Overall Treatment of Process Effluent from Ammonium Molybdate AITranslate
Abstract AITranslate
Study is made of the treatment of acid effluent from ammonium molybdate plant by addition of ammonium sulfide and pH value control with ammonia spirit.Under proper condition,over 90% of heavy metals Cu,Pb,Zn,Fe in the effluent are precipitated and removed,>98% Mo coprecipitated into the residue.Then,the precipitation residue is dissolved by ammonia spirit with 84.59% Mo converted into ammonium molybdate solution,while Fe,Cu,Pb in the residue are basically insoluable,part of Zn going to ammornium molybdate solution ,which can go directly back to the main circuit of ammonium moybdate.The treated acid effluent is retreated for removal of alkali metal ion before crystalized to produce ammonium nitrate.
KeyWords AITranslate
1梁宏,卢基爵.离子交换法从含钼酸性废液中回收钼[J].中国钼业,1999,23(3):43-45. 被引量:19
2张兴元.用离子交换法从酸沉母液中回收钼[J].中国钼业,1997,21(4):23-25. 被引量:6
3桂林,王淑芳,马成兵.钼酸铵生产中的废水处理[J].中国钼业,1999,23(5):25-26. 被引量:17
4张建刚,段黎萍,李俊平,祖庸.钼酸铵生产废液的综合治理[J].化工环保,2000,20(1):28-31. 被引量:16
1张洪利,李吉峰,卢爱刚,焦更生,王福民.钼酸铵工业酸性废液制备硝铵磷工艺[J].化工进展,2011,30(S1):551-553.
2刘敏婕,马全智,李辉.离子交换法综合处理钼酸铵生产废水的研究[J].中国钼业,2006,30(3):27-29. 被引量:14
3姬涛,金奇庭,郭新超,孙长顺.钼酸铵生产酸洗废水的治理[J].工业用水与废水,2007,38(4):12-14. 被引量:5
4张恒涛,黄宇广.钼加工废水资源化处理示范工程[J].中国给水排水,2010,26(14):99-101. 被引量:5
5张恒涛,高湘,黄宇广.钼加工废水资源化处理示范工程[J].环保科技,2011,17(1):28-31.
6马高峰,雷宁,郭金亮,王子川,孙宝莲,白宏斌,冯宝奇.钼酸铵生产废液及氨浸渣中钼的回收[J].中国钼业,2011,35(6):3-5. 被引量:6
7王晓娟.钼酸铵生产酸性废水处理方法[J].广州化工,2013,41(5):53-54. 被引量:3
8陈晓青,惠越.关于钼酸铵水洗废水回收钼的研究[J].广州化工,2013,41(7):117-119. 被引量:2
9李建华.钼加工企业钼酸铵生产废水的综合治理方法[J].有色金属加工,2013,42(3):32-34.
10陈昆昆,马光,孟晗琪,王治钧,王靖坤,吴永谦.D296树脂从含钼酸性溶液中吸附钼的试验研究[J].中国钼业,2014,38(2):47-50. 被引量:8
1张洪利,李吉峰,卢爱刚,焦更生,王福民.钼酸铵工业酸性废液制备硝铵磷工艺[J].化工进展,2011,30(S1):551-553.
2张文朴.我国钼资源综合利用与再生研发进展评述[J].中国资源综合利用,2006,24(12):4-7. 被引量:8
3张文朴.我国钼资源中稀贵金属的综合利用与再生回收研发进展[J].稀有金属与硬质合金,2007,35(2):35-39. 被引量:5
4张文朴.我国钼资源及稀贵金属的回收与综合利用[J].资源再生,2007(11):26-29. 被引量:2
5陈敏.用树脂回收钼酸铵生产废液中钼及有价资源的研究及生产实践[J].中国钼业,2008,32(5):11-13. 被引量:7
6李青.复合絮凝剂PAC+PDMDAAC对生活污水的处理研究[J].科技情报开发与经济,2008,18(31):130-132. 被引量:1
7张蕾,刘雪岩,姜晓庆,李绮,康平利.纳米TiO_2对钼(Ⅵ)的吸附性能[J].中国有色金属学报,2010,20(2):301-307. 被引量:23
8郗大来,张雄康,蔡卫东.采用离子交换树脂回收钼酸铵生产过程中酸洗废液中钼的工艺[J].中国钼业,2011,35(6):38-40. 被引量:1
9专利技术[J].中国钼业,2011,35(6):40-40.
