Dynamic Covalent Bond Network-Based Carbon Nanocomposite for a Self-Healing Tactile Sensor Dynamic Covalent Bond Network-Based Carbon Nanocomposite for a Self-Healing Tactile Sensor AITranslate
Abstract AITranslate
Capacitive tactile sensors using dielectric polymer materials as dielectric layers have been studied due to their high sensitivity and flexibility with a variety of types of materials in response to external stimuli. However, a polymer-based tactile sensor device is limited in long-term use due to a lack of mechanical stability against repeated external stimuli. In this study, a dynamic covalent polymer-based carbon composite material with high sensitivity, structural stability as well as self-healing ability was manufactured and applied as a capacitive tactile sensor dielectric layer. A polymer chain with a disulfide dynamic covalent bond was used as a composite matrix, and carbon nanofibers were applied as fillers to dramatically increase the dielectric constant of the material. The material-based capacitive tactile sensor not only had a high response signal even at a low external stimulus (0.5 kPa) but also had a high sensitivity (46.7 MPa–1) according to the intensity of the stimulus (0.5–17.5 kPa). In addition, the sensor device had a short response of less than 0.2 s and a recovery time of 0.25 s to external stimuli with a stable response signal for 5000 repetitive stimuli. Furthermore, after self-healing deformation of the dielectric layer, the sensor device showed the same level of sensitivity to external stimuli as before deformation by more than 95%.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c00632
Chinese Library Classification Number:
Citation Information:
Capacitive tactile sensors using dielectric polymer materials as dielectric layers have been studied due to their high sensitivity and flexibility with a variety of types of materials in response to external stimuli. However, a polymer-based tactile sensor device is limited in long-term use due to a lack of mechanical stability against repeated external stimuli. In this study, a dynamic covalent polymer-based carbon composite material with high sensitivity, structural stability as well as self-healing ability was manufactured and applied as a capacitive tactile sensor dielectric layer. A polymer chain with a disulfide dynamic covalent bond was used as a composite matrix, and carbon nanofibers were applied as fillers to dramatically increase the dielectric constant of the material. The material-based capacitive tactile sensor not only had a high response signal even at a low external stimulus (0.5 kPa) but also had a high sensitivity (46.7 MPa–1) according to the intensity of the stimulus (0.5–17.5 kPa). In addition, the sensor device had a short response of less than 0.2 s and a recovery time of 0.25 s to external stimuli with a stable response signal for 5000 repetitive stimuli. Furthermore, after self-healing deformation of the dielectric layer, the sensor device showed the same level of sensitivity to external stimuli as before deformation by more than 95%.
quote
| GB/T 7714-2015 | [1] Trong Danh Nguyen, Thi Thu Trinh Phan, Yeon Jeong Nam, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00632. |
| MLA | [1] Trong Danh Nguyen, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00632. |
| APA | [1] Trong Danh Nguyen, Thi Thu Trinh Phan, Yeon Jeong Nam, & Jun Seop Lee. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00632 |
| IEEE | [1] Trong Danh Nguyen, Thi Thu Trinh Phan, Yeon Jeong Nam, and Jun Seop Lee, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00632. keywords: {capacitive tactile sensor polymer composite relative permittivity healable carbon nanofiber} |