Long Two-Dimensional Folding Chain Structure Formation of Poly(vinylidene fluoride) in Solutions of a Polar Solvent, N-Methylpyrrolidone AITranslate

Tokyo University of Agriculture and Technology; Tokyo University of Agriculture and Technology; Tokyo University of Agriculture and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The conformation and structure of poly(vinylidene fluoride) (PVDF; (̵CH2CF2)̵n) samples with wide-range weight average molar masses (Mw) ranging from 100 to 3300 kg mol–1 dissolved in a highly polar solvent, N-methylpyrrolidone (NMP), were fully reconsidered based on the newly obtained results using small- to wide-angle X-ray scattering (S-WAXS), static light scattering (SLS), and viscometric techniques. The dependencies of scattering intensities on the scattering vector (q) observed in the S-WAXS experiments showed the characteristic local structure of long columnar particles with rather an extended rectangular or long two-dimensional folding chain structure in the solution. The q dependencies of the concentration reduced excess Rayleigh ratios for each PVDF sample determined in the SLS experiments provided the Mw dependence of the radius of gyration (Rg) approximately described in the manner Rg ∝ Mw∼0.6 in the solution and were similar to those of flexible polymer chains dissolved in good solvents as reported previously. Using a rectangular columnar (parallelepiped) particle model, the global structure of PVDF molecules in the solution was analyzed, and the particle length (L) of each PVDF sample was carefully determined. The determined L value was not proportional to Mw or the weight average contour length (l) but demonstrated the relationship L ∝ Mw∼0.6. Then, the relationship was finally obtained over the entire examined Mw range, which implies that PVDF molecules behave as long rigid rectangular columnar particles in the solution. Consequently, the obtained SLS data revealed that the folding number, lL–1, gradually increases from 5 to 24 with increasing Mw value. The Mw dependence of intrinsic viscosity ([η]) also clearly demonstrated the rigid rectangular columnar particle behavior for all of the PVDF samples in the NMP solution. The obtained results in this study would be extremely important to improve the performance of commercial lithium ion batteries.

KeyWords AITranslate

poly(vinylidene fluoride) Nmethylpyrrolidone static light scattering Rayleigh ratio small to wideangle Xray scattering rigid rod Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01630

Chinese Library Classification Number:

Citation Information:

The conformation and structure of poly(vinylidene fluoride) (PVDF; (̵CH2CF2)̵n) samples with wide-range weight average molar masses (Mw) ranging from 100 to 3300 kg mol–1 dissolved in a highly polar solvent, N-methylpyrrolidone (NMP), were fully reconsidered based on the newly obtained results using small- to wide-angle X-ray scattering (S-WAXS), static light scattering (SLS), and viscometric techniques. The dependencies of scattering intensities on the scattering vector (q) observed in the S-WAXS experiments showed the characteristic local structure of long columnar particles with rather an extended rectangular or long two-dimensional folding chain structure in the solution. The q dependencies of the concentration reduced excess Rayleigh ratios for each PVDF sample determined in the SLS experiments provided the Mw dependence of the radius of gyration (Rg) approximately described in the manner Rg ∝ Mw∼0.6 in the solution and were similar to those of flexible polymer chains dissolved in good solvents as reported previously. Using a rectangular columnar (parallelepiped) particle model, the global structure of PVDF molecules in the solution was analyzed, and the particle length (L) of each PVDF sample was carefully determined. The determined L value was not proportional to Mw or the weight average contour length (l) but demonstrated the relationship L ∝ Mw∼0.6. Then, the relationship was finally obtained over the entire examined Mw range, which implies that PVDF molecules behave as long rigid rectangular columnar particles in the solution. Consequently, the obtained SLS data revealed that the folding number, lL–1, gradually increases from 5 to 24 with increasing Mw value. The Mw dependence of intrinsic viscosity ([η]) also clearly demonstrated the rigid rectangular columnar particle behavior for all of the PVDF samples in the NMP solution. The obtained results in this study would be extremely important to improve the performance of commercial lithium ion batteries.

quote

GB/T 7714-2015 [1] Yuki Nohara, Erika Saiki, Toshiyuki Shikata. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01630.
MLA [1] Yuki Nohara, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01630.
APA [1] Yuki Nohara, Erika Saiki, & Toshiyuki Shikata. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01630
IEEE [1] Yuki Nohara, Erika Saiki, and Toshiyuki Shikata, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01630. keywords: {poly(vinylidene fluoride);Nmethylpyrrolidone;static light scattering;Rayleigh ratio;small to wideangle Xray scattering;rigid rod;Show More}