Preparation of Lithium-ion Battery-Grade Cobalt Sulfate by Solvent Extraction AITranslate

Hunan Rare Earth Metal Material Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Research is made on the process for preparation of lithium-ion battery-grade cobalt sulfate from crude cobalt hydroxide.And the process flowsheet is as follows:impurity removal by preferential dissolution with dilute sulfuric acid,reducing leaching,Fe,Mn and As removal by oxide precipitation,Ca and Mg removal by fluoride precipitation,deep purification and impurity removal by extraction with P204,Ni and Co separation and Na removal by extraction with P507.The electronic-grade cobalt sulfate suitable for producing lithium cobalt oxide has been obtained through the above process.

KeyWords AITranslate

cobalt hydroxide leaching purification extraction cobalt sulfate

1习小明,黄焯枢.一种制备锂钴氧化合物(LiCoO2)的湿化学方法[P].中国专利:CN1357491A,2002-07-10.

2周炳珍.用P204和P507脱除含钴废料中的杂质生产高纯度氯化钴[J].有色金属:冶炼部分,2002(6):16-17. 被引量:13

1王胜.离心萃取器协同萃取分离镍钴[J].有色金属工程,2014,4(2):42-44. 被引量:1

2张悦,何丽杰,张守庆,史春薇,杨占旭.废旧锂离子电池的回收技术现状及展望[J].电源技术,2018,42(8):1230-1232. 被引量:5

3张中华.高纯氯化铵产品质量的影响因素及消除措施[J].纯碱工业,2019,0(4):21-23.

4彭志宏,何芳,贾浩,李小斌,周秋生,齐天贵,刘桂华.从硫酸钴水溶液中制备球形碳酸钴(英文)[J].中国有色金属学报:英文版,2020,30(2):509-517. 被引量:2

1梁新成,张勉.电动车退役锂电池回收研究[J].电源技术,2020,44(5):771-773. 被引量:3

2李之钦,庄绪宁,宋小龙,李斐,李英顺,顾卫华,白建峰.废锂离子电池正极材料的火法资源化技术研究进展[J].环境工程,2021,39(4):115-122. 被引量:9

3杜晗,陈立群,黄苏勇.液相沉淀法制备超细碳酸钴的工艺研究[J].生物化工,2022,8(1):48-50.

4李棉,程琍琍,杨幼明,牛飞,张小林,刘东辉.锂离子电池回收利用技术研究进展[J].稀有金属,2022,46(3):349-366. 被引量:10

5朱慧琴.废旧锂离子电池中钴、锂离子回收的最优条件选择[J].山东化工,2022,51(18):16-19.

6宋晨杰,黄凯.类球形草酸钴沉淀粉末的制备研究[J].硬质合金,2023,40(1):31-41.

7肖忠良,尹碧露,宋刘斌,匡尹杰,赵亭亭,刘成,袁荣耀.废旧锂离子电池回收工艺研究进展及其安全风险分析[J].化工学报,2023,74(4):1446-1456.

8陈政,柴慧森,邵鸿媚,崔勇.废旧锂离子电池绿色环保回收流程研究[J].辽宁化工,2023,52(8):1145-1148.

1陈江英,李翔晟.微合金化元素Ce对AZ91镁合金显微组织和力学性能的影响[J].铸造技术,2014,35(7):1441-1443. 被引量:4

2含CO的铝电解着色液的再生[J].电镀与精饰,2003,25(4):44-44.

3邹智.原子吸收分光光度法测定粗制氢氧化钴中的镁[J].湖南有色金属,2015,31(6):78-80. 被引量:2

4杨明波,程亮,潘复生.Effects of calcium addition on as-cast microstructure and mechanical properties of Mg-5Zn-5Sn alloy[J].中国有色金属学报:英文版,2010,20(5):769-775. 被引量:9

5崔仲鸣,陈青秋,赫青山,王静静,冯创举.镀液成分对高精度电镀金刚石工具镀层机械性能的影响[J].制造业自动化,2015,37(17):60-63. 被引量:2

6沈盛军,杨淼,张岚.Gd合金化对汽车发动机用AM50合金组织和性能的影响[J].特种铸造及有色合金,2016,36(3):313-316. 被引量:1

7元鹏鹏,李能和,樊自田.稀土Ce对管线钢在混凝土环境中腐蚀行为的影响[J].铸造技术,2016,37(7):1342-1345. 被引量:1

8覃奇贤.2005110 电镀镍-钴合金[J].电镀与精饰,2005,27(1):54-54. 被引量:1

9王莉萍,吴玉程,李云,张勇,李广海.化学镀Co-B合金(Ⅰ)[J].电镀与精饰,2004,26(6):1-4. 被引量:2

10李辉,张洁,刘相法,边秀房,马家骥.铝合金液直流电除氢除钠的试验研究[J].铸造,1995,44(12):1-4. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TG804.2[金属学及工艺—公差测量技术]

Citation Information:

Research is made on the process for preparation of lithium-ion battery-grade cobalt sulfate from crude cobalt hydroxide.And the process flowsheet is as follows:impurity removal by preferential dissolution with dilute sulfuric acid,reducing leaching,Fe,Mn and As removal by oxide precipitation,Ca and Mg removal by fluoride precipitation,deep purification and impurity removal by extraction with P204,Ni and Co separation and Na removal by extraction with P507.The electronic-grade cobalt sulfate suitable for producing lithium cobalt oxide has been obtained through the above process.

quote

GB/T 7714-2015 [1] SU Hua. Preparation of Lithium-ion Battery-Grade Cobalt Sulfate by Solvent Extraction[J]. Rare Metals and Cemented Carbides, 2011(2): 14-17.
MLA [1] SU Hua. "Preparation of Lithium-ion Battery-Grade Cobalt Sulfate by Solvent Extraction." Rare Metals and Cemented Carbides, no. 2, 2011, pp. 14-17.
APA [1] SU Hua. (2011). Preparation of Lithium-ion Battery-Grade Cobalt Sulfate by Solvent Extraction. Rare Metals and Cemented Carbides(2), 14-17.
IEEE [1] SU Hua, "Preparation of Lithium-ion Battery-Grade Cobalt Sulfate by Solvent Extraction," Rare Metals and Cemented Carbides, no. 2, pp. 14-17, 2011. keywords: {cobalt hydroxide;leaching;purification;extraction;cobalt sulfate}