Technical Study on Phosphorus Removal with Chromium Nitrate from Ammonium Tungstate Solution AITranslate

School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The chromium nitrate precipitation method was used to deeply remove phosphorus from ammonium tungstate solution.The effects on phosphorus removal were systematically investigated of chromium nitrate addition,reaction temperature,reaction time,ammonium tungstate solution pH and initial phosphorus concentration.The results show that under the optimal conditions of the chrome addition of 3 times the theoretical quantity,temperature of 55 ℃,time of 120 min,ammonium tungstate solution pH of 9.81 and initial phosphorus concentration of 37.4 mg/L,the residual phosphorus concentration in ammonium tungstate solution after phosphorus removal is 14.95 g/L,which meets the requirement for preparation of APT-0 grade products.

KeyWords AITranslate

ammonium tungstate solution chromium nitrate precipitation phosphorus removal

1陈树茂,郭永忠.离子交换法处理仲钨酸铵结晶母液试验与实践[J].中国钨业,2001,16(3):22-24. 被引量:14

2王建华.磷酸铵镁结晶法除磷工艺在工业废水处理中的应用[J].化学工业与工程技术,2013,34(5):41-44. 被引量:5

3姚涛,蔡伟民,李龙海.磷酸铵镁法处理含氮磷废水研究进展[J].中国给水排水,2005,21(2):31-33. 被引量:38

4孙体昌,崔志广,黄国忠,李维,常江,江冠男.用沉淀气浮法从回流液中回收氨氮和磷的研究[J].工业水处理,2005,25(3):45-48. 被引量:16

5张继华.化学沉淀法处理磷化废水[J].工业水处理,2000,20(5):43-44. 被引量:24

6徐丰果,罗建中,凌定勋.废水化学除磷的现状与进展[J].工业水处理,2003,23(5):18-20. 被引量:151

7林平,颜志伟.废水除磷工艺发展现状[J].中小企业管理与科技,2015(26):236-236. 被引量:2

8余敏露,何思思,罗杨春,胡如意,M.S.Le.浅谈水体除磷的方法研究进展[J].中国科技博览,2016,0(9):389-390. 被引量:3

9邱维,张智.城市污水化学除磷的探讨[J].重庆环境科学,2002,24(2):81-84. 被引量:96

10万林生,赖星任,黄海,赵立夫,章秋霖.仲钨酸铵结晶过程掺Cr制备APT的物化性能研究[J].稀有金属与硬质合金,2015,43(5):1-3 15. 被引量:3

1黄超,宫晨彪,徐国钻,刘德刚,贺山明,梁勇.离子交后液回收钨废水中MnO除磷的研究[J].中国钨业,2020,35(2):45-50. 被引量:1

1戴林明,彭玉玲.Ca(OH)_(2)-FeSO_(4)混凝沉淀法脱除钨冶炼废水中氟、磷、砷的研究[J].中国钨业,2021,36(2):48-52. 被引量:4

1汪流培,张贵清,关文娟,曾理,周钦,夏允.从含钒钨酸铵溶液中萃取分离微量钒的研究[J].稀有金属与硬质合金,2017,45(4):1-5. 被引量:1

2马莉,刘双.单克隆抗体纯化方法比较论述[J].中国畜牧兽医文摘,2018,34(1):75-75. 被引量:5

3廖添,宋亭,杨定乔,吕梅香,曾和平.Fe、Cr共掺杂TiO_2纳米球增强光催化制氢[J].华南师范大学学报:自然科学版,2017,49(5):35-41. 被引量:8

4李小玲,肖红新,王芳.铅试金法测定硅氧烷铂配合物中的铂[J].贵金属,2017,38(4):66-68. 被引量:3

5杨青青,杨帆.乳制品检测前处理中沉淀蛋白方法的探讨[J].科学时代:下,2010(5X):30-30. 被引量:1

6周旋,吴昊,张椿.卵磷脂提取、分离纯化的研究进展[J].饮料工业,2017,20(6):61-65. 被引量:3

7沈益秀,吕新宇,邱滔.Cu0.5Zn0.5Cr0.5Al1.5O4尖晶石的制备及其催化性能[J].精细化工,2017,34(10):1148-1152.

8张秀飞,白海瑞,郭冬青.热轧双相钢DP600氧化物缺陷分析与控制[J].包钢科技,2018,44(1):54-57.

9陈文溪,郭一令.络合电镀废水处理的研究[J].环境保护与循环经济,2017,37(10):32-35. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF841.1[冶金工程—有色金属冶金]

Citation Information:

The chromium nitrate precipitation method was used to deeply remove phosphorus from ammonium tungstate solution.The effects on phosphorus removal were systematically investigated of chromium nitrate addition,reaction temperature,reaction time,ammonium tungstate solution pH and initial phosphorus concentration.The results show that under the optimal conditions of the chrome addition of 3 times the theoretical quantity,temperature of 55 ℃,time of 120 min,ammonium tungstate solution pH of 9.81 and initial phosphorus concentration of 37.4 mg/L,the residual phosphorus concentration in ammonium tungstate solution after phosphorus removal is 14.95 g/L,which meets the requirement for preparation of APT-0 grade products.

quote

GB/T 7714-2015 [1] HU Xiao-mi, WAN Lin-sheng, QIU Ya-ming, et al. Technical Study on Phosphorus Removal with Chromium Nitrate from Ammonium Tungstate Solution[J]. Rare Metals and Cemented Carbides, 2018(1): 1-4.
MLA [1] HU Xiao-mi, et al., "Technical Study on Phosphorus Removal with Chromium Nitrate from Ammonium Tungstate Solution." Rare Metals and Cemented Carbides, no. 1, 2018, pp. 1-4.
APA [1] HU Xiao-mi, WAN Lin-sheng, QIU Ya-ming, LIU Peng, PAN Ming-ran, & YANG Liang. (2018). Technical Study on Phosphorus Removal with Chromium Nitrate from Ammonium Tungstate Solution. Rare Metals and Cemented Carbides(1), 1-4.
IEEE [1] HU Xiao-mi, WAN Lin-sheng, QIU Ya-ming, LIU Peng, PAN Ming-ran, and YANG Liang, "Technical Study on Phosphorus Removal with Chromium Nitrate from Ammonium Tungstate Solution," Rare Metals and Cemented Carbides, no. 1, pp. 1-4, 2018. keywords: {ammonium tungstate solution;chromium nitrate;precipitation;phosphorus removal}