Constructing a 3D multichannel structure to enhance performance of Ni–Co–Mn hydroxide electrodes for flexible supercapacitors AITranslate
Abstract AITranslate
The balancing of the electrochemical performance,mechanical stability,and processing technology for applying supercapacitors to flexible and wearable electronics continues to encounter severe challenges.Herein,we prepare Ni-Co-Mn hydroxide electrodes with a threedimensional multichannel structure via a simple hydrothermal method.These are constructed using vertically contiguous nano sheets with a uniform thickness and rough surface.The electrodes can provide numerous electroactive sites and accelerate the transmission of electrolyte ions.The relationship between the structure and electrochemical performances is verified by experiments and theoretical calculations.Two-dimensional(2D)planar and one-dimensional(1D)fiber electrodes are prepared using a flexible carbon cloth(CC)and carbon fiber(CF),respectively,as substrates.The assembled quasi-solid-state flexible asymmetric supercapacitor(FASC)with a twodimensional sandwich structure using NiCoMn-OH/CC as the electrode achieves a remarkable energy density of73.8 Wh·kg-1at a power density of 1.03 kW·kg-1.The quasi-solid-state FASC with a 1D linear structure using NiCoMn-OH/CF as the electrode also attains a high energy density(12.9 Wh·kg-1at a power density of0.75 W·kg-1).Moreover,the electrochemical performances of the NiCoMn/CC//AC/CC and NiCoMn/CF//AC/CF FASCs are not disturbed at different bending angles(0°,45°,90°,135°and 180°),This indicates the superior flexibility of the devices.We also assemble a self-powered energy-harvesting storage system by integrating FASCs and commercial solar cells to verify its practicability.It displays sustainable development potential for energy storage.
KeyWords AITranslate
1Ji-Qiu Qi,Meng-Yuan Huang,Chen-Ya Ruan,Dong-Dong Zhu,Lei Zhu,Fu-Xiang Wei,Yan-Wei Sui,Qing-Kun Meng.Construction of CoNi_(2)S_(4) nanocubes interlinked by few-layer Ti_(3)C_(2)T_(x) MXene with high performance for asymmetric supercapacitors[J].Rare Metals,2022,41(12):4116-4126. 被引量:2
2Qing Xia,Tong Xia,Xiang Wu.PPy decoratedα-Fe_(2)O_(3) nanosheets as flexible supercapacitor electrodes[J].Rare Metals,2022,41(4):1195-1201. 被引量:3
3Jia Yao,Houzhao Wan,Chi Chen,Jie Ji,Nengze Wang,Zhaohan Zheng,Jinxia Duan,Xunying Wang,Guokun Ma,Li Tao,Hanbin Wang,Jun Zhang,Hao Wang.Oxygen‑Defect Enhanced Anion Adsorption Energy Toward Super‑Rate and Durable Cathode for Ni–Zn Batteries[J].Nano-Micro Letters,2021,13(11):128-141. 被引量:4
1Gege Li,Lin Zhou,Zhonglin Ye,Haixing Zhao.Research on Link Prediction Algorithms Based on Multichannel Structure Modelling[J].国际计算机前沿大会会议论文集,2023(2):269-284.
2陈勇超,李亚丽,董云霞,李东昊,沈思锦,胡继东,付玉军,贺德衍,栗军帅.泡沫镍上生长的具有三明治纳米结构的MnCo_(2)O_(4)@NiCoMnS_(4)用于高性能水系非对称超级电容器[J].Science China Materials,2024,67(3):816-823.
3YANG SHUANGSHUANG.Diversified Elderly Care Services to Promote the Silver Economy[J].China Today,2024,73(3):34-37.
4Cui-Ting Ding,Jin-Qiu Yuan,Meng-Ying Xie,Qing-Yuan Liu,Zeng-Guang Yao,Shi-Yu Zhang,Run-Nan Zhang,Hong Wu,Zhong-Yi Jiang.Research Progress in the Fabrication of Covalent Organic Framework Membranes for Chemical Separations[J].Chinese Journal of Polymer Science,2024,42(2):141-158.
