daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Adsorption and Sensing Performance toward Methanol Vapor on SnS/SnS2 In-Plane Heterostructures Adsorption and Sensing Performance toward Methanol Vapor on SnS/SnS2 In-Plane Heterostructures AITranslate

Tianjin University; Tianjin University; Tianjin University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Group-IV monochalcogenides MX (M = Ge, Sn; X = S, Se) show great potential in gas-sensing applications due to their unique two-dimensional (2D) geometry with a puckered layer and high oxidation resistance. In terms of gas-sensing response modulation, creating 2D heterojunctions has been demonstrated to be highly effective. In this work, a unique in-plane heterostructure of SnS/SnS2 was prepared by thermally induced phase transition from n-type SnS2 to p-type SnS for a promising methanol sensor. Differing from common vertically stacked van der Waals heterojunctions, plentiful grain boundaries and lattice defects are generated in the SnS/SnS2 lateral heterostructure, inducing further structural symmetry breaking, due to the obvious lattice mismatch between orthogonal SnS and hexagonal SnS2. The special local irregularity with a grain boundary relaxation effect existed around the highly active sites of the generated vacancy defects and the lattice Sn atoms at SnS/SnS2 grain boundaries, which can trigger strong adsorption of methanol molecules on the lateral heterostructured sensing surface. Meanwhile, the SnS/SnS2 lateral heterojunctions with strong in-plane covalent bonding show significant modulation on the electron transport characteristic. Resultantly, the sensor based on the as-prepared SnS/SnS2 in-plane heterostructure is revealed to display a 7.1 times enhancement in sensing response toward 25 ppm methanol at room temperature compared with a pristine SnS sensor and shows the capability to detect rarefied methanol vapor as low as 100 ppb.

KeyWords AITranslate

gas sensor twodimensional SnS inplane heterostructure heterogeneous modulation effect interface reconstruction
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c00911

Chinese Library Classification Number:

Citation Information:

Group-IV monochalcogenides MX (M = Ge, Sn; X = S, Se) show great potential in gas-sensing applications due to their unique two-dimensional (2D) geometry with a puckered layer and high oxidation resistance. In terms of gas-sensing response modulation, creating 2D heterojunctions has been demonstrated to be highly effective. In this work, a unique in-plane heterostructure of SnS/SnS2 was prepared by thermally induced phase transition from n-type SnS2 to p-type SnS for a promising methanol sensor. Differing from common vertically stacked van der Waals heterojunctions, plentiful grain boundaries and lattice defects are generated in the SnS/SnS2 lateral heterostructure, inducing further structural symmetry breaking, due to the obvious lattice mismatch between orthogonal SnS and hexagonal SnS2. The special local irregularity with a grain boundary relaxation effect existed around the highly active sites of the generated vacancy defects and the lattice Sn atoms at SnS/SnS2 grain boundaries, which can trigger strong adsorption of methanol molecules on the lateral heterostructured sensing surface. Meanwhile, the SnS/SnS2 lateral heterojunctions with strong in-plane covalent bonding show significant modulation on the electron transport characteristic. Resultantly, the sensor based on the as-prepared SnS/SnS2 in-plane heterostructure is revealed to display a 7.1 times enhancement in sensing response toward 25 ppm methanol at room temperature compared with a pristine SnS sensor and shows the capability to detect rarefied methanol vapor as low as 100 ppb.

quote

GB/T 7714-2015 [1] Yuxiang Qin, Shuhan Chen, Yinan Bai. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c00911.
MLA [1] Yuxiang Qin, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c00911.
APA [1] Yuxiang Qin, Shuhan Chen, & Yinan Bai. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c00911
IEEE [1] Yuxiang Qin, Shuhan Chen, and Yinan Bai, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c00911. keywords: {gas sensor twodimensional SnS inplane heterostructure heterogeneous modulation effect interface reconstruction}