daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on Physicochemical Properties of APT Prepared by Doping Cr during Ammonium Paratungstate Crystallization AITranslate

School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Cr-doped APT powders were prepared by doping chromium acetate during ammonium paratungstate crystallization,and then their physicochemical properties were studied.The results show that the impurity elements are in line with the standard of APT-0in GB/T 10116—2007(Ammonium Paratungstate)except for chromium element.Chromium exists in APT powders mainly in the form of amorphous chromium hydroxide.As growth of APT crystal is inhibited by amorphous chromium hydroxide precipitated before APT,Cr-doped APT has smaller particle size,lower bulk density and slightly wider particle size distribution than ordinary Cr-free products.Cr-doped APT powders have macroscopically and microscopically uniform composition.

KeyWords AITranslate

ammonium paratungstate(APT) crystallization Cr-doped APT physicochemical property

1万林生,肖学有,赵立夫,陈邦明,杨树生,杨凤丽.一种单晶仲钨酸铵及其制备方法[P]. 中国专利:CN102061524A,

2Carla E. Giacomelli,Marcelo J. Avena,Osvaldo R. Camara,Carlos P. De Pauli.Some Physicochemical Properties of the Chromium(III) Hydrous Oxide-Aqueous Solution Interface[J]. Journal of Colloid And Interface Science . 1995 (1)

1万林生,许立强,黄海,赵立夫,梁勇,杨运光,章秋霖.掺Cr的APT为原料制备的WO_3和W粉的物化性能研究[J].稀有金属与硬质合金,2016,44(4):32-37.

2万林生,曾学品,赖星任,杨亮,刘鹏.仲钨酸铵结晶掺Cr制备的WC粉和超细硬质合金的性能研究[J].稀有金属与硬质合金,2016,44(6):54-59. 被引量:6

3胡小洣,万林生,邱亚明,刘鹏,潘明然,杨亮.钨酸铵溶液中硝酸铬除磷工艺研究[J].稀有金属与硬质合金,2018,46(1):1-4. 被引量:1

1郭圣达,余飞,易健宏,郭建锋,陈颢,王文静,羊建高.粉末原料对SPS法制备WC-6Co硬质合金组织性能的影响[J].稀有金属与硬质合金,2019,47(3):79-85. 被引量:4

2李阳.基于中性网络模型的制盐结晶粒度控制方法[J].盐科学与化工,2019,48(6):51-54.

3刘觐,易志强,谭敦强,陆磊,康林萍,陈志刚.中和-蒸发联合结晶法制备高品质仲钨酸铵的工艺及机理研究[J].江西科学,2019,37(4):590-594. 被引量:3

4黄超,宫晨彪,徐国钻,刘德刚,贺山明,梁勇.离子交后液回收钨废水中MnO除磷的研究[J].中国钨业,2020,35(2):45-50. 被引量:1

5陈亿,谢中华,李继红,徐双,余春荣,张威.连续结晶法制备粗颗粒仲钨酸铵工艺研究[J].中国钨业,2020,35(2):61-66. 被引量:4

6严维,王水龙,郭圣达,郭建锋,黄星,陈颢,李律达,曹赛鹏.Mo添加对WC-6Co硬质合金组织性能的影响[J].稀有金属与硬质合金,2020,48(4):73-78. 被引量:3

7徐利华,程华金,刘庆生.响应曲面法优化钨酸铵蒸发结晶工艺[J].稀有金属与硬质合金,2022,50(2):8-14. 被引量:1

1郅晓科,叶学海,赵桢,何爱珍,王旭阳,章甦,时洁.Cr掺杂对Li_(1.2)Ni_(0.2)Mn_(0.6)O_2结构和电化学性能的影响[J].广州化工,2013,41(6):75-77.

2郭睿倩,李民军.仲钨酸铵的粒度控制[J].稀有金属与硬质合金,1999,27(4):46-49. 被引量:5

3乙烯氯衍生产品在高聚物中的应用[J].合成材料老化与应用,2012,41(1):55-56.

