Effect of In Content on Three-way Catalytic Performance of In-Ag-Ce-O/γ-Al_2O_3 Catalyst AITranslate
Abstract AITranslate
Three-way catalyst was prepared by isovolumetric impregnation with the scattered metal In,the transition metal Ag and the rare earth metal Ce as the active components andγ-Al2O3 as the carrier.The microstructure of the catalyst was characterized by XRD,BET,SEM and N2 adsorption technology.The influence of In content on catalyst performance was also investigated.The results show that the catalyst activity can be improved after In addition resulting in AgInO2 phase appearing in its XRD pattern.However,the catalyst activity gradually decreases with the increase of In content.The results from BET and SEM show that the increase of In content causes aggregation of the active ingredients to reduce their dispersion degree and decrease of the specific surface area of the catalyst to reduce its catalytic activity.In-Ag-Ce-O/γ-Al2O3 catalyst has the strongest three-way catalytic activity when its active ingredient In content is 2%.
KeyWords AITranslate
1李明利,余琼,马兰,周春江,逯庆国,徐英,郭洪光,黄凤莉,曹慧,吕绯.汽车尾气净化催化剂研究发展现状[J].兵器材料科学与工程,2012,35(6):96-98. 被引量:10
2陈昊,王学涛,康淑娟.贵金属三效催化剂的研究进展[J].化学与生物工程,2010,27(6):1-3. 被引量:5
3康新婷,汤慧萍,张健,吴贤.汽车尾气净化用贵金属催化剂研究进展[J].稀有金属材料与工程,2006,35(A02):442-447. 被引量:24
4Sara Erkfeldt,Martin Petersson,Anders Palmqvist.Alumina-supported In 2 O 3 , Ga 2 O 3 and B 2 O 3 catalysts for lean NO x reduction with dimethyl ether[J]. Applied Catalysis B, Environmental . 2012
5Dong Yang,Junhua Li,Mingfen Wen,Chongli Song.Selective catalytic reduction of NO x with methane over indium supported on tungstated zirconia[J]. Catalysis Communications . 2007 (12)
6T. Kobayashi,T. Yamada,K. Kayano.Effect of basic metal additives on NO x reduction property of Pd-based three-way catalyst[J]. Applied Catalysis B, Environmental . 2001 (3)
1罗孟飞,袁贤鑫.Ag-Ce/γ-Al_2O_3催化剂上CO的氧化[J].催化学报(英文),1995,16(4):328-331. 被引量:5
2郑华荣,陈永娟,董辉,李朝晖.制备方法对AgInO_2结构及光催化性能的影响[J].无机化学学报,2011,27(3):468-472. 被引量:1
3常青云,贺泓,曲久辉,赵进才.Ag-Ce/AlPO4催化剂在水中催化杀菌的影响因素[J].催化学报(英文),2008,29(3):215-220. 被引量:3
4物理化学[J].中国学术期刊文摘,2008,14(13):71-87.
5许承志,郑美琴,陈铿,胡晖,陈晓晖.CeO_x掺杂TiO_2-SiO_2载体对Ag基柴油脱硫吸附剂性能的影响(英文)[J].燃料化学学报,2016,44(8):943-953. 被引量:1
6岳宝华,周仁贤,郑小明.制备条件对SiO_2改性氧化铝材料耐热性能的影响[J].无机化学学报,2007,23(3):533-536. 被引量:19
7王璐璐,夏长泰,许鹏,狄聚青,赛青林,牟菲.Energy transfer in Ce,Nd,and Yb co-doped YAG phosphors[J].中国光学快报:英文版,2013(6):58-61.
Basic Information:
DOI:
Chinese Library Classification Number:O643.361[理学—物理化学]
Citation Information:
Three-way catalyst was prepared by isovolumetric impregnation with the scattered metal In,the transition metal Ag and the rare earth metal Ce as the active components andγ-Al2O3 as the carrier.The microstructure of the catalyst was characterized by XRD,BET,SEM and N2 adsorption technology.The influence of In content on catalyst performance was also investigated.The results show that the catalyst activity can be improved after In addition resulting in AgInO2 phase appearing in its XRD pattern.However,the catalyst activity gradually decreases with the increase of In content.The results from BET and SEM show that the increase of In content causes aggregation of the active ingredients to reduce their dispersion degree and decrease of the specific surface area of the catalyst to reduce its catalytic activity.In-Ag-Ce-O/γ-Al2O3 catalyst has the strongest three-way catalytic activity when its active ingredient In content is 2%.
quote
| GB/T 7714-2015 | [1] LIU Jing-min, WU Shuang, XU Zhen-chong, et al. Effect of In Content on Three-way Catalytic Performance of In-Ag-Ce-O/γ-Al_2O_3 Catalyst[J]. Rare Metals and Cemented Carbides, 2015(3): 40-43. |
| MLA | [1] LIU Jing-min, et al., "Effect of In Content on Three-way Catalytic Performance of In-Ag-Ce-O/γ-Al_2O_3 Catalyst." Rare Metals and Cemented Carbides, no. 3, 2015, pp. 40-43. |
| APA | [1] LIU Jing-min, WU Shuang, XU Zhen-chong, & ZANG Shu-liang. (2015). Effect of In Content on Three-way Catalytic Performance of In-Ag-Ce-O/γ-Al_2O_3 Catalyst. Rare Metals and Cemented Carbides(3), 40-43. |
| IEEE | [1] LIU Jing-min, WU Shuang, XU Zhen-chong, and ZANG Shu-liang, "Effect of In Content on Three-way Catalytic Performance of In-Ag-Ce-O/γ-Al_2O_3 Catalyst," Rare Metals and Cemented Carbides, no. 3, pp. 40-43, 2015. keywords: {In-Ag-Ce-O/γ-Al2O3 catalyst;indium content;isovolumetric impregnation;three-way catalyst;automobile exhaust} |