daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research on Process of Rare Earth Recovery from Rare Earth Electrolysis Slag by Roasting with Sodium Hydroxide AITranslate

School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In view of low efficiency of rare earth recovery from rare earth molten salt electrolysis slag in fluoride salt system,a novel technology of roasting with sodium hydroxide-selective leaching with hydrochloric acid was proposed.The effects were systematically investigated of roasting temperature,roasting time,sodium hydroxide dosage,hydrochloric acid concentration,liquid-solid ratio,leaching temperature and leaching time on rare earth recovery from the slag.The leaching rate of rare earth is as high as 99.22% under the following conditions:roasting temperature of 600 ℃,roasting time of 1.5 h,the mass ratio of sodium hydroxide to the slag of 0.8∶1,hydrochloric acid concentration of 2 mol/L,liquid to solid ratio of 8∶1,leaching temperature of 40 ℃ and leaching time of 15 min.

KeyWords AITranslate

rare earth molten salt electrolysis slag fluoride salt system sodium hydroxide roasting selective leaching with hydrochloric acid

1李新市.中国稀土战略的几个热点问题[J].理论研究,2011(3):46-49. 被引量:6

2李建.白云鄂博稀土资源的利用现状、主要问题及解决对策[J].山西师范大学学报:自然科学版,2008,22(z1):76-77. 被引量:9

3张忠,李振宏.国家实施稀土资源战略储备的意义及方式建议[J].稀土信息,2010,16(3):32-33. 被引量:13

4许涛,彭会清,林忠,吕保义.稀土固体废物的成因、成分分析及综合利用[J].稀土,2010,31(2):34-39. 被引量:25

5李健靓,王瑶,张欣.稀土镁基贮氢合金的研究进展[J].金属功能材料,2013,20(4):49-53. 被引量:9

6马建波,湛永钟,周卫平,黄国瑞,刘佑良,林栽汉.磁热效应和室温稀土磁制冷材料研究现状[J].材料导报,2008,22(11):34-37. 被引量:9

7天津包钢稀土研究院“稀土光谱转换材料应用研发技术”获得突破性进展[J].稀土,2015,0(2):85-85. 被引量:1

8稀土永磁材料在新能源领域潜力巨大[J].中国有色冶金,2015,44(3):40-40. 被引量:1

9董方,蔡国君.铈对202不锈钢夹杂物形态和力学性能的影响[J].中国稀土学报,2010,28(3):372-378. 被引量:5

10梁勇,吕江涛,林如丹,刘玉城,廖春发.Dy_2O_3(Dy)-HCl-CaF_2-H_2O体系热力学研究[J].湿法冶金,2016,35(6):469-472. 被引量:2

1赖耀斌,徐建兵,李忠岐,梁鑫,陈东英.真空蒸馏法综合回收稀土熔盐电解渣工艺研究[J].真空科学与技术学报,2021,41(4):332-335. 被引量:3

2赖耀斌,徐建兵,李忠岐,梁鑫,陈冬英.从蒸馏渣中回收稀土工艺研究[J].有色金属:冶炼部分,2021(9):80-83. 被引量:1

3佟志芳,温皓,胡晓飞.稀土电解熔盐渣焙烧产物酸浸提取稀土、锂和氟[J].有色金属科学与工程,2022,13(4):141-147.

4钟立钦,叶春林,廖良芳,曹磊,熊仕显,廖春发.稀土熔盐电解渣回收利用技术现状及展望[J].稀有金属与硬质合金,2023,51(2):20-25.

5梁颜祯,邱廷省,邓建红,朱冬梅,吴昊,王淼.稀土熔盐渣中有价金属综合回收技术研究现状及进展[J].稀土,2023,44(2):13-23.

1佟志芳,温皓,胡晓飞.稀土电解熔盐渣焙烧产物酸浸提取稀土、锂和氟[J].有色金属科学与工程,2022,13(4):141-147.

2钟立钦,叶春林,廖良芳,曹磊,熊仕显,廖春发.稀土熔盐电解渣回收利用技术现状及展望[J].稀有金属与硬质合金,2023,51(2):20-25.