4亓淑艳,丁嘉宝,司梦瑶,任美婷.Cr掺杂对尖晶石型CoFe_(2-x)Cr_xO_4的结构及光催化性能的影响[J].材料导报,2012,26(14):33-35. 被引量:1

5鲍仁强,徐时清,赵士龙,王玮,章珏,郑飞.Cr掺杂微晶玻璃光谱特性[J].武汉理工大学学报,2007,29(E01):1-4.

6SHANG Yongbin,XIAO Shuqin,QIU Xiaolin,WEI Yarning.Influence of Cr on the Electronic Properties of Passive Film on B30 Alloy in NaOH Solution[J].高等学校化学研究:英文版,2015,0(4):603-610.

7LinlinZhu,Jong Pyo Kim,Sou Hwan Son,Jung Hoon Park.Structural,Sintering and Electrical Properties of Cr-doped La_(0.6)Sr_(0.4)Cr_xFe_(1-x)O_(3-δ)(x=0.10,0.20) Oxides[J].材料科学技术:英文版,2012,28(7):654-660.

8鲁辉,张岩.Cr掺杂Ba_(0.5)Sr_(0.5)Co_(0.8)Fe_(0.1)Cr_(0.1)O_(3-δ)钙钛矿型膜的透氧性能研究[J].材料导报,2011,25(2):43-46. 被引量:1

9Xiang XlA,Xiangping JIANG,Chao CHEN,Xingan JIANG,Na TU,Yunjing CHEN.Effects of Cr2O3 doping on the microstructure and electrical properties of (Ba,Ca)(Zr,Ti)O3 lead-free ceramics[J].材料学前沿:英文版,2016,0(2):203-210. 被引量:3

10张晓光.工业硅中杂质元素含量的测定[J].中国科技博览,2014(32):22-22.

Basic Information:

DOI:

Chinese Library Classification Number:TQ113.79[化学工程—无机化工]

Citation Information:

Cr-doped APT powders were prepared by doping chromium acetate during ammonium paratungstate crystallization,and then their physicochemical properties were studied.The results show that the impurity elements are in line with the standard of APT-0in GB/T 10116—2007(Ammonium Paratungstate)except for chromium element.Chromium exists in APT powders mainly in the form of amorphous chromium hydroxide.As growth of APT crystal is inhibited by amorphous chromium hydroxide precipitated before APT,Cr-doped APT has smaller particle size,lower bulk density and slightly wider particle size distribution than ordinary Cr-free products.Cr-doped APT powders have macroscopically and microscopically uniform composition.

quote

GB/T 7714-2015 [1] WAN Lin-sheng, LAI Xing-ren, HUANG Hai, et al. Study on Physicochemical Properties of APT Prepared by Doping Cr during Ammonium Paratungstate Crystallization[J]. Rare Metals and Cemented Carbides, 2015(5): 1-3 15.
MLA [1] WAN Lin-sheng, et al., "Study on Physicochemical Properties of APT Prepared by Doping Cr during Ammonium Paratungstate Crystallization." Rare Metals and Cemented Carbides, no. 5, 2015, pp. 1-3 15.
APA [1] WAN Lin-sheng, LAI Xing-ren, HUANG Hai, ZHAO Li-fu, & ZHANG Qiu-lin. (2015). Study on Physicochemical Properties of APT Prepared by Doping Cr during Ammonium Paratungstate Crystallization. Rare Metals and Cemented Carbides(5), 1-3 15.
IEEE [1] WAN Lin-sheng, LAI Xing-ren, HUANG Hai, ZHAO Li-fu, and ZHANG Qiu-lin, "Study on Physicochemical Properties of APT Prepared by Doping Cr during Ammonium Paratungstate Crystallization," Rare Metals and Cemented Carbides, no. 5, pp. 1-3 15, 2015. keywords: {ammonium paratungstate(APT);crystallization;Cr-doped APT;physicochemical property}