daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

The Latest Research and Future Development of the Cemented Carbide with Nonuniform Microstructure AITranslate

Jiangxi University of Technology Engineering Research Institute;Jiangxi University of Technology Engineering Research Institute;Jiangxi University of Technology Engineering Research Institute;Jiangxi University of Technology Engineering Research Institute;Jiangxi University of Technology Engineering Research Institute;Jiangxi University of Technology Engineering Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Preparation methods, domestic and oversea development and problems are reviewed of the cemented carbides with nonuniform microstructure. The preparation processes of this type o{ cemented carbides have many influencing factors with complicated steps,and the microstructure of their products is difficult to be precisely controlled. Therefore, development trends in this field are proposed.

KeyWords AITranslate

cemented carbide nonuniform microstructure preparation process the latest development devel-opment trend

1张忠健,汪晓,李仁琼,胡茂中.中国硬质合金产业的技术进步[J].硬质合金,2007,24(1):33-38. 被引量:22

2周建华,卢伟民.国内外硬质合金生产现状及近期发展动向分析[J].稀有金属与硬质合金,2006,34(1):36-41. 被引量:25

3林晨光.中国超细和纳米晶WC-Co硬质合金的研究开发概况[J].中国钨业,2005,20(2):19-23. 被引量:27

4郭圣达,羊建高,黄海平,许方,胡咏梅,郑彪华.粗晶硬质合金硬度和强度影响因素的分析研究[J].稀有金属与硬质合金,2012,40(4):56-58. 被引量:10

5白英龙,吴冲浒,杨霞,徐猛,果世驹.粗细晶WC基体对WC-Co非均匀结构显微组织形成的影响[J].粉末冶金技术,2012,30(2):89-97. 被引量:14

6许雄亮,吴建国.非均匀结构硬质合金的性能探讨[J],硬质合金,2002,19(z):15-18.

7付龙,柳学全,李一,丁存光,李立鑫,姜丽娟.国内外矿用高耐磨、高韧性硬质合金新技术[J].硬质合金,2012,29(4):254-261. 被引量:31

8刘华平,胡其龙,刘兵国,余立新.国内外凿岩用球齿合金的现状、前景与发展趋势[J].粉末冶金工业,2006,16(3):39-44. 被引量:11

9李沐山.20世纪90年代世界硬质合金材料技术进展[M].株洲:《硬质合金》编辑部,2005.

10Moriguchi H. Cemented carbide alloy for cutting tool and coated cemented carbide alloy[P]. EP Pat:0665308 B1,2000-01-05.

1郑清宏,刘江,时凯华,黄伟.粗细WC晶粒配比对双晶结构硬质合金力学性能与组织结构的影响[J].稀有金属与硬质合金,2020(1):75-79. 被引量:4

2江丙武,蔡海燕,宋耀强,赵东,阳进,黄蕊,杜秋容.国内外路面铣刨刀具用硬质合金的现状与发展趋势[J].硬质合金,2014,31(3):194-200. 被引量:1

3朱国丽,何清勇,唐琛,王权,张平,乔娇.WC-10%Co非均匀结构细晶合金的研究[J].硬质合金,2015,32(2):88-94. 被引量:5

4蒙世合,罗海辉,彭宇.WC晶粒离散度对WC-Co硬质合金断裂韧性的影响[J].硬质合金,2017,34(1):14-20. 被引量:11

5郭智兴,杨梅,熊计,鲜广,叶俊镠.非均匀结构硬质合金制备及无损检测综合实验[J].实验技术与管理,2018,35(2):81-84. 被引量:6

6朱立荣,龙坚战,谢浩,涂俊平.两种粒度WC配比与球磨时间对WC-20%Co粗晶合金显微组织的影响[J].硬质合金,2018,35(4):265-272. 被引量:2

7倪培燊,陈少华,卢洋,赵哲,邓欣,刘建业,戚文军,牛留辉,王忠平,李章序,屈志,金枫.SLM打印制备WC-16%Co硬质合金工艺与样品特性研究[J].硬质合金,2019,36(3):177-183. 被引量:3

8顾金宝,高建,时凯华,舒军,曾伟,董凯林,董定乾.矿用WC-Co梯度硬质合金的制备及应用研究现状[J].稀有金属与硬质合金,2019,47(4):83-88. 被引量:3

9李律达,郭圣达,羊建高,王水龙,陈颢,曹赛鹏,黄星,张建波.添加剂对双晶结构硬质合金微观组织和性能的影响[J].稀有金属与硬质合金,2020,48(5):72-77.

10顾金宝,时凯华,董定乾,刁椿珉,曾伟,董凯林,向新.两步球磨制备非均匀结构硬质合金的组织与性能研究[J].四川冶金,2021,43(1):21-25.

