Ambipolar Photoresponse of CsPbX3-ZnO (X = Cl, Br, and I) Heterojunctions Ambipolar Photoresponse of CsPbX3-ZnO (X = Cl, Br, and I) Heterojunctions AITranslate

Nanjing Normal University; Nanjing Normal University; Nanjing Normal University; Nanjing Normal University; Nanjing Normal University; Nanjing Normal University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

All-inorganic perovskite CsPbX3 (X = Cl, Br, and I) quantum dots (QDs) are emerging as attractive materials for photodetectors due to their prominent positive photoresponse. In this work, ambipolar photodetectors were constructed based on heterojunctions of CsPbX3 QDs and ZnO nanocrystals (NCs). The transition between the positive photoconductivity (PPC) and negative photoconductivity (NPC) was successfully controlled not only by the drain-source voltage (VDS) but also by the excitation wavelength and CsPbX3 crystal size. A high responsivity (R), on–off ratio (η), and detectivity (D*) were achieved for NPC (R = 1046 mA/W, η = 281, and D* = 1.65 × 1011 Jones), with PPC (R = 146 mA/W, η = 64, and D* = 1.54 × 1011 Jones) simultaneously revealed in the same device. A general mechanism combining the type-II heterojunction, the component and size-related band structure, and most critically the in-band trap states of the perovskites was established for understanding the unique ambipolar property. It exhibits application potential in developing functional photodetectors, memristors, and optical logic devices.

KeyWords AITranslate

perovskite ZnO quantum dots heterojunction ambipolar photoresponse
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01085

Chinese Library Classification Number:

Citation Information:

All-inorganic perovskite CsPbX3 (X = Cl, Br, and I) quantum dots (QDs) are emerging as attractive materials for photodetectors due to their prominent positive photoresponse. In this work, ambipolar photodetectors were constructed based on heterojunctions of CsPbX3 QDs and ZnO nanocrystals (NCs). The transition between the positive photoconductivity (PPC) and negative photoconductivity (NPC) was successfully controlled not only by the drain-source voltage (VDS) but also by the excitation wavelength and CsPbX3 crystal size. A high responsivity (R), on–off ratio (η), and detectivity (D*) were achieved for NPC (R = 1046 mA/W, η = 281, and D* = 1.65 × 1011 Jones), with PPC (R = 146 mA/W, η = 64, and D* = 1.54 × 1011 Jones) simultaneously revealed in the same device. A general mechanism combining the type-II heterojunction, the component and size-related band structure, and most critically the in-band trap states of the perovskites was established for understanding the unique ambipolar property. It exhibits application potential in developing functional photodetectors, memristors, and optical logic devices.

quote

GB/T 7714-2015 [1] Jiakun An, Gaoyu Chen, Xia Zhu, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01085.
MLA [1] Jiakun An, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01085.
APA [1] Jiakun An, Gaoyu Chen, Xia Zhu, Xin Lv, Jianchun Bao, & Xiangxing Xu. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01085
IEEE [1] Jiakun An, Gaoyu Chen, Xia Zhu, Xin Lv, Jianchun Bao, and Xiangxing Xu, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01085. keywords: {perovskite ZnO quantum dots heterojunction ambipolar photoresponse}