Infrared Light Detection Technology Based on Organics AITranslate
Abstract AITranslate
This decade has seen rapid developments in infrared light sensing and imaging, utilizing innovative materials and deliberate structural designs. Organic semiconducting materials are promising in the next-generation infrared sensing applications due to their unique properties including solution processability, tunable optoelectronic property, and biocompatibility. This Spotlight aims to provide a snapshot of the recent advances in organic infrared light detection technology, specifically for wavelengths beyond 1000 nm, focusing on performance enhancements and new function realizations. Several innovative proof-of-concept demonstrations illustrate the benefits of the rapidly developing organic infrared technology. Finally, we discuss the challenges and perspectives of organic infrared technology.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c01561
Chinese Library Classification Number:
Citation Information:
This decade has seen rapid developments in infrared light sensing and imaging, utilizing innovative materials and deliberate structural designs. Organic semiconducting materials are promising in the next-generation infrared sensing applications due to their unique properties including solution processability, tunable optoelectronic property, and biocompatibility. This Spotlight aims to provide a snapshot of the recent advances in organic infrared light detection technology, specifically for wavelengths beyond 1000 nm, focusing on performance enhancements and new function realizations. Several innovative proof-of-concept demonstrations illustrate the benefits of the rapidly developing organic infrared technology. Finally, we discuss the challenges and perspectives of organic infrared technology.
quote
| GB/T 7714-2015 | [1] Ning Li, Xin Hu, Xiubao Sui, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01561. |
| MLA | [1] Ning Li, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01561. |
| APA | [1] Ning Li, Xin Hu, Xiubao Sui, Qian Chen, & Tse Nga Ng. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01561 |
| IEEE | [1] Ning Li, Xin Hu, Xiubao Sui, Qian Chen, and Tse Nga Ng, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01561. keywords: {organic semiconductors infrared detection band tunable photoresponse photomultiplication pixeless imaging} |