Effect of SiO2Coating on the CO Poisoning Resistance of ZrCo Hydrogen Storage Alloy AITranslate
Abstract AITranslate
In order to improve the poisoning resistance of ZrCo alloy against CO impurity gas,ZrCo alloy particles were embedded into SiO2matrix by SiO2sol coating method to prepare ZrCo/SiO2composites with different mass ratios.The phase composition,micro-morphology,and elemental composition of the samples were characterized by X-ray diffractometer,scanning electron microscope,transmission electron microscope,and energy-dispersive X-ray spectrometer.The effects of CO concentration and SiO2coating ratio on the hydrogen absorption kinetic performance of ZrCo/SiO2were investigated by using a hydrogen storage material performance test device in a mixed H2/CO atmosphere,and the hydrogen absorption behavior of the samples was analyzed by kinetic model.The experimental results show that ZrCo hydrogen storage alloy particles are well bonded with the SiO2matrix and uniformly distributed in the matrix.The SiO2coating effectively improves the hydrogen absorption rate of ZrCo alloy in H2/CO atmosphere.When the mass ratio of ZrCo/SiO2is 1∶1.5,it takes only 5 h for the composite to reach the saturation hydrogen absorption capacity in H2containing 0.5%(molar ratio)CO,whereas it takes 55 h for the uncoated ZrCo.Therefore,the ZrCo/SiO2composites have good CO poisoning resistance and certain cycling pulverization resistance.
KeyWords AITranslate
Basic Information:
DOI:
Chinese Library Classification Number:TG139.7[一般工业技术—材料科学与工程]
Citation Information:
In order to improve the poisoning resistance of ZrCo alloy against CO impurity gas,ZrCo alloy particles were embedded into SiO2matrix by SiO2sol coating method to prepare ZrCo/SiO2composites with different mass ratios.The phase composition,micro-morphology,and elemental composition of the samples were characterized by X-ray diffractometer,scanning electron microscope,transmission electron microscope,and energy-dispersive X-ray spectrometer.The effects of CO concentration and SiO2coating ratio on the hydrogen absorption kinetic performance of ZrCo/SiO2were investigated by using a hydrogen storage material performance test device in a mixed H2/CO atmosphere,and the hydrogen absorption behavior of the samples was analyzed by kinetic model.The experimental results show that ZrCo hydrogen storage alloy particles are well bonded with the SiO2matrix and uniformly distributed in the matrix.The SiO2coating effectively improves the hydrogen absorption rate of ZrCo alloy in H2/CO atmosphere.When the mass ratio of ZrCo/SiO2is 1∶1.5,it takes only 5 h for the composite to reach the saturation hydrogen absorption capacity in H2containing 0.5%(molar ratio)CO,whereas it takes 55 h for the uncoated ZrCo.Therefore,the ZrCo/SiO2composites have good CO poisoning resistance and certain cycling pulverization resistance.
quote
| GB/T 7714-2015 | [1] SU Min-an, KOU Hua-qin, YE Rong-xing, et al. Effect of SiO2Coating on the CO Poisoning Resistance of ZrCo Hydrogen Storage Alloy[J]. Rare Metals and Cemented Carbides, 2025(1): 89-97. |
| MLA | [1] SU Min-an, et al., "Effect of SiO2Coating on the CO Poisoning Resistance of ZrCo Hydrogen Storage Alloy." Rare Metals and Cemented Carbides, no. 1, 2025, pp. 89-97. |
| APA | [1] SU Min-an, KOU Hua-qin, YE Rong-xing, BAO Jin-chun, & ZHOU Lin-sen. (2025). Effect of SiO2Coating on the CO Poisoning Resistance of ZrCo Hydrogen Storage Alloy. Rare Metals and Cemented Carbides(1), 89-97. |
| IEEE | [1] SU Min-an, KOU Hua-qin, YE Rong-xing, BAO Jin-chun, and ZHOU Lin-sen, "Effect of SiO2Coating on the CO Poisoning Resistance of ZrCo Hydrogen Storage Alloy," Rare Metals and Cemented Carbides, no. 1, pp. 89-97, 2025. keywords: {ZrCo alloy;hydrogen storage;SiO;sol;coating;CO poisoning resistance;hydrogen absorption} |