Basic Kinetic Equations of Solid-liquid Phase Flow Powder Binder of PIM AITranslate
Abstract AITranslate
Assuming that during the phase flow of PIM particle-binder,the powder particles are spherical with irregular size,the powder particles and gas molecule have similar physical and kinetic properties.Study is made on the particle phase motion during PIM two-phase flow based on the method similar to gas molecule kinectics.Comparison is made between the powder particle motion and gas molecule motion during PIM mould-filling.Based on Boltzmann equation,analysis is made of the physical and kinectic parameters of the powder particle,quality/moment/and energy conservation equation of the PIM particle-binder flow are established,providing a theoretical basis for digital simulation of the two-phase flow and analysis of two-phase separation.
KeyWords AITranslate
1Qu Xuanhui, Li Yimin, Yue Hongsheng, Mao Jinying, Zhu Lei and Huang Baiyun State Key Laboratory for Powder Metallurgy, Central South University of Technology, Changsha 410083, P. R. China.NUMERICAL SIMULATION OF FEEDSTOCK MELT FILLING IN A CYLINDRICAL CAVITY WITH SOLIDIFICATION IN POWDER INJECTION MOLDING[J].中国有色金属学会会刊:英文版,1998,0(4):13-18. 被引量:9
1张晓岩,武彬,肖建中.陶瓷注射成型数值模拟及其进展[J].材料导报,2005,19(F05):219-221. 被引量:3
2徐华安,熊惟皓,叶大萌.粉末注射成形充模流动模拟研究现状与展望[J].材料导报,2006,20(11):84-86. 被引量:4
3王程成,贺德龙,鞠梦婷,韦家虎,益小苏.注射成型水溶性陶瓷型芯技术[J].航空材料学报,2015,35(4):83-95. 被引量:2
4刘飞,李文明,王青云.数值模拟研究浇口方式对粉末注射成形铣刀粉体分布的影响[J].粉末冶金材料科学与工程,2018,23(3):292-297. 被引量:3
1徐华安,熊惟皓,叶大萌.粉末注射成形充模流动模拟研究现状与展望[J].材料导报,2006,20(11):84-86. 被引量:4
2严志云,严友兰.陶瓷螺杆的粉末注射成型模拟研究[J].塑料制造,2010(4):89-92. 被引量:2
3王匀,刘炯,戴亚春,孙宪萍,王雪鹏.陶瓷微注射成型技术的研究与进展[J].硅酸盐通报,2012,31(5):1155-1160. 被引量:4
4王程成,贺德龙,鞠梦婷,韦家虎,益小苏.注射成型水溶性陶瓷型芯技术[J].航空材料学报,2015,35(4):83-95. 被引量:2
5冯书林.浅析房屋建筑施工中的防潮技术[J].建材与装饰,2017,0(30):33-34. 被引量:2
6汪传生,胡纪全,朱琳.椎间融合器金属粉末注塑成型模具设计研究[J].橡胶工业,2018,65(1):89-93. 被引量:4
7崔利群,韩胜利,施麒,李达人,胡建召,刘祖岩.钨铜粉末轧制的有限元模拟研究[J].粉末冶金材料科学与工程,2019,24(5):406-412. 被引量:1
8谢兴铖,曹瑞军,李增德,周增林,李卿,李悦,贾斌.大长径比超细WC-Co圆棒PIM充模过程的数值模拟[J].稀有金属材料与工程,2021,50(1):160-166.
9刘富初,黄捷飞,龚小龙,涂梭,韩光超,樊自田.复杂内腔铸件用水溶性型芯的研究进展(1)[J].现代铸铁,2021,41(5):52-58.
10侯成龙,郭俊卿,陈拂晓,皇涛.金属粉末注射成形技术及其数值模拟[J].粉末冶金技术,2022,40(1):72-79. 被引量:1
1米山哲人,徐秀芝.两相分离型高性能Sm2(Co,Cu,Fe,Zr)17系磁体[J].国外稀有金属,1990(3):34-37.
2毛金英,曲选辉,李志林.粉末注射成形充模过程凝固层形成规律研究[J].中国锰业,1999,17(1):44-48. 被引量:1
3王玉会,曲选辉,何新波.粉末注射成形多相流动过程数值模拟模型[J].北京科技大学学报,2007,29(7):717-720. 被引量:5
4曲选辉,毛金英,乐红胜,林好转,李益民.粉末注射成形充模过程凝固层形成规律研究[J].粉末冶金材料科学与工程,1998,3(3):153-159. 被引量:1
5张琳,卜庆选,尤一匡,胡爱萍.高炉冷却壁冷却水管内液固两相流强化传热实验研究[J].铸造技术,2009,30(11):1465-1467. 被引量:2
6毛金英,曲选辉,乐红胜,林好转,李益民.粉末注射成形充模过程中凝固层形成规律的计算与分析[J].粉末冶金技术,1999,17(1):14-18. 被引量:8
7赵洪亮,张廷安,张超,刘燕,赵秋月,王淑婵,豆志河.改进Intermig桨种分槽搅拌性能的数值模拟[J].过程工程学报,2011,11(1):15-19. 被引量:9
8刘绍军,曲选辉,李益民,黄伯云.金属注射成形过程中的粉末堆积问题[J].材料科学与工程,1998,16(4):44-47. 被引量:1
9陶杰武,段柏华,何新波,秦明礼,曲选辉.注射成形低合金钢支持块零件的研究[J].粉末冶金技术,2006,24(2):131-135.
10王玉会,曲选辉,何新波,张勇,林冰涛,藏若愚.粉末注射成形充模过程特有边界层效应的数值模拟[J].机械工程材料,2008,32(2):77-80. 被引量:4
Basic Information:
DOI:
Chinese Library Classification Number:TF124.39[冶金工程—粉末冶金]
Citation Information:
Assuming that during the phase flow of PIM particle-binder,the powder particles are spherical with irregular size,the powder particles and gas molecule have similar physical and kinetic properties.Study is made on the particle phase motion during PIM two-phase flow based on the method similar to gas molecule kinectics.Comparison is made between the powder particle motion and gas molecule motion during PIM mould-filling.Based on Boltzmann equation,analysis is made of the physical and kinectic parameters of the powder particle,quality/moment/and energy conservation equation of the PIM particle-binder flow are established,providing a theoretical basis for digital simulation of the two-phase flow and analysis of two-phase separation.
quote
| GB/T 7714-2015 | [1] ZHENG Zhou-shun, QU Xuan-hui, HAN Xu-li. Basic Kinetic Equations of Solid-liquid Phase Flow Powder Binder of PIM[J]. Rare Metals and Cemented Carbides, 2002(4): 1-5. |
| MLA | [1] ZHENG Zhou-shun, et al., "Basic Kinetic Equations of Solid-liquid Phase Flow Powder Binder of PIM." Rare Metals and Cemented Carbides, no. 4, 2002, pp. 1-5. |
| APA | [1] ZHENG Zhou-shun, QU Xuan-hui, & HAN Xu-li. (2002). Basic Kinetic Equations of Solid-liquid Phase Flow Powder Binder of PIM. Rare Metals and Cemented Carbides(4), 1-5. |
| IEEE | [1] ZHENG Zhou-shun, QU Xuan-hui, and HAN Xu-li, "Basic Kinetic Equations of Solid-liquid Phase Flow Powder Binder of PIM," Rare Metals and Cemented Carbides, no. 4, pp. 1-5, 2002. keywords: {powder injection molding;solid-liquid phase flow;boltzmann equation} |