The Measures of Lowing Residual Stress from Metal-Ceramic Field Diffusion Bonding AITranslate

Taiyuan University of Science and Technology;Taiyuan University of Science and Technology;Taiyuan University of Science and Technology;Taiyuan University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This paper describes the mechanism, characteristics and applications of field diffusion connection. It is pointed out that the presence of residual stress can affect the bonding quality. Based on the analysis on how the residual stress is generated from metal-ceramic filed diffusion bonding,detailed measures are given to lower the influence.

KeyWords AITranslate

metal-ceramic field diffusion bonding residual stress bonding quantity technological measures

1Katsuhiko Tanaka,Eiichi Takata,Kuniki Ohwada.Anodic bonding of lead zirconate titanate ceramics to silicon with intermediate glass layer[J].Snsors and Actuators,1998,A69:199-203.

2张丽娜,喻萍,周彤,米运卿,孟庆森,薛锦.钠硼硅酸玻璃与铝的阳极焊工艺及结合机理[J].中国有色金属学报,2001,11(z2):160-163. 被引量:1

3室松岗雄.活性合金化法によるヤラシツケ技术[J].真空,1961,4(5):182-188.

1贾托胜,刘翠荣,吴志生.铝场致扩散连接中的电特性及界面电化学反应[J].铝加工,2010,33(4):15-18.

2陈少平,孟庆森.陶瓷与金属场致扩散连接的应用及发展[J].太原理工大学学报,2003,34(2):173-177.

3潘瑞,王清,孙东立.陶瓷与金属扩散连接和场致扩散连接研究现状和进展[J].焊接,2012(9):13-16. 被引量:2

4喻萍,孟庆森,薛锦.玻璃与硅片场致扩散连接过程中的电流特性与断口分析[J].洛阳工学院学报,2002,23(4):31-33.

5窦林萍,孟庆森,薛锦.陶瓷(玻璃)与金属基复合材料场致扩散连接机理研究[J].材料热处理学报,2004,25(1):8-11.

6孟庆森,俞萍,张丽娜,薛锦.金属与硼硅玻璃场致扩散连接形成机理[J].焊接学报,2001,22(4):63-65. 被引量:14

7刘子建,刘翠荣,孟庆森.降低阳极连接中残余应力的措施[J].铝加工,2007,30(4):46-48.

8曹军,范俊玲,薛铜龙.镀钯铜线性能对键合质量的影响研究[J].材料科学与工艺,2014,22(5):48-53. 被引量:7

9曹军,丁雨田,郭廷彪.铜线性能及键合参数对键合质量的影响[J].材料科学与工艺,2012,20(4):76-79. 被引量:10

10孟庆森,张莉娜,喻萍,薛锦.硼硅玻璃与单晶硅场致扩散连接形成机理分析[J].材料热处理学报,2001,22(4):17-20. 被引量:10

Basic Information:

DOI:

Chinese Library Classification Number:TG456.9[金属学及工艺—焊接]

Citation Information:

This paper describes the mechanism, characteristics and applications of field diffusion connection. It is pointed out that the presence of residual stress can affect the bonding quality. Based on the analysis on how the residual stress is generated from metal-ceramic filed diffusion bonding,detailed measures are given to lower the influence.

quote

GB/T 7714-2015 [1] LIU Zi-jian, WANG Jiu-hai, LIU Cui-rong, et al. The Measures of Lowing Residual Stress from Metal-Ceramic Field Diffusion Bonding[J]. Rare Metals and Cemented Carbides, 2007(3): 58-60.
MLA [1] LIU Zi-jian, et al., "The Measures of Lowing Residual Stress from Metal-Ceramic Field Diffusion Bonding." Rare Metals and Cemented Carbides, no. 3, 2007, pp. 58-60.
APA [1] LIU Zi-jian, WANG Jiu-hai, LIU Cui-rong, & MENG Qing-sen. (2007). The Measures of Lowing Residual Stress from Metal-Ceramic Field Diffusion Bonding. Rare Metals and Cemented Carbides(3), 58-60.
IEEE [1] LIU Zi-jian, WANG Jiu-hai, LIU Cui-rong, and MENG Qing-sen, "The Measures of Lowing Residual Stress from Metal-Ceramic Field Diffusion Bonding," Rare Metals and Cemented Carbides, no. 3, pp. 58-60, 2007. keywords: {metal-ceramic;field diffusion bonding;residual stress;bonding quantity;technological measures}