Effect of WC Addition Amount on Microstructure and Properties of Ni-based Plasma Cladding Layer AITranslate
Abstract AITranslate
In order to improve the mechanical properties of Ni-based plasma cladding layer, single crystal WC powder was added into the Ni-based powder.The influence of adding different amounts of WC on the microstructure and mechanical properties of Ni-based plasma cladding layer was studied by SEM analysis, hardness test, wear resistance test and other methods.The results show that when 0~30% WC is added into Ni60 alloy powder, with WC addition amount increasing, the macroscopic morphology of Ni-based plasma cladding layer gradually deteriorates, and undecomposed WC particles gather more and more at the fusion line, while the surface hardness of the cladding layer shows an increasing trend, and the wear resistance is gradually improved.In actual production, it is necessary to comprehensively consider the macro-morpho-logy and property requirements of Ni-based cladding layer before reasonably determining WC addition amount.
KeyWords AITranslate
1方爽,于秋颖,东赟鹏,王淑云.镍基粉末高温合金粉末直接锻造技术[J].热加工工艺,2021,50(11):18-24. 被引量:2
2谢凡,时凯华,顾金宝.传统方法制备超细WC粉末的质量控制研究进展[J].稀有金属与硬质合金,2021,49(3):31-36. 被引量:2
3平学龙,符寒光,孙淑婷.激光熔覆制备硬质颗粒增强镍基合金复合涂层的研究进展[J].材料导报,2019,33(9):1535-1540. 被引量:30
4孟莹,朱小鹏,杜鹏程,雷明凯.超音速火焰喷涂Ni60-40WC涂层高频感应重熔处理及其水润滑摩擦磨损性能[J].材料保护,2018,51(12):82-89. 被引量:12
5张锋刚.脉冲频率对IPEB辐照WC-13Ni硬质合金显微组织与硬度的影响[J].稀有金属与硬质合金,2019,47(5):74-78. 被引量:1
6李云峰,石岩.WC对激光熔覆层组织及耐磨耐冲击性的影响[J].中国表面工程,2021,34(2):104-113. 被引量:7
7时运,杜晓东,庄鹏程,王长剑,高万东.等离子熔覆技术的研究现状及展望[J].表面技术,2019,48(12):23-33. 被引量:23
8杨效田,李秀倩,李霞,杨强斌,周俊,李文生.WC含量对定向结构Ni60涂层耐蚀性能的影响[J].稀有金属材料与工程,2020,49(10):3604-3611. 被引量:3
1崔陈,朱协彬,程敬卿,刘振华,韩顺顺.等离子熔覆Fe基/WC-10Co-4Cr涂层的组织与性能研究[J].表面技术,2023,52(7):167-176. 被引量:1
1罗汝恺,卢威,魏仕勇,万珍珍,金莹.等离子转移弧电流对Ni60涂层质量的影响[J].热处理技术与装备,2023,44(3):12-14.
1黄海博,孙文磊.Ni60激光熔覆工艺参量对涂层裂纹及厚度的影响[J].激光技术,2021,45(6):788-793. 被引量:6
2庞德禹,张尚毅,周晓宏.等离子熔覆金属基/陶瓷复合涂层性能分析[J].兰州工业学院学报,2022,29(1):65-67. 被引量:1
3嵇友迪,龚红英,徐培全.45钢激光熔覆Ni60合金粉末工艺参数的多目标优化[J].上海工程技术大学学报,2021,35(4):315-320.
4江柯燃.探究建筑混凝土原材料的检测及管理[J].建材发展导向,2022,20(7):7-9.
5林欣源,尤庆健,李寒菲,张国良.聚乙烯醇对磷酸钾镁水泥砂浆粘结性能的影响[J].福建建设科技,2022(1):51-53.
6缪喆宇,高义民,王怡然,施庆峰,亓云飞.激光熔覆工艺参数对铜/钢双金属复合材料组织的影响[J].铸造,2022,71(2):151-157. 被引量:2
7朱海,袭著鑫,张剑,于明玉,孙朝伟.工艺参数对侧向搅拌摩擦增材成型的影响[J].塑性工程学报,2022,29(2):143-149.
8周金锁,季英萍,纪宏波.铝合金压铸拨叉组织和力学性能研究[J].宁波工程学院学报,2022,34(1):1-6.
9秦亚,席静静.轧制及热处理工艺对Q345E组织及力学性能的影响[J].科技创新与应用,2022,12(7):104-106.
10张泽群,陈质彬,董其娟,邬聪,李宗欣,王禾祖,吴飞,张博威,吴俊升.低合金钢、不锈钢和铝镁合金在模拟深海环境中的电偶腐蚀行为研究[J].中国腐蚀与防护学报,2022,42(3):417-424. 被引量:4
Basic Information:
DOI:
Chinese Library Classification Number:TG178[金属学及工艺—金属表面处理]
Citation Information:
In order to improve the mechanical properties of Ni-based plasma cladding layer, single crystal WC powder was added into the Ni-based powder.The influence of adding different amounts of WC on the microstructure and mechanical properties of Ni-based plasma cladding layer was studied by SEM analysis, hardness test, wear resistance test and other methods.The results show that when 0~30% WC is added into Ni60 alloy powder, with WC addition amount increasing, the macroscopic morphology of Ni-based plasma cladding layer gradually deteriorates, and undecomposed WC particles gather more and more at the fusion line, while the surface hardness of the cladding layer shows an increasing trend, and the wear resistance is gradually improved.In actual production, it is necessary to comprehensively consider the macro-morpho-logy and property requirements of Ni-based cladding layer before reasonably determining WC addition amount.
quote
| GB/T 7714-2015 | [1] DING Zi-yang, BAI Ling, JIN Yu-xia, et al. Effect of WC Addition Amount on Microstructure and Properties of Ni-based Plasma Cladding Layer[J]. Rare Metals and Cemented Carbides, 2022(1): 32-36. |
| MLA | [1] DING Zi-yang, et al., "Effect of WC Addition Amount on Microstructure and Properties of Ni-based Plasma Cladding Layer." Rare Metals and Cemented Carbides, no. 1, 2022, pp. 32-36. |
| APA | [1] DING Zi-yang, BAI Ling, JIN Yu-xia, & MA Zong-bin. (2022). Effect of WC Addition Amount on Microstructure and Properties of Ni-based Plasma Cladding Layer. Rare Metals and Cemented Carbides(1), 32-36. |
| IEEE | [1] DING Zi-yang, BAI Ling, JIN Yu-xia, and MA Zong-bin, "Effect of WC Addition Amount on Microstructure and Properties of Ni-based Plasma Cladding Layer," Rare Metals and Cemented Carbides, no. 1, pp. 32-36, 2022. keywords: {Ni-based plasma cladding layer;WC addition amount;microstructure;mechanical property} |