3李迅,贾艳虹,窦强,杨洋.放射性废盐的真空蒸馏净化技术研究[J].无机盐工业,2023,55(7):97-102.

1王海辉,逄启寿,郜飘飘.稀土电解槽温度场的模拟分析与研究[J].稀有金属与硬质合金,2017,45(4):12-15. 被引量:10

2范亚卓,邓斌,穆天柱,赵三超,苗庆东,谢波,朱福兴.熔盐电解制备骨骼3D打印用非球形高纯钛粉[J].钢铁钒钛,2017,38(6):43-46. 被引量:1

3唐浩,任一鸣,邵浪,钟毅,高瑞.熔盐电解法乏燃料干法后处理技术研究进展[J].核化学与放射化学,2017,39(6):385-396. 被引量:13

4苏严.氟盐体系稀土电解炉筑炉工艺改进[J].铜业工程,2017(5):51-53.

5刘勇,刘珍珍,刘牡丹,周吉奎,马致远.稀有金属富集渣中稀土和钪的提取[J].有色金属:冶炼部分,2017(12):40-42. 被引量:2

6于雅樵,刘玉宝,陈国华,袁晓鸣,高日增,张文灿.液态阴极熔盐电解法制备钇锌合金热力学分析[J].包钢科技,2018,44(1):72-74.

7梁红玉,李建中,田彦文,邹赫,胡绍争.不同g-C_3N_4/WO_3异质结材料的制备及其光催化性能研究[J].石油化工高等学校学报,2018,31(1):23-29. 被引量:3

8刘明月.食用植物油中残留溶剂测定方法的优化[J].食品安全导刊,2018,0(3):95-95.

9芬兰新技术可从电子垃圾中回收稀土等元素[J].家电科技,2018(1):11-11.

10焦芸芬,王旭,廖春发,孙强超,蔡伯清,汤浩.Na3AlF6-AlF3-LiF-MgF2-Al2O3-Sm2O3熔盐体系表面张力的研究[J].稀有金属,2018,42(1):75-82. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TF845[冶金工程—有色金属冶金]

Citation Information:

In view of low efficiency of rare earth recovery from rare earth molten salt electrolysis slag in fluoride salt system,a novel technology of roasting with sodium hydroxide-selective leaching with hydrochloric acid was proposed.The effects were systematically investigated of roasting temperature,roasting time,sodium hydroxide dosage,hydrochloric acid concentration,liquid-solid ratio,leaching temperature and leaching time on rare earth recovery from the slag.The leaching rate of rare earth is as high as 99.22% under the following conditions:roasting temperature of 600 ℃,roasting time of 1.5 h,the mass ratio of sodium hydroxide to the slag of 0.8∶1,hydrochloric acid concentration of 2 mol/L,liquid to solid ratio of 8∶1,leaching temperature of 40 ℃ and leaching time of 15 min.

quote

GB/T 7714-2015 [1] LI Yong-kang, LIANG Yong, SHAO Long-bin, et al. Research on Process of Rare Earth Recovery from Rare Earth Electrolysis Slag by Roasting with Sodium Hydroxide[J]. Rare Metals and Cemented Carbides, 2018(1): 5-9.
MLA [1] LI Yong-kang, et al., "Research on Process of Rare Earth Recovery from Rare Earth Electrolysis Slag by Roasting with Sodium Hydroxide." Rare Metals and Cemented Carbides, no. 1, 2018, pp. 5-9.
APA [1] LI Yong-kang, LIANG Yong, SHAO Long-bin, ZOU Yu, & LIANG Xin. (2018). Research on Process of Rare Earth Recovery from Rare Earth Electrolysis Slag by Roasting with Sodium Hydroxide. Rare Metals and Cemented Carbides(1), 5-9.
IEEE [1] LI Yong-kang, LIANG Yong, SHAO Long-bin, ZOU Yu, and LIANG Xin, "Research on Process of Rare Earth Recovery from Rare Earth Electrolysis Slag by Roasting with Sodium Hydroxide," Rare Metals and Cemented Carbides, no. 1, pp. 5-9, 2018. keywords: {rare earth;molten salt electrolysis slag;fluoride salt system;sodium hydroxide roasting;selective leaching with hydrochloric acid}