Highly Refractive Aromatic Polybenzoxazoles Derived from Sulfur-Containing Dibenzoyl Chlorides AITranslate
Abstract AITranslate
A series of aromatic polybenzoxazoles (PBOs) containing sulfur atoms in their main chains were developed. All of the PBOs were prepared from synthesized hydroxyl-diamine 4,4′-bis(4-amino-3-hydroxyphenylthio)diphenylsulfide (3SDA) and aromatic diacyl chlorides, such as 4,4′-((thiobis(4,1-phenylene))bis(sulfanediyl))dibenzoyl chloride (3SDBC), trans-1,4-cyclohexanedicarbonyl dichloride (trans-CHDC), isophthaloyl dichloride (IPC), and 4,4′-oxybis(benzoyl chloride) (OBC), via a conventional two-step procedure. The PBOs exhibited high thermal stability, thermal decomposition temperature (>430 °C), and glass-transition temperature (204–255 °C). The PBO derived from 3SDA and 3SDBC exhibited a very high refractive index, i.e., 1.7862 at 637 nm due to the high sulfur content (21.79%).
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00694
Chinese Library Classification Number:
Citation Information:
A series of aromatic polybenzoxazoles (PBOs) containing sulfur atoms in their main chains were developed. All of the PBOs were prepared from synthesized hydroxyl-diamine 4,4′-bis(4-amino-3-hydroxyphenylthio)diphenylsulfide (3SDA) and aromatic diacyl chlorides, such as 4,4′-((thiobis(4,1-phenylene))bis(sulfanediyl))dibenzoyl chloride (3SDBC), trans-1,4-cyclohexanedicarbonyl dichloride (trans-CHDC), isophthaloyl dichloride (IPC), and 4,4′-oxybis(benzoyl chloride) (OBC), via a conventional two-step procedure. The PBOs exhibited high thermal stability, thermal decomposition temperature (>430 °C), and glass-transition temperature (204–255 °C). The PBO derived from 3SDA and 3SDBC exhibited a very high refractive index, i.e., 1.7862 at 637 nm due to the high sulfur content (21.79%).
quote
| GB/T 7714-2015 | [1] Hyeonil Kim, Hyeonuk Yeo, Heung Cho Ko, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00694. |
| MLA | [1] Hyeonil Kim, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00694. |
| APA | [1] Hyeonil Kim, Hyeonuk Yeo, Heung Cho Ko, & NamHo You. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00694 |