Effects of Double Aging on Mechanical Properties and Corrosion Resistance of the Al-Cu-Li-Zr Alloy Containing Sc AITranslate
Abstract AITranslate
The effects of double aging on mechanical properties and corrosion resistance of the Al-Cu-Li-Zr alloy containing Sc were studied by tensile test at room temperature,TEM and corrosion experiment.The results show that the alloy treated with double aging can show optimal comprehensive properties of strength and plasticity.Compared with the alloy treated with T8 peak aging,that with double aging has improved elongation even without its strength reduced.The main precipitated strengthening phase of the alloy is T1 phase.After double aging,fine and dispersive T1 phase precipitates in the grain interior,distributed uniformly in the alloy to improve its corrosion resistance.
KeyWords AITranslate
1梁文杰,潘青林,朱朝明,何运斌,刘元斐,尹志民.微量Sc对Al-Cu-Li-Zr合金的微观组织和拉伸性能的影响[J].稀有金属材料与工程,2006,35(4):550-553. 被引量:12
2王芝秀,郑子樵,李海.铝锂合金的微合金化及其作用机理[J].材料导报,2003,17(10):11-15. 被引量:18
3TAN Cheng yu,ZHENG Zi qiao,XIA Chang qing,LIANG Ying (Department of Materials Science and Engineering, Central South University of Technology, Changsha 410083, China).The Aging Feature of Al-L-Cu-Mg-Zr Alloy Containing Sc[J].中南大学学报:英文版,2000,12(2):65-67. 被引量:22
4尹登峰,周东海.时效工艺对Al-Li-Cu-Mg-Zr合金组织和性能的影响[J].铝加工,1996,19(1):19-23. 被引量:2
5尹志民,陈小群,章泗琪,张伟斌.2091Al-Li合金的形变热处理[J].金属学报,1991,27(2). 被引量:13
1梁文杰,潘清林,何运斌.双级时效对含Sc的Al-Cu-Li-Zr合金组织与性能的影响[J].中南大学学报:自然科学版,2011,42(8):2260-2265. 被引量:2
2朱朝明,潘青林,王新宇,梁文杰,何运斌,刘元斐.含钪Al-Cu-Li-Zr合金的热处理[J].轻合金加工技术,2005,33(12):41-44. 被引量:3
3梁文杰,潘青林,何运斌.含钪Al-Cu-Li-Zr合金的热处理制度[J].材料热处理学报,2011,32(9):72-77. 被引量:3
4梁文杰,潘清林,何运斌.含钪Al-Cu-Li-Zr合金的热变形行为及组织演化[J].中国有色金属学报,2011,21(5):988-994. 被引量:1
5潘清林,李运春,梁文杰,何运斌,周迎春,路聪阁,刘晓艳.预变形对新型含钪Al-Cu-Li-Zr合金剥蚀性能的影响[J].中南大学学报:自然科学版,2008,39(4):735-740. 被引量:5
6隆平,潘清林,梁文杰,张小刚.含钪Al-Cu-Li-Zr合金高温压缩变形组织的研究[J].金属世界,2008(2):7-11.
7梁文杰,潘青林,朱朝明,何运斌,刘元斐,尹志民.微量Sc对Al-Cu-Li-Zr合金的微观组织和拉伸性能的影响[J].稀有金属材料与工程,2006,35(4):550-553. 被引量:12
8张健,马云龙,李劲风,朱瑞华,刘晴,向胜,郑子樵.微合金化对Al-Cu-Li-Zr合金拉伸性能和微观组织的影响[J].锻压技术,2015,40(7):131-135. 被引量:3
9隆平,李擎,梁文杰,朱朝明,潘青林.热处理对含钪Al-Cu-Li-Zr合金组织与性能的影响[J].矿冶工程,2005,25(5):62-65. 被引量:7
10周昌荣,刘心宇,潘青林.微量钪在Al-Cu-Li-Zr合金中的存在形式和作用[J].材料工程,2006,34(z1):225-228. 被引量:4
Basic Information:
DOI:
Chinese Library Classification Number:TG146.45[金属学及工艺—金属材料]
Citation Information:
The effects of double aging on mechanical properties and corrosion resistance of the Al-Cu-Li-Zr alloy containing Sc were studied by tensile test at room temperature,TEM and corrosion experiment.The results show that the alloy treated with double aging can show optimal comprehensive properties of strength and plasticity.Compared with the alloy treated with T8 peak aging,that with double aging has improved elongation even without its strength reduced.The main precipitated strengthening phase of the alloy is T1 phase.After double aging,fine and dispersive T1 phase precipitates in the grain interior,distributed uniformly in the alloy to improve its corrosion resistance.
quote
| GB/T 7714-2015 | [1] LIANG Wen-jie, PAN Qing-lin, HE Yun-bin. Effects of Double Aging on Mechanical Properties and Corrosion Resistance of the Al-Cu-Li-Zr Alloy Containing Sc[J]. Rare Metals and Cemented Carbides, 2011(2): 33-37. |
| MLA | [1] LIANG Wen-jie, et al., "Effects of Double Aging on Mechanical Properties and Corrosion Resistance of the Al-Cu-Li-Zr Alloy Containing Sc." Rare Metals and Cemented Carbides, no. 2, 2011, pp. 33-37. |
| APA | [1] LIANG Wen-jie, PAN Qing-lin, & HE Yun-bin. (2011). Effects of Double Aging on Mechanical Properties and Corrosion Resistance of the Al-Cu-Li-Zr Alloy Containing Sc. Rare Metals and Cemented Carbides(2), 33-37. |
| IEEE | [1] LIANG Wen-jie, PAN Qing-lin, and HE Yun-bin, "Effects of Double Aging on Mechanical Properties and Corrosion Resistance of the Al-Cu-Li-Zr Alloy Containing Sc," Rare Metals and Cemented Carbides, no. 2, pp. 33-37, 2011. keywords: {Al-Cu-Li-Zr alloy containing Sc;double aging;microstructure;mechanical property;corrosion resistance} |