5Qi-Ye Ju,Jia-Jia Zheng,Li Xu,Hai-Yan Jiang,Zi-Qian Xue,Lu Bai,Yang-Yang Guo,Ming-Shui Yao,Ting-Yu Zhu.Enhanced carbon capture with motif-rich amino acid loaded defective robust metal-organic frameworks[J].Nano Research,2024,17(3):2004-2010.
6耿上帅,王皓企,梁飞,王立君,魏东,闫涛,闫良国.钴锰共掺杂金属有机框架催化过一硫酸盐降解四环素的性能[J].中国粉体技术,2024,30(2):113-122.
7Miao YANG,Chufan PENG,Haixia LU,Rufeng LIANG,Hui TANG,Zhongmei QIN,Shengjiu GU.Fresh Processing Technology in Polygonatum odoratum Production Area and Its Comparison with Traditional Processing[J].Medicinal Plant,2024,15(1):38-40.
8Gao He-mei,Li Hong-mei,Jiang Cheng-zhe.Research Progress on Nutrients of Artemisia argyi[J].Journal of Northeast Agricultural University(English Edition),2023,30(4):89-96.
9Yu-Qin Mao,Guang-He Dong,Wei-Bin Zhu,Yuan-Qing Li,Pei Huang,Shao-Yun Fu.Novel sandwich structured glass fiber Cloth/Poly(ethylene oxide)-MXene composite electrolyte[J].Nano Materials Science,2024,6(1):60-67.
10Zhang Yichi,Wang Run,Feng Liyan,Ouyang Yan.Comprehensive Evaluation of New Energy Investment in the Maritime Silk Road(Ⅱ)[J].China Oil & Gas,2023,30(5):30-36.
Basic Information:
DOI:
Chinese Library Classification Number:TM53[电气工程—电器]
Citation Information:
The balancing of the electrochemical performance,mechanical stability,and processing technology for applying supercapacitors to flexible and wearable electronics continues to encounter severe challenges.Herein,we prepare Ni-Co-Mn hydroxide electrodes with a threedimensional multichannel structure via a simple hydrothermal method.These are constructed using vertically contiguous nano sheets with a uniform thickness and rough surface.The electrodes can provide numerous electroactive sites and accelerate the transmission of electrolyte ions.The relationship between the structure and electrochemical performances is verified by experiments and theoretical calculations.Two-dimensional(2D)planar and one-dimensional(1D)fiber electrodes are prepared using a flexible carbon cloth(CC)and carbon fiber(CF),respectively,as substrates.The assembled quasi-solid-state flexible asymmetric supercapacitor(FASC)with a twodimensional sandwich structure using NiCoMn-OH/CC as the electrode achieves a remarkable energy density of73.8 Wh·kg-1at a power density of 1.03 kW·kg-1.The quasi-solid-state FASC with a 1D linear structure using NiCoMn-OH/CF as the electrode also attains a high energy density(12.9 Wh·kg-1at a power density of0.75 W·kg-1).Moreover,the electrochemical performances of the NiCoMn/CC//AC/CC and NiCoMn/CF//AC/CF FASCs are not disturbed at different bending angles(0°,45°,90°,135°and 180°),This indicates the superior flexibility of the devices.We also assemble a self-powered energy-harvesting storage system by integrating FASCs and commercial solar cells to verify its practicability.It displays sustainable development potential for energy storage.
quote
| GB/T 7714-2015 | [1] Zhi-Hui Xu, Shi-Shuai Sun, Xue-Lei Li, et al. Rare Metals, 2024(1): 148-163. |
| MLA | [1] Zhi-Hui Xu, et al., Rare Metals, no. 1, 2024, pp. 148-163. |
| APA | [1] Zhi-Hui Xu, Shi-Shuai Sun, Xue-Lei Li, Zhi-Hui Zhang, Hai-Ying Li, Shuang-Ting Ruan, & Shou-Gen Yin. (2024). Rare Metals(1), 148-163. |
| IEEE | [1] Zhi-Hui Xu, Shi-Shuai Sun, Xue-Lei Li, Zhi-Hui Zhang, Hai-Ying Li, Shuang-Ting Ruan, and Shou-Gen Yin, Rare Metals, no. 1, pp. 148-163, 2024. |