10宋宝旭,刘四清.国内选矿厂废水处理现状与研究进展[J].矿冶,2012,21(2):97-103. 被引量:36
1徐劼.钼冶炼工业废水的处理和有价资源的回收[J].嘉兴学院学报,2006,18(3):31-35. 被引量:2
2李峰,田建荣.钼酸铵生产中废水的循环利用[J].河北化工,2007,30(10):68-69. 被引量:1
3李建华.钼加工企业钼酸铵生产废水的综合治理方法[J].有色金属加工,2013,42(3):32-34.
4汪金发,华东发.钼酸铵生产中的“三废”治理及综合利用[J].中国钼业,1998,22(4):43-48. 被引量:10
5桂林,王淑芳,马成兵.钼酸铵生产中的废水处理[J].中国钼业,1999,23(5):25-26. 被引量:17
6姬涛,金奇庭,郭新超,孙长顺.钼酸铵生产酸洗废水的治理[J].工业用水与废水,2007,38(4):12-14. 被引量:5
7孟庆国,刘衍贞.从生产废渣中回收钼的工艺研究[J].潍坊学院学报,2002,2(6):55-56. 被引量:1
8史兴元.利用钼酸铵尾渣生产钼酸钠的研究——钼尾渣中钼金属的再回收[J].中国钼业,1998,22(4):91-93. 被引量:9
9刘晨明,林晓,陶莉,田萍,李金涛,曹宏斌.精馏法处理钼酸铵生产中的高浓度氨氮废水[J].有色金属:冶炼部分,2015(11):69-74. 被引量:8
10张恒涛,高湘,黄宇广.钼加工废水资源化处理示范工程[J].环保科技,2011,17(1):28-31.
Basic Information:
DOI:
Chinese Library Classification Number:X758[环境科学与工程—环境工程]
Citation Information:
Study is made of the treatment of acid effluent from ammonium molybdate plant by addition of ammonium sulfide and pH value control with ammonia spirit.Under proper condition,over 90% of heavy metals Cu,Pb,Zn,Fe in the effluent are precipitated and removed,>98% Mo coprecipitated into the residue.Then,the precipitation residue is dissolved by ammonia spirit with 84.59% Mo converted into ammonium molybdate solution,while Fe,Cu,Pb in the residue are basically insoluable,part of Zn going to ammornium molybdate solution ,which can go directly back to the main circuit of ammonium moybdate.The treated acid effluent is retreated for removal of alkali metal ion before crystalized to produce ammonium nitrate.
quote
| GB/T 7714-2015 | [1] XU Jie, XIAO Lian-sheng, ZHANG Qi-xiu. Overall Treatment of Process Effluent from Ammonium Molybdate[J]. Rare Metals and Cemented Carbides, 2002(4): 6-8. |
| MLA | [1] XU Jie, et al., "Overall Treatment of Process Effluent from Ammonium Molybdate." Rare Metals and Cemented Carbides, no. 4, 2002, pp. 6-8. |
| APA | [1] XU Jie, XIAO Lian-sheng, & ZHANG Qi-xiu. (2002). Overall Treatment of Process Effluent from Ammonium Molybdate. Rare Metals and Cemented Carbides(4), 6-8. |
| IEEE | [1] XU Jie, XIAO Lian-sheng, and ZHANG Qi-xiu, "Overall Treatment of Process Effluent from Ammonium Molybdate," Rare Metals and Cemented Carbides, no. 4, pp. 6-8, 2002. keywords: {ammonium molybdate;effluent treatment;precipitation} |