Experimental Study on Extraction and Recovery of Scandium from Tungsten Residue AITranslate
Abstract AITranslate
Scandium was extracted and recovered from the acid leaching solution of tungsten residue with primary amine N1923 as the extractant.The effects were studied of solution acidity,extractant volume fraction,phase ratio and extraction time on scandium extraction as well as the effect of hydrochloric acid concentration on scandium stripping.The results show that the extractant of primary amine N1923 has a good selectivity to scandium.The optimum conditions for extraction are as follows:solution acidity 0.25mol/L,extractant volume fraction 10%,O/A phase ratio 1∶1,and extraction time 5min.The proper stripping agent is 3.5mol/L dilute hydrochloric acid.Under the above optimum conditions,the extraction rate of scandium reaches 96.42%,the stripping rate is 98.28%,and the total recovery rate of scandium extraction is 92.33%.
KeyWords AITranslate
1[日]关根达也,长谷川佑子 著,腾藤 译.溶剂萃取化学[M]. 原子能出版社, 1981
2Weiwei Wang,Yoko Pranolo,Chu Yong Cheng.Metallurgical processes for scandium recovery from various resources: A review[J]. Hydrometallurgy . 2011 (1)
3A. Ditze,K. Kongolo.Recovery of scandium from magnesium, aluminium and iron scrap[J]. Hydrometallurgy . 1997 (1)
4Xu Shaoquan,Li Suqing.Review of the extractive metallurgy of scandium in China (1978–1991)[J]. Hydrometallurgy . 1996 (3)
5Guo Gongyi,Chen Yuli,Li Yu.Solvent Extraction off Scandium from Wolframite Residue[J]. JOM . 1988 (7)
6Sekine T,Hasegawa Y,Solvent Extraction Chemistry.Marcel Dekker. New York . 1977
7Fedorchak M A,Ladd J A,MacInnis M B,et al.Recovery of tungsten,scandium,iron,and manganese from tungsten bearing material. US Pat:4808384 . 1989
8US Department of the Interior,US Geological Survey.Mineral commodity summaries:2010. . 2010
9US Department of the Interior,US Geological Survey.Minerals yearbook——Rare earths. . 2007
1杨俊彦,齐申,刘海,王文科,黄景存,张建东,车小奎,宋波,王力军.钨冶炼渣综合回收利用的研究进展[J].工程科学学报,2018,40(12):1468-1475. 被引量:5
2李青刚,彭桢,张贵清,曹佐英,曾理,关文娟.液相沉淀法制备草酸钪粉末及其形貌控制[J].稀有金属与硬质合金,2019,47(1):11-15. 被引量:1
3董方,高利坤,陈龙,王鹏,马方通.钪的资源及回收提取技术发展现状[J].矿产综合利用,2016,0(4):21-26. 被引量:17
4彭桢,李青刚,李兆洋,张贵清,曹佐英,关文娟.用离子交换法去除含钪溶液中的杂质(英文)[J].中南大学学报:英文版,2018,25(12):2953-2961. 被引量:3
5谢建清.钨渣回收利用技术研究现状[J].中国钨业,2019,34(1):50-57. 被引量:5
6朱心蕊,刘旭恒,陈星宇,李江涛,何利华,赵中伟.钨冶炼渣的综合利用及发展趋势[J].矿产保护与利用,2019,39(3):119-124. 被引量:9
7李俊杰,何德文,周康根,龚丹丹.钨渣综合利用研究现状[J].矿产保护与利用,2019,39(3):125-132. 被引量:8
8范科彪,郑雅杰,王钫,李海波.电解回收铁钨锡合金粉中的铁[J].中国有色金属学报,2019,29(10):2421-2432. 被引量:3
9孙帅,孙宏骞,宋静,曲景奎,齐涛.钪资源现状及溶剂萃取在钪提取过程中的应用研究进展[J].过程工程学报,2020,20(8):877-886. 被引量:7
10马兵,杜布云,严小飞,康国栋.钨渣制备玻璃化产物危险特性与力学性能研究[J].生态与农村环境学报,2021,37(9):1218-1224.
1葛阳阳,孟建卫,张凯熙,郭静粉.含氟助剂两段酸浸提取钒钛磁铁矿尾矿中的钪[J].稀土,2022,43(4):73-80. 被引量:2
2杨玉珠,周强.2016年云南选矿年评[J].云南冶金,2017,46(2):24-40.
3杨大锦.2016年云南冶金年评[J].云南冶金,2017,46(2):58-78.
4肖军辉,王进明,王振.川西含钪稀土矿中钪的赋存状态研究[J].稀土,2018,39(2):40-47. 被引量:8
5刘牡丹,刘勇,刘珍珍.稀有金属伴生铁精矿回收稀土和钪的工艺研究[J].稀有金属与硬质合金,2018,46(4):6-10.
