daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Effect of SPS Temperature on the Microstructure and Properties of WCoB-TiC Cermets AITranslate

School of Materials and Metallurgy,Wuhan University of Science and Technology;School of Materials and Metallurgy,Wuhan University of Science and Technology;School of Materials and Metallurgy,Wuhan University of Science and Technology;School of Materials and Metallurgy,Wuhan University of Science and Technology;School of Materials and Metallurgy,Wuhan University of Science and Technology;School of Materials and Metallurgy,Wuhan University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

WCoB-TiC cermets were prepared by the spark plasma sintering process.The effects of SPS temperature on the microstructure and mechanical properties of WCoB-TiC were investigated.The experimental results show that the density and hardness of the cermets firstly increase and then decrease with the increase of sintering temperature.When the sintering temperature is 1300℃,the microstructure compactness of the WCoB-TiC cermet is the best,the density reaches 9.33g/cm3,and the hardness and bending strength are the highest,which are 92HRA and 824MPa,respectively.When the sintering temperature is increased from 1100°C to 1300°C,the fracture mode of the cermets gradually changes from cleavage fracture to quasi-cleavage fracture.When the sintering temperature reaches 1400℃,the grain growth leads to the decline of various mechanical properties of the cermet.

KeyWords AITranslate

spark plasma sintering WCoB-TiC sintering temperaturre microstructure cermet

1Tong Zhang,Haiqing Yin,Cong Zhang,Xuanhui Qu.Microstructure and mechanical properties of Cr doped WCoB based cermets by spark plasma sintering and first principle calculation[J].自然科学进展·国际材料:英文版,2020,30(3):417-423. 被引量:1

2鲁振运,杜劲,胡冬梅,王一飞,孙玉晶,张重彦.硬质合金增韧补强机理研究进展[J].有色金属工程,2020,10(7):40-46. 被引量:4

3宋晓艳,刘雪梅,张久兴.SPS过程中导电粉体的显微组织演变规律及机理[J].中国科学:E辑,2005,35(5):459-469. 被引量:26

4孙帆,郑勇,吴鹏,常有余.三元硼化物基硬质合金烧结过程中的相变和微观组织的演化[J].硬质合金,2010,27(6):332-337. 被引量:4

5王盼,潘应君,徐源源,柯德庆,黄辽.烧结方式对WCoB-TiC复相金属陶瓷微观组织及力学性能的影响[J].武汉科技大学学报,2017,40(5):374-378. 被引量:2

1李晓雪,陈革.不同载荷对20CrMnTi-SnAgCu-Graphene复合材料性能的影响[J].造纸装备及材料,2022,51(2):60-62. 被引量:1

1张洪毅,张博,武明远.拉挤成型碳纤维增强复合材料常温静力性能分析[J].造纸装备及材料,2023,52(5):94-96.

1刘朝猛,吴懿姿.体育器材用TiAl_(3)/AlSi11Cu3铝合金组织和力学性能优化[J].铸造,2022,71(2):176-181. 被引量:3

2张堃,吴姚莎,刘晓飞,王丽荣,曾思惠.TiB_(2)/AlSi10Mg选区激光熔化成形组织与性能[J].有色金属工程,2021,11(12):43-49. 被引量:4

3瞿海霞,唐成龙,顾廷权.热挤压模具用钴基合金微观组织及高温摩擦磨损性能研究[J].宝钢技术,2020(4):38-46.

4王庆娟,樊瑞雪,刘丹,张玉峰,王伟,杜忠泽,刘世锋.放电等离子烧结法制备石墨烯-铜铬锆合金的组织与性能[J].稀有金属材料与工程,2022,51(2):414-421.

5彭翔,刘文才,吴国华.Li含量对铸态Mg-xLi-3Al-2Zn-0.5Y合金微观组织与力学性能的影响[J].中国有色金属学报:英文版,2022,32(3):838-849.

6朱梓坤,韩阳,张舟,张义,周龙早.Q690D低合金高强钢模拟焊接热影响区的组织和性能[J].焊接,2022(1):26-33. 被引量:1

7魏天翔,颜亮.放电等离子烧结温度对Fe-Si/MnZn(Fe_(2)O_(4))_(2)软磁复合材料组织与磁性能的影响[J].机械工程材料,2022,46(1):35-40.

8尚方静,王文先,杨涛,刘瑞峰,周峻.镍包覆氧化铝增强铁基复合材料的界面行为及其耐磨性(英文)[J].稀有金属材料与工程,2022,51(2):422-428.

9李伟健,崔泽琴,马丽莉,李国凯,宫殿清.不同含量HAp对Zn-Mg/HAp复合材料组织与腐蚀行为的影响[J].热加工工艺,2022,51(2):82-86.

10王法,江河,董建新.放电等离子烧结制备对Ni/SiCf界面反应的影响[J].稀有金属材料与工程,2022,51(2):599-606.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.41[金属学及工艺—金属材料]

Citation Information:

WCoB-TiC cermets were prepared by the spark plasma sintering process.The effects of SPS temperature on the microstructure and mechanical properties of WCoB-TiC were investigated.The experimental results show that the density and hardness of the cermets firstly increase and then decrease with the increase of sintering temperature.When the sintering temperature is 1300℃,the microstructure compactness of the WCoB-TiC cermet is the best,the density reaches 9.33g/cm3,and the hardness and bending strength are the highest,which are 92HRA and 824MPa,respectively.When the sintering temperature is increased from 1100°C to 1300°C,the fracture mode of the cermets gradually changes from cleavage fracture to quasi-cleavage fracture.When the sintering temperature reaches 1400℃,the grain growth leads to the decline of various mechanical properties of the cermet.

quote

GB/T 7714-2015 [1] ZHU Xing-yu, PAN Ying-jun, ZHANG Heng, et al. Effect of SPS Temperature on the Microstructure and Properties of WCoB-TiC Cermets[J]. Rare Metals and Cemented Carbides, 2022(1): 27-31.
MLA [1] ZHU Xing-yu, et al., "Effect of SPS Temperature on the Microstructure and Properties of WCoB-TiC Cermets." Rare Metals and Cemented Carbides, no. 1, 2022, pp. 27-31.
APA [1] ZHU Xing-yu, PAN Ying-jun, ZHANG Heng, KE De-qing, ZHENG Shi-en, & YANG Ling. (2022). Effect of SPS Temperature on the Microstructure and Properties of WCoB-TiC Cermets. Rare Metals and Cemented Carbides(1), 27-31.
IEEE [1] ZHU Xing-yu, PAN Ying-jun, ZHANG Heng, KE De-qing, ZHENG Shi-en, and YANG Ling, "Effect of SPS Temperature on the Microstructure and Properties of WCoB-TiC Cermets," Rare Metals and Cemented Carbides, no. 1, pp. 27-31, 2022. keywords: {spark plasma sintering;WCoB-TiC;sintering temperaturre;microstructure;cermet}