daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Adhesion and Stiffness Matching in Epoxy-Vitrimers/Strain Sensor Fiber Laminates AITranslate

PSL University; PSL University; PSL University;Department of Functional Materials, Empa - Swiss Federal Laboratories for Materials Science and Technology;Department of Functional Materials, Empa - Swiss Federal Laboratories for Materials Science and Technology; PSL University; PSL University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hybrid networks, including physical and chemical cross-links, were synthesized from biosourced fatty acid fragments, linked to each other by a controlled number of nonexchangeable ether bonds, exchangeable ester bonds, and noncovalent hydrogen bonds. The mechanical properties of these networks are tuned by the ratio of di- versus tetraepoxide and the stoichiometry acid/epoxy. Creep tests and insolubility demonstrated the vitrimer or vitrimer-like nature of the resulting materials. The thermostimulated welding ability of the materials was exploited to incorporate strain sensors by embedding electrically conductive fibers into the rubbery vitrimer matrix. Both the efficiency of the welding procedure at moderate temperatures (80 °C) and the tunability of mechanical properties are attractive assets for the effective incorporation of thermodegradable conductive fibers while preserving their mechanical and electrical integrity. The mechanical and electrical behaviors of the sensor composites were simultaneously tested, either in quasi-static or in cyclic tensile experiments, at room temperature and at a larger distance from Tg of the matrices. The study emphasizes the importance of matching Young’s moduli of components in composite samples, which is strongly temperature-dependent.

KeyWords AITranslate

soft robotics elastomeric vitrimer electrically conductive composites matrix−sensor fiber laminates stiffness matching
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01648

Chinese Library Classification Number:

Citation Information:

Hybrid networks, including physical and chemical cross-links, were synthesized from biosourced fatty acid fragments, linked to each other by a controlled number of nonexchangeable ether bonds, exchangeable ester bonds, and noncovalent hydrogen bonds. The mechanical properties of these networks are tuned by the ratio of di- versus tetraepoxide and the stoichiometry acid/epoxy. Creep tests and insolubility demonstrated the vitrimer or vitrimer-like nature of the resulting materials. The thermostimulated welding ability of the materials was exploited to incorporate strain sensors by embedding electrically conductive fibers into the rubbery vitrimer matrix. Both the efficiency of the welding procedure at moderate temperatures (80 °C) and the tunability of mechanical properties are attractive assets for the effective incorporation of thermodegradable conductive fibers while preserving their mechanical and electrical integrity. The mechanical and electrical behaviors of the sensor composites were simultaneously tested, either in quasi-static or in cyclic tensile experiments, at room temperature and at a larger distance from Tg of the matrices. The study emphasizes the importance of matching Young’s moduli of components in composite samples, which is strongly temperature-dependent.

quote

GB/T 7714-2015 [1] Jakob Langenbach, Camille BakkaliHassani, QuentinArthur Poutrel, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01648.
MLA [1] Jakob Langenbach, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01648.
APA [1] Jakob Langenbach, Camille BakkaliHassani, QuentinArthur Poutrel, Antonia Georgopoulou, Frank Clemens, François Tournilhac, & Sophie Norvez. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01648
IEEE [1] Jakob Langenbach, Camille BakkaliHassani, QuentinArthur Poutrel, Antonia Georgopoulou, Frank Clemens, François Tournilhac, and Sophie Norvez, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01648. keywords: {soft robotics;elastomeric vitrimer;electrically conductive composites;matrix−sensor fiber laminates;stiffness matching}