Development of Anode Material for Lithium-ion Battery AITranslate

Chang'an University School of Earth Science and Land and Resources;Chang'an University School of Earth Science and Land and Resources;Chang'an University School of Earth Science and Land and Resources;Chang'an University School of Earth Science and Land and Resources;Chang'an University School of Earth Science and Land and Resources
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The latest development of anode material for lithium-ion batteries is reviewed in terms of structure,performance, electrochemical reaction mechanism, synthesis method and development tendency. The future application of the said material is also presented.

KeyWords AITranslate

lithium-ion battery anode material latest development development tendency

1ZHU Xianjun,ZHAN Hui,LIU Hanxing,ZHOU Yunhong.Synthesis and characterization of LiNi_(0.95-x)Co_xAl_(0.05)O_2 for lithium-ion batteries[J].稀有金属:英文版,2006,25(4):303-308. 被引量:10

2吴楠,张乃庆,刘伶,孙克宁.锂离子电池正极材料层状LiMnO_2的研究进展[J].功能材料信息,2006,3(3):19-21. 被引量:4

3钟参云,曲涛,田彦文.锂离子电池正极材料LiFePO_4的研究进展[J].稀有金属与硬质合金,2005,33(2):38-42. 被引量:7

1陈杨,周振君,童昀,朱海霞.锂离子电池新型正极材料LiFePO_4/C的合成[J].稀有金属与硬质合金,2008,36(3):35-37. 被引量:1

1白立朋,李秋红,陈立宝,陈杰,王太宏.形貌对LiFePO_4性能影响的研究进展[J].微纳电子技术,2010,47(3):152-156. 被引量:2

1李军,陶熏,黄际伟.锂-空气电池的研究进展与展望[J].电源技术,2013,37(4):686-689. 被引量:1

2陈深,毛晓明,房敏,刘文胜.微电网中储能技术研究进展与展望[J].广东电力,2014,27(2):11-16. 被引量:17

3廖卫平,何凌枫.感应电动机负荷模型参数辨识研究进展与展望[J].山东工业技术,2016(10):168-169.

4陈深,毛晓明,房敏.风力和光伏发电短期功率预测研究进展与展望[J].广东电力,2014,27(1):18-23. 被引量:10

5方小利,潘璇,陈伟.钙钛矿相有机金属卤化物太阳电池研究进展与展望[J].材料导报,2015,29(9):13-19. 被引量:4

6董全峰,王翀,郑明森.锂硫电池关键材料研究进展与展望[J].化学进展,2011,23(2):533-539. 被引量:18

7唐婧璇.浅议FACTS协调控制研究进展与展望[J].科技与企业,2015(12):247-247.

8蒋志君.高温超导强电应用研究进展与展望[J].低温与超导,2009,37(10):17-20. 被引量:2

9杜联兴.变压器故障诊断研究进展与展望[J].广东电力,2013,26(3):1-5. 被引量:6

10蒋晨阳,刘青,梁宵.多个FACTS元件间交互影响分析与协调控制研究进展与展望[J].华北电力技术,2016(5):35-43.

Basic Information:

DOI:

Chinese Library Classification Number:TM912.9[电气工程—电力电子与电力传动]

Citation Information:

The latest development of anode material for lithium-ion batteries is reviewed in terms of structure,performance, electrochemical reaction mechanism, synthesis method and development tendency. The future application of the said material is also presented.

quote

GB/T 7714-2015 [1] CHEN Yang, ZHOU Zhen-jun, TONG Yun, et al. Development of Anode Material for Lithium-ion Battery[J]. Rare Metals and Cemented Carbides, 2007(3): 54-57.
MLA [1] CHEN Yang, et al., "Development of Anode Material for Lithium-ion Battery." Rare Metals and Cemented Carbides, no. 3, 2007, pp. 54-57.
APA [1] CHEN Yang, ZHOU Zhen-jun, TONG Yun, ZHU Hai-xia, & ZHANG Li-jun. (2007). Development of Anode Material for Lithium-ion Battery. Rare Metals and Cemented Carbides(3), 54-57.
IEEE [1] CHEN Yang, ZHOU Zhen-jun, TONG Yun, ZHU Hai-xia, and ZHANG Li-jun, "Development of Anode Material for Lithium-ion Battery," Rare Metals and Cemented Carbides, no. 3, pp. 54-57, 2007. keywords: {lithium-ion battery;anode material;latest development;development tendency}