consumption,high vanadium leaching rate and so on.
KeyWords AITranslate
1鲁兆伶.用酸法从石煤中提取五氧化二钒的试验研究与工业实践[J].湿法冶金,2002,21(4):175-183. 被引量:139
2潘勇,于吉顺,吴红丹.石煤提钒的工艺评价[J].矿业快报,2007,23(4):10-13. 被引量:37
3申小清,杨林莎,许闽,李中军.从含钒酸浸液中回收钒的工艺研究[J].河南化工,1999,18(1):16-18. 被引量:6
4谭爱华.某石煤钒矿空白焙烧-碱浸提钒工艺研究[J].湖南有色金属,2008,24(1):24-26. 被引量:34
5戴文灿,朱柒金,陈庆邦,刘如意,孙水裕.石煤提钒综合利用新工艺的研究[J].有色金属:选矿部分,2000(3):15-17. 被引量:44
6肖松文,梁经冬.钠化焙烧提钒机理研究的新进展[J].矿冶工程,1994,14(2):53-55. 被引量:22
7何东升,冯其明,张国范,欧乐明,卢毅屏,邵延海.碱法从石煤中浸出钒试验研究[J].有色金属:冶炼部分,2007(4):15-17. 被引量:33
8彭声谦,许国镇.石煤提钒中钠盐的作用[J].西南工学院学报,1998,13(1):9-12. 被引量:17
9范必威,林海玲.方山口石煤提钒焙烧工艺研究[J].湿法冶金,2001,20(2):79-83. 被引量:25
10邹晓勇,彭清静,欧阳玉祝,田仁国.高硅低钙钒矿的钙化焙烧过程[J].过程工程学报,2001,1(2):189-192. 被引量:59
1白桦,李阳.石煤提钒工艺中的新型焙烧装置[J].有色冶金节能,2012,27(3):29-30. 被引量:1
2白桦.新型流态化石煤焙烧装置[J].工程设计与研究(长沙),2012(1):1-3.
3冯雅丽,蔡震雷,李浩然,汪平,刘欣伟,杨志超.循环流态化焙烧加压浸出从极难浸石煤中提取钒[J].中国有色金属学报,2012,22(7):2052-2060. 被引量:6
4邢学永,万洪强,宁顺明,佘宗华,吴江华.某石煤矿浓酸熟化两段逆流浸出钒的研究[J].有色金属:冶炼部分,2013(6):26-29. 被引量:15
5邱伟佳,魏昶,邓志敢,李旻廷,李兴彬,张帆.石煤发电飞灰碱浸提钒工艺[J].过程工程学报,2014,14(3):421-426. 被引量:2
6汪劲鹏,张一敏,黄晶,袁益忠.微波强化石煤提钒酸浸工艺的研究[J].有色金属:冶炼部分,2015(10):54-57. 被引量:6
7唐丁玲,宋浩,刘丁丁,吴卫红,郑成航,高翔.废弃脱硝催化剂碱浸提取钒和钨的浸出动力学研究[J].环境工程学报,2017,11(2):1093-1100. 被引量:12
8钟楚彬,刘耀驰.石煤复合碱循环浸出提钒研究[J].矿冶工程,2017,37(4):98-103. 被引量:7
1邢学永,宁顺明.石煤发热值与提钒工艺选择[J].中国有色冶金,2013,42(6):28-31. 被引量:3
2李婕,刘旭恒.碱法从石煤选矿钒精矿中提取五氧化二钒中间试验[J].有色金属:冶炼部分,2014(2):31-34. 被引量:4
3邱伟佳,魏昶,邓志敢,李旻廷,李兴彬,张帆.石煤发电飞灰碱浸提钒工艺[J].过程工程学报,2014,14(3):421-426. 被引量:2
4刘娟,张一敏,黄晶,刘涛,黄献宝,马浩.机械活化强化石煤酸浸提钒的动力学研究[J].有色金属:冶炼部分,2014(7):27-31. 被引量:5
5胡杨甲,张一敏.钙含量对含钒页岩钠盐焙烧-水浸提钒的影响[J].有色金属:冶炼部分,2014(9):34-38. 被引量:9
6万洪强,宁顺明,佘宗华,邢学永,王文娟,吴江华.石煤钒矿浓酸熟化浸出工艺优化[J].稀有金属,2014,38(5):880-886. 被引量:6
7齐兆树,李青刚.从碱性含钒溶液中萃取钒的研究[J].有色金属:冶炼部分,2014(10):43-48. 被引量:3
8蒋谋锋,张一敏,包申旭,杨晓.含钒石煤钒钾镁硫酸浸出相关性研究[J].有色金属:冶炼部分,2014(11):34-38. 被引量:8
9刘涛,胡鹏程,张一敏,袁益忠.含钒石煤微波焙烧提钒试验研究[J].有色金属:冶炼部分,2015(1):46-49. 被引量:15
10黄献宝,陈铁军,张一敏,马浩,李道,汪劲鹏.石煤流态化焙烧—酸浸提钒工艺研究[J].有色金属:冶炼部分,2014(12):19-23. 被引量:4
1薛光,于永江.边磨边浸氰化提高金、银浸出率的试验研究[J].黄金,2010(4):42-43. 被引量:8
2卢友中,曾青云,陈庆根.微波辅助碱分解低品位黑(白)钨精矿[J].矿产综合利用,2009(5):20-23. 被引量:9
3张邦胜,蒋开喜,王海北.全湿法处理钼镍矿的新工艺[J].四川有色金属,2012(3):26-28. 被引量:2
4伍莺,陈冬英,欧阳红,周洁英.从稀土抛光粉废料中回收稀土试验研究[J].湿法冶金,2015,34(5):398-401. 被引量:4
