Super-Low-Addition Biobased Flame Retardant Dedicated to Polylactic Acid through Ionic Reaction between Phytic Acid and Taurine AITranslate
Abstract AITranslate
The fully biobased flame retardant, which is based on the green and convenient ionic reaction of phytic acid (PA) and taurine (TA) in water, brings flame retardancy to polylactic acid (PLA) efficiently. PLA composite passes UL-94 V-0 rating in vertical combustion successively with only 0.5 wt % reactant of PA and TA (PA-TA). Moreover, the peak heat release rate (PHRR) and the total heat release rate (THR) of PLA composite are reduced by 13.1 and 10.0% with 5.0 wt % PA-TA. Moreover, the elongation at break of PLA with 5.0 wt % PA-TA is 92.7% higher than that of pure PLA due to the ultralow addition and the interaction of hydrogen bonds between the flame retardant and the matrix material. The resultant fully biodegradable flame-retardant PLA composites reported here could be widely applied in electronic appliances, automobiles, and other fields.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00671
Chinese Library Classification Number:
Citation Information:
The fully biobased flame retardant, which is based on the green and convenient ionic reaction of phytic acid (PA) and taurine (TA) in water, brings flame retardancy to polylactic acid (PLA) efficiently. PLA composite passes UL-94 V-0 rating in vertical combustion successively with only 0.5 wt % reactant of PA and TA (PA-TA). Moreover, the peak heat release rate (PHRR) and the total heat release rate (THR) of PLA composite are reduced by 13.1 and 10.0% with 5.0 wt % PA-TA. Moreover, the elongation at break of PLA with 5.0 wt % PA-TA is 92.7% higher than that of pure PLA due to the ultralow addition and the interaction of hydrogen bonds between the flame retardant and the matrix material. The resultant fully biodegradable flame-retardant PLA composites reported here could be widely applied in electronic appliances, automobiles, and other fields.
quote
| GB/T 7714-2015 | [1] Feiyang Wu, Jian Xu, Xueyang Qiu, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00671. |
| MLA | [1] Feiyang Wu, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00671. |
| APA | [1] Feiyang Wu, Jian Xu, Xueyang Qiu, Shichao Lin, Menghuan Zhang, Meng Ma, Yanqin Shi, Huiwen He, Si Chen, & Xu Wang. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00671 |
| IEEE | [1] Feiyang Wu, Jian Xu, Xueyang Qiu, Shichao Lin, Menghuan Zhang, Meng Ma, Yanqin Shi, Huiwen He, Si Chen, and Xu Wang, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00671. keywords: {superlow addition;biodegradable;flame retardant;polylactic acid (PLA);ionic reaction} |