Abstract AITranslate

ion:The extraction of rare earths by A101 in HCl solution within magnetic field was studied.The principle of extraction was discussed and the effect of magnetic field on extractability was analyzed.The data illustrated the extractability was slightly increased in the magnetic field,which could be explained by the same extraction principle.It is the change of physical properties of system that makes the extractability increase.The magnetic field does not have periodical relationship with the distribution ratio and magnetic length of rare earths.

KeyWords AITranslate

solvent extraction A101 rare earths

1陈洲溪.磁场对有机溶剂萃取稀土元素的影响[J].湖南冶金,1984,(2):1-1.

1段秀丽,朱洋,马学景,孙继兵,步绍静,杨薇.铁磁材料在化工分离过程中的应用[J].材料导报:纳米与新材料专辑,2016,30(2):84-86.

2杜朝军,杨幼明.物理场强化萃取技术及应用[J].江西有色金属,2003,17(3):34-36. 被引量:6

1孙庆磊,梁月荣,陆建良.超声波在茶叶提取中的应用[J].茶叶,2006,32(2):79-82. 被引量:32

2卢友中.萃取新技术在有色冶金中的应用[J].上海有色金属,2007,28(3):137-140. 被引量:6

3纪存兴,石磊,李金英,赵志军,侯艳丽,唐占梅,李中平,凡金龙,张东翔.静电场激励液-液体系相间铜反萃传质特性[J].原子能科学技术,2010,44(8):953-957.

4林忠宁,何友建,陆烝,刘明香,陈敏健.响应面分析法优选灵芝超声波提取工艺的研究[J].中国食品学报,2012,12(7):97-104. 被引量:12

5段秀丽,朱洋,马学景,孙继兵,步绍静,杨薇.铁磁材料在化工分离过程中的应用[J].材料导报:纳米与新材料专辑,2016,30(2):84-86.

6马露,张鹏,唐杰,张运菊,肖棱,袁小超.工业含Cr^(6+)废水处理技术研究进展[J].绵阳师范学院学报,2022,41(11):39-48.

1郑晓玲,倪兆艾.N_(503)萃取稀土元素的研究[J].稀土,1990,11(5):18-22. 被引量:1

2马荣骏,马伟.在磁场作用下用乙酰胺萃取五价砷[J].湿法冶金,1998(2):42-44. 被引量:4

3罗电宏,马荣骏.用溶剂萃取技术从含微量金的废液中回收金[J].有色金属,2003,55(1):34-36. 被引量:5

4陆雍华,陆忠娥,童剑英,顾正康.N,N-二仲辛基乙酰胺萃取原子吸收光谱法测定矿石中金[J].冶金分析,1989,9(2):39-41. 被引量:4

5王靖芳,冯彦琳,李慧妍.N,N-二(1-甲庚基)乙酰胺萃取铼的研究[J].稀有金属,1995,19(3):228-230. 被引量:8

6周扬,李学玲,顾烁玥,杨项军.用N503/TBP从碱性氰化液中萃取低浓度金[J].中国有色金属学报,2009,19(7):1345-1349. 被引量:8

7封文江,方戈亮,王传银,徐琦,张礼庆.纳米晶(Fe,Cr)-N的制备与磁性[J].沈阳师范大学学报:自然科学版,2008,26(1):61-64. 被引量:4

8贾琼,吴杰,李婷婷,周伟红.磷酸三丁酯与三烷基胺类萃取剂对锌离子的协同萃取[J].分析化学,2008,36(5):619-622. 被引量:11

9赵兵,卢立柱,林平,江莉.溶剂在浆萃取Au(Ⅲ)过程中阳离子对溶剂污物形成的影响[J].稀有金属与硬质合金,1993,21(S1):278-281.

10林建军,钟依均,陈建荣,许峰,胡建华.N503萃淋树脂吸附镓的研究[J].中国有色金属学报,1996,6(1):40-43. 被引量:6

Basic Information:

DOI:

Chinese Library Classification Number:TF845[冶金工程—有色金属冶金]

Citation Information:

ion:The extraction of rare earths by A101 in HCl solution within magnetic field was studied.The principle of extraction was discussed and the effect of magnetic field on extractability was analyzed.The data illustrated the extractability was slightly increased in the magnetic field,which could be explained by the same extraction principle.It is the change of physical properties of system that makes the extractability increase.The magnetic field does not have periodical relationship with the distribution ratio and magnetic length of rare earths.

quote

GB/T 7714-2015 [1] LUO Dian-hong, MA Rong-jun. Extraction of Rare Earths by A101 within Magnetic Field[J]. Rare Metals and Cemented Carbides, 2002(3): 14-16.
MLA [1] LUO Dian-hong, and MA Rong-jun. "Extraction of Rare Earths by A101 within Magnetic Field." Rare Metals and Cemented Carbides, no. 3, 2002, pp. 14-16.
APA [1] LUO Dian-hong, & MA Rong-jun. (2002). Extraction of Rare Earths by A101 within Magnetic Field. Rare Metals and Cemented Carbides(3), 14-16.
IEEE [1] LUO Dian-hong and MA Rong-jun, "Extraction of Rare Earths by A101 within Magnetic Field," Rare Metals and Cemented Carbides, no. 3, pp. 14-16, 2002. keywords: {solvent extraction;A101;rare earths}