Abstract AITranslate

Area-selective atomic layer deposition (ALD) has the potential to significantly improve current fabrication approaches by introducing a bottom-up process in which robust and conformal thin films are selectively deposited onto patterned substrates. This bottom-up approach requires selective areas of the substrates to be masked to inhibit deposition. Spontaneous self-assembly and organization of a mask, incorporating adhesion and other functions, are particularly attractive for this role as they do not require a separate patterning step. Here, we make use of the pH/light tunability of catechol adhesion to develop a catechol-functionalized polymer that exhibits tunable adhesion strengths on different materials based on their specific chemistry. Tunable selective deposition was shown between metal/metal oxide substrates by controlling the local pH. Moreover, by controlling the adhesion strength through UV light, the deposition of hafnium oxide (HfO2) during ALD was successfully inhibited.

KeyWords AITranslate

areaselective atomic layer deposition selective deposition tunable adhesion catecholfunctionalized polymer Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00692

Chinese Library Classification Number:

Citation Information:

Area-selective atomic layer deposition (ALD) has the potential to significantly improve current fabrication approaches by introducing a bottom-up process in which robust and conformal thin films are selectively deposited onto patterned substrates. This bottom-up approach requires selective areas of the substrates to be masked to inhibit deposition. Spontaneous self-assembly and organization of a mask, incorporating adhesion and other functions, are particularly attractive for this role as they do not require a separate patterning step. Here, we make use of the pH/light tunability of catechol adhesion to develop a catechol-functionalized polymer that exhibits tunable adhesion strengths on different materials based on their specific chemistry. Tunable selective deposition was shown between metal/metal oxide substrates by controlling the local pH. Moreover, by controlling the adhesion strength through UV light, the deposition of hafnium oxide (HfO2) during ALD was successfully inhibited.

quote

GB/T 7714-2015 [1] Hellen Papananou, Reika Katsumata, Zachary Neary, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00692.
MLA [1] Hellen Papananou, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00692.
APA [1] Hellen Papananou, Reika Katsumata, Zachary Neary, Rubayn Goh, Xiangxi Meng, Ratchana Limary, & Rachel A. Segalman. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00692
IEEE [1] Hellen Papananou, Reika Katsumata, Zachary Neary, Rubayn Goh, Xiangxi Meng, Ratchana Limary, and Rachel A. Segalman, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00692. keywords: {areaselective atomic layer deposition;selective deposition;tunable adhesion;catecholfunctionalized polymer;Show More}