daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Functional Hierarchical Pores in Polymer Monoliths: Macromolecular Synthesis and Selective Removal of Dyes AITranslate

Seoul National University; Chonnam National University; Chonnam National University; Seoul National University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We describe the design of functional hierarchical pores in polymer monoliths on the basis of inverse, water-in-oil (w/o), high internal phase emulsions. The emulsion structure was formed and stabilized using functional microporous organic polymers as a Pickering agent, which not only provides an emulsion template to form the multiscale pores but also imparts photocatalytic activity to the polymer monoliths. Thus, inverse Pickering emulsions were obtained from styrene–water (2:8, v/v) with internal water droplets; then, a subsequent polymerization reaction created polymer monoliths in various shapes, which caused large interconnected pores as well as functional micropores primarily positioned at the interface. The monoliths absorbed a large amount of various solvents due to their amphiphilicity in the interior pore walls, and the combination of anionic moieties and π-conjugation in the micropores allowed selective, rapid photocatalytic degradation toward positively charged organic dyes. The design concept presented here would be used toward the elimination of prevalent aromatic pollutants in aqueous environments and other purification/filtration systems.

KeyWords AITranslate

microporous polymers inverse high internal phase emulsion Pickering agents hierarchical pores photocatalytic degradation
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01241

Chinese Library Classification Number:

Citation Information:

We describe the design of functional hierarchical pores in polymer monoliths on the basis of inverse, water-in-oil (w/o), high internal phase emulsions. The emulsion structure was formed and stabilized using functional microporous organic polymers as a Pickering agent, which not only provides an emulsion template to form the multiscale pores but also imparts photocatalytic activity to the polymer monoliths. Thus, inverse Pickering emulsions were obtained from styrene–water (2:8, v/v) with internal water droplets; then, a subsequent polymerization reaction created polymer monoliths in various shapes, which caused large interconnected pores as well as functional micropores primarily positioned at the interface. The monoliths absorbed a large amount of various solvents due to their amphiphilicity in the interior pore walls, and the combination of anionic moieties and π-conjugation in the micropores allowed selective, rapid photocatalytic degradation toward positively charged organic dyes. The design concept presented here would be used toward the elimination of prevalent aromatic pollutants in aqueous environments and other purification/filtration systems.

quote

GB/T 7714-2015 [1] Doyeon Kim, Hea Ji Kim, Hyungwoo Kim, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01241.
MLA [1] Doyeon Kim, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01241.
APA [1] Doyeon Kim, Hea Ji Kim, Hyungwoo Kim, & Ji Young Chang. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01241
IEEE [1] Doyeon Kim, Hea Ji Kim, Hyungwoo Kim, and Ji Young Chang, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01241. keywords: {microporous polymers;inverse high internal phase emulsion;Pickering agents;hierarchical pores;photocatalytic degradation}