6马升峰,徐惠,许延辉,王荣,刘铃声,王永利,刘存良.白云鄂博选铌尾矿浸出液制备高纯Sc2O3的工艺研究[J].中国稀土学报,2019,37(6):724-729. 被引量:4
7彭团儿,王玉文,郭珍旭,刘广学,刘艳华,刘磊.可用于制备发泡陶瓷的固废综合利用现状及研究进展[J].佛山陶瓷,2020,30(2):1-9. 被引量:15
8余春荣,黄亮,徐双,李跃海,陆晓晖.钨渣脱水过程中加压过滤机的应用实践[J].中国钨业,2019,34(6):43-47.
9孙帅,孙宏骞,宋静,曲景奎,齐涛.钪资源现状及溶剂萃取在钪提取过程中的应用研究进展[J].过程工程学报,2020,20(8):877-886. 被引量:7
10李桂春,孟齐,康华,闫晓慧.碘化浸出液电沉积金工艺[J].中国有色金属学报,2020,30(8):1925-1933. 被引量:3
1薛生晖,陈洲溪.伯胺N1923从钨酸钠溶液中萃取磷和砷的机理研究[J].矿冶工程,1990,10(2):40-44.
2李永绣,倪兆艾.伯胺N1923对氯化稀土的萃取机理[J].稀有金属,1992,16(5):324-328. 被引量:2
3张安运,杨子超,王秀山,阎居梅.HPMBP与N_(1923)协萃钯(Ⅱ)的性能和动力学研究[J].化工冶金,1991,12(4):306-312.
4马雪阳,梁斌,吕莉,刘维燥,李春.从钛白废酸中萃取回收钛[J].钢铁钒钛,2016,37(4):62-68. 被引量:7
5王玮.氧化铜矿硫酸搅拌浸出工艺研究[J].中国资源综合利用,2016,34(12):23-25. 被引量:2
6张大力,柯家骏,卢立柱.硫代磷酸/伯胺N_(1923)协同萃取锌和镉的机理[J].过程工程学报,2003,3(4):313-316. 被引量:5
7柴金岭.伯胺N1923和三苯基氧化膦萃取Au(Ⅲ)[J].贵金属,1993,14(4):10-16. 被引量:5
8范元俊.铟萃取工艺条件的探讨[J].株冶科技,2001,29(1):18-20. 被引量:7
9彭真,罗明标,蒋小辉,花榕,廖桢葳.协同萃取法回收地浸采铀工艺树脂中铼[J].稀有金属,2011,35(6):922-927. 被引量:7
10钟学明.从钨渣中提取氧化钪的工艺研究[J].江西冶金,2002,22(3):19-22. 被引量:24
Basic Information:
DOI:
Chinese Library Classification Number:TF845.1[冶金工程—有色金属冶金]
Citation Information:
Scandium was extracted and recovered from the acid leaching solution of tungsten residue with primary amine N1923 as the extractant.The effects were studied of solution acidity,extractant volume fraction,phase ratio and extraction time on scandium extraction as well as the effect of hydrochloric acid concentration on scandium stripping.The results show that the extractant of primary amine N1923 has a good selectivity to scandium.The optimum conditions for extraction are as follows:solution acidity 0.25mol/L,extractant volume fraction 10%,O/A phase ratio 1∶1,and extraction time 5min.The proper stripping agent is 3.5mol/L dilute hydrochloric acid.Under the above optimum conditions,the extraction rate of scandium reaches 96.42%,the stripping rate is 98.28%,and the total recovery rate of scandium extraction is 92.33%.
quote
| GB/T 7714-2015 | [1] LIU Cai-yun, FU Jian-gang. Experimental Study on Extraction and Recovery of Scandium from Tungsten Residue[J]. Rare Metals and Cemented Carbides, 2015(5): 4-8 11. |
| MLA | [1] LIU Cai-yun, and FU Jian-gang. "Experimental Study on Extraction and Recovery of Scandium from Tungsten Residue." Rare Metals and Cemented Carbides, no. 5, 2015, pp. 4-8 11. |
| APA | [1] LIU Cai-yun, & FU Jian-gang. (2015). Experimental Study on Extraction and Recovery of Scandium from Tungsten Residue. Rare Metals and Cemented Carbides(5), 4-8 11. |
| IEEE | [1] LIU Cai-yun and FU Jian-gang, "Experimental Study on Extraction and Recovery of Scandium from Tungsten Residue," Rare Metals and Cemented Carbides, no. 5, pp. 4-8 11, 2015. keywords: {tungsten residue;scandium;extraction;primary amine N1923;recovery} |