5库建刚,王安理,张文彬.低品位氧化钼精矿常压碱浸试验研究[J].中国有色冶金,2009,38(5):59-62. 被引量:5
6隋丽丽,翟玉春.从高钛渣沉钛液中提铝[J].矿冶,2015,24(3):38-41.
7李政锋.氧压碱浸镍钼矿提钼试验研究[J].湖南有色金属,2017,33(1):30-33. 被引量:2
8李培佑,张能成,林喜斌.从废催化剂中回收钼的工艺流程研究[J].中国钼业,1999,23(1):16-21. 被引量:10
9刘振楠.含钨萤石中矿高压浸出钨、铷试验研究[J].湖南有色金属,2016,32(2):33-35.
10徐志峰,月日辉,严康,王成彦.复杂高硅钴白合金碱焙烧脱硅预处理[J].中国有色金属学报,2012,22(10):2916-2923. 被引量:7
Basic Information:
DOI:
Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]
Citation Information:
Vanadium was extracted from carbonaceous shale by blank roasting-pressurized high temperature alkali leaching.The effects of calcine grain size,liquid to solid ratio,leaching time and temperature,and alkali dosage on vanadium leaching rate were investigated.The results show that when the process of blank roasting-pressurized high temperature alkali leaching is applied in treating with carbonaceous shale,the vanadium leaching rate is satisfactory under the conditions of 3% NaOH dosage,195 ℃ leaching temperature and 2 h leaching time.Compared with blank roasting-atmospheric alkali leaching,the applied process has the advantages of less alkali consumption,high vanadium leaching rate and so on.
quote
| GB/T 7714-2015 | [1] KE Zhao-hua, LI Qing-gang, CENG Cheng-wei. Vanadium Extraction from Carbonaceous Shale by Blank Roasting-Pressurized High Temperature Alkali Leaching[J]. Rare Metals and Cemented Carbides, 2011(2): 10-13. |
| MLA | [1] KE Zhao-hua, et al., "Vanadium Extraction from Carbonaceous Shale by Blank Roasting-Pressurized High Temperature Alkali Leaching." Rare Metals and Cemented Carbides, no. 2, 2011, pp. 10-13. |
| APA | [1] KE Zhao-hua, LI Qing-gang, & CENG Cheng-wei. (2011). Vanadium Extraction from Carbonaceous Shale by Blank Roasting-Pressurized High Temperature Alkali Leaching. Rare Metals and Cemented Carbides(2), 10-13. |
| IEEE | [1] KE Zhao-hua, LI Qing-gang, and CENG Cheng-wei, "Vanadium Extraction from Carbonaceous Shale by Blank Roasting-Pressurized High Temperature Alkali Leaching," Rare Metals and Cemented Carbides, no. 2, pp. 10-13, 2011. keywords: {vanadium extraction from carbonaceous shale;blank roasting;pressurized high temperature alkali leaching;vanadium leaching rate} |