Simple and Scalable Protocol for Producing Hydrophobic Polymer Brushes Beyond Wafer-Scale Dimensions toward Real-Life Applications AITranslate

National Institute of Advanced Industrial Science and Technology (AIST); University of Sheffield;National Institute of Advanced Industrial Science and Technology (AIST)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Wafer-scale fabrication of polymer brushes has recently attracted considerable attention because of their applicability in a wide variety of real-life applications. In this study, we have demonstrated a simple, facile, and scalable approach of grafting a wide variety of hydrophobic polymer brushes onto organic/inorganic substrates via surface-initiated atom transfer radical polymerization under air (named water-accelerated “paint-on” SI-ATRP). A mixture of ethanol and water was used as a solvent to demonstrate the water-accelerated SI-ATRP of 12 water-insoluble vinyl monomers having hydrophobic functional (alkyl, aromatic, and perfluoroalkyl) groups. Thanks to the addition of a small amount of water, uniform hydrophobic polymer brushes with sufficient thicknesses (more than 20 nm) could be easily grafted from organic/inorganic substrates covered with surface initiator layers (SILs) in a short reaction time of 5–30 min without any severe experimental conditions. The degree of hydrophobicity of the resulting polymer brush surfaces could be arbitrarily tuned from a relatively hydrophobic (water contact angle (CA): 79°) to a highly hydrophobic (water CA: 119°) state by selecting monomers. In addition, using an optimized water-accelerated paint-on SI-ATRP, we have successfully prepared perfluorinated polymer brushes having excellent liquid repellency, antismudge/self-cleaning, and anti-icing properties on glass slides above wafer-scale dimensions (e.g., about 21 cm × 30 cm, nearly letter size).

KeyWords AITranslate

polymer brush surfaceinitiated atom transfer radical polymerization (SIATRP) hydrophobicity Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01244

Chinese Library Classification Number:

Citation Information:

Wafer-scale fabrication of polymer brushes has recently attracted considerable attention because of their applicability in a wide variety of real-life applications. In this study, we have demonstrated a simple, facile, and scalable approach of grafting a wide variety of hydrophobic polymer brushes onto organic/inorganic substrates via surface-initiated atom transfer radical polymerization under air (named water-accelerated “paint-on” SI-ATRP). A mixture of ethanol and water was used as a solvent to demonstrate the water-accelerated SI-ATRP of 12 water-insoluble vinyl monomers having hydrophobic functional (alkyl, aromatic, and perfluoroalkyl) groups. Thanks to the addition of a small amount of water, uniform hydrophobic polymer brushes with sufficient thicknesses (more than 20 nm) could be easily grafted from organic/inorganic substrates covered with surface initiator layers (SILs) in a short reaction time of 5–30 min without any severe experimental conditions. The degree of hydrophobicity of the resulting polymer brush surfaces could be arbitrarily tuned from a relatively hydrophobic (water contact angle (CA): 79°) to a highly hydrophobic (water CA: 119°) state by selecting monomers. In addition, using an optimized water-accelerated paint-on SI-ATRP, we have successfully prepared perfluorinated polymer brushes having excellent liquid repellency, antismudge/self-cleaning, and anti-icing properties on glass slides above wafer-scale dimensions (e.g., about 21 cm × 30 cm, nearly letter size).

quote

GB/T 7714-2015 [1] Tomoya Sato, Gary J. Dunderdale, Atsushi Hozumi. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01244.
MLA [1] Tomoya Sato, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01244.
APA [1] Tomoya Sato, Gary J. Dunderdale, & Atsushi Hozumi. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01244
IEEE [1] Tomoya Sato, Gary J. Dunderdale, and Atsushi Hozumi, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01244. keywords: {polymer brush;surfaceinitiated atom transfer radical polymerization (SIATRP);hydrophobicity;Show More}