1郑清宏,刘江,时凯华,黄伟.粗细WC晶粒配比对双晶结构硬质合金力学性能与组织结构的影响[J].稀有金属与硬质合金,2020(1):75-79. 被引量:4

2邓四文.相同硬度的高钴和低钴含量硬质合金性能比较[J].理化检验:物理分册,2022,58(6):21-25.

3谢晨辉,谭立群,彭宇,周华堂.硬质合金的非常规检测技术[J].硬质合金,2018,35(6):390-402. 被引量:2

4郭娟,李军民.新型硬质合金刀具材料的组织与性能分析[J].工具技术,2016,50(2):63-66.

5臧健,赵军,李安海,王福增.导热系数对钛合金切削绝热剪切影响的有限元模拟[J].硬质合金,2016,33(3):181-187. 被引量:2

6陈国庆,柳峻鹏,张秉刚,冯吉才.硬质合金与钢电子束焊接接头缺陷及断裂分析[J].焊接学报,2017,38(10):1-5. 被引量:7

7朱立荣,龙坚战,谢浩,涂俊平.两种粒度WC配比与球磨时间对WC-20%Co粗晶合金显微组织的影响[J].硬质合金,2018,35(4):265-272. 被引量:2

8张湘.碳化温度对超细WC粉末性能与合金性能的影响[J].硬质合金,2019,36(5):361-367. 被引量:4

9鲁忠臣,曾美琴,王为,朱敏.等离子球磨技术在制备WC-Co硬质合金中的应用[J].硬质合金,2020,37(1):1-18. 被引量:1

10雒飞飞.硬质合金分析检测技术分析[J].中国设备工程,2020(16):153-154.

1易凯华,孙宝琦.“均匀”还是“非均匀”辩析[J].稀有金属与硬质合金,1994,22(3):45-48. 被引量:3

2白英龙,吴冲浒,杨霞,徐猛,果世驹.粗细晶WC基体对WC-Co非均匀结构显微组织形成的影响[J].粉末冶金技术,2012,30(2):89-97. 被引量:14

3张齐勋.非均匀结构WC-Co硬质合金[J].中南工业大学学报,1995,26(3):365-368. 被引量:3

4朱国丽,何清勇,唐琛,王权,张平,乔娇.WC-10%Co非均匀结构细晶合金的研究[J].硬质合金,2015,32(2):88-94. 被引量:5

5李继承,陈小伟,黄风雷.块体金属玻璃压缩变形和破坏特性的有限元模拟研究[J].固体力学学报,2016,37(S1):56-64. 被引量:2

6吴建国.焊接球齿钎头用硬质合金KK30牌号的研制[J].凿岩机械气动工具,2011,37(4):21-23.

7张正富,彭金辉.提高钻采工具用硬质合金性能的新技术[J].粉末冶金技术,2011,29(2):142-148. 被引量:4

8林晨光,楚建新,叶军.“金属布”硬质复合涂层的微观组织及性能[J].中国有色金属学报,1996,6(1):93-97. 被引量:1

9胡启明.YT合金改性研究[J].硬质合金,2000,17(1):30-33.

10倪培君,蔡和平,张维国,郭智敏,郝丽萍.非均匀结构件材料密度工业CT定量检测方法[J].无损检测,2012,34(2):11-15. 被引量:6

Basic Information:

DOI:

Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]

Citation Information:

Preparation methods, domestic and oversea development and problems are reviewed of the cemented carbides with nonuniform microstructure. The preparation processes of this type o{ cemented carbides have many influencing factors with complicated steps,and the microstructure of their products is difficult to be precisely controlled. Therefore, development trends in this field are proposed.

quote

GB/T 7714-2015 [1] GUO Sheng-da, LV Jian, CHEN Hao, et al. The Latest Research and Future Development of the Cemented Carbide with Nonuniform Microstructure[J]. Rare Metals and Cemented Carbides, 2013(6): 67-69.
MLA [1] GUO Sheng-da, et al., "The Latest Research and Future Development of the Cemented Carbide with Nonuniform Microstructure." Rare Metals and Cemented Carbides, no. 6, 2013, pp. 67-69.
APA [1] GUO Sheng-da, LV Jian, CHEN Hao, YANG Jian-gao, ZHONG Ming-long, & ZHU Er-tao. (2013). The Latest Research and Future Development of the Cemented Carbide with Nonuniform Microstructure. Rare Metals and Cemented Carbides(6), 67-69.
IEEE [1] GUO Sheng-da, LV Jian, CHEN Hao, YANG Jian-gao, ZHONG Ming-long, and ZHU Er-tao, "The Latest Research and Future Development of the Cemented Carbide with Nonuniform Microstructure," Rare Metals and Cemented Carbides, no. 6, pp. 67-69, 2013. keywords: {cemented carbide;nonuniform microstructure;preparation process;the latest development;devel-opment trend}