The Influence of Forming Sintering Process on the Electrical Properties of Tantalum Capacitors with Solid Electrolyte AITranslate

Hunan Xiangyi Zhongyuan Electronics Co., Ltd.;Hunan Xiangyi Zhongyuan Electronics Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made on the influence of pressing density and sintering temperature on the electrical properties of a typical tantalum capacitor with 16 V/100 μF solid electrolyte using tantalum powder with a specific capacity of 30 000 μF ·V/g as the raw material. The results show that both the porosity and the specific capacity of Ta anode sheets decrease with the increase of pressing density. And the leakage current coefficient decreases down to a minimum of 4.5 × 10^-4 μA/(μF·V) at a pressing density of 5.5 g/cm^3. Furthermore,the increase of sintering temperature has resulted in less specific capacity, lower leakage current coefficient of Ta anode sheets and more product loss.

KeyWords AITranslate

tantalum powder pressing density sintering temperature tantalum electrolytic capacitor electrical property

1夏耀勤,王敬生.钽电容器的应用现状和展望[J].电子元件与材料,1999,18(2):34-36. 被引量:9

2侯宝峰,湛永中,马翠英.100mF·V/g钽粉在片式钽电容器上的应用研究[J].电子工艺技术,2006,27(3):141-144. 被引量:7

3梁雅丽,王英红.高比容钽粉在电容器中的应用[J].电子元件与材料,2006,25(5):46-48. 被引量:6

4Jae Sik Yoon,Byung Il Kim. Characteristics and production of tantalum powders for solid-electrolyte capacitor [J]. Journal of Powder Sources,2007, (164) :959-963.

5伍尊中,姚卫东,袁坤阳.氧含量对钽电解电容器阳极氧化膜形成及漏电流的影响[J].稀有金属与硬质合金,2006,34(2):32-34. 被引量:17

1鄢波,阳元江,肖毅,王安玖,杨槐香,王刚.中压大容量新型高能非固体电解质钽电容器研制[J].材料导报:纳米与新材料专辑,2014,28(1):180-182. 被引量:1

2张学清,郭顺,杨国启,谢群力,左婧懿,罗文.煅烧工艺对钽粉微观结构和电性能的影响[J].稀有金属,2018,42(1):67-74. 被引量:3

3郑鹏,赵春霞,王小明,王晓明.磁选对钽粉性能影响的研究[J].湖南有色金属,2021,37(1):55-57.

4赵春霞,赵勇刚,王小明,王晓明,郑鹏.团化工艺对钽粉性能影响的研究[J].湖南有色金属,2021,37(2):49-52. 被引量:2

5许宁辉,朱利,王娟,牛卫东.成型烧结过程对钽阳极电性能的影响[J].材料开发与应用,2022,37(3):69-74.

6许志林,杜显锋,杨晓丽,梁仲帅,熊礼龙.钽电解电容器用钽阳极制备技术的研究进展[J].电子元件与材料,2023,42(8):907-921.

1刘建清,袁艳丰,徐震宇.一种高压大容量非固体电解质钽电容器的研究[J].电子元件与材料,2020,39(8):96-100. 被引量:2

2李福成.钠还原高比容钽粉湿法提纯过程中酸洗新工艺[J].河南理工大学学报:自然科学版,2022,41(4):176-180. 被引量:1

3张洪刚,李仲香.钽粉细粉对钽阳极块性能的影响分析[J].湖南有色金属,2022,38(6):56-58.

4吴凡,张治国,索艳格.液相还原法制备微米级银粉及其性能研究[J].电镀与精饰,2023,45(3):18-25.

5许志林,杜显锋,杨晓丽,梁仲帅,熊礼龙.钽电解电容器用钽阳极制备技术的研究进展[J].电子元件与材料,2023,42(8):907-921.

1袁艳丰,彭南瑞.非固体电解质钽电容器阴极表面的处理方法[J].河南科技,2014,33(4X):64-64.

2王雅先,尤耀廉,杨俊林.稀土磁性材料压制密度与产品成型性的研究[J].内蒙古石油化工,2009,35(20):11-11.

3刘志亮.无引线片状固体电解质钽电容器的研制[J].电子元件与材料,1995,14(1):24-29.

4聂春杰,张学政,孙凌杰.非固体电解质钽电容器阴极表面处理[J].电子元件与材料,2013,32(6):71-72.

5王兆翔.关于固体电解质钽电容器储存稳定性(上)[J].电子质量,2000,0(3):21-25.

6伍尊中,姚卫东,袁坤阳.氧含量对钽电解电容器阳极氧化膜形成及漏电流的影响[J].稀有金属与硬质合金,2006,34(2):32-34. 被引量:17

7王兆翔.关于固体电解质钽电容器储存稳定性的研究[J].电子元器件应用,2000,2(7):26-30.

8栗丞君.固体电解质钽电容器专用焊料(DHL)的研制[J].有色金属与稀土应用,1996(1):9-13.

9梁雅丽,王英红.高比容钽粉在电容器中的应用[J].电子元件与材料,2006,25(5):46-48. 被引量:6

10王兆翔.关于固体电解质钽电容器储存稳定性(下)[J].电子质量,2000(4):21-23. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TM535.1[电气工程—电器]

Citation Information:

Study is made on the influence of pressing density and sintering temperature on the electrical properties of a typical tantalum capacitor with 16 V/100 μF solid electrolyte using tantalum powder with a specific capacity of 30 000 μF ·V/g as the raw material. The results show that both the porosity and the specific capacity of Ta anode sheets decrease with the increase of pressing density. And the leakage current coefficient decreases down to a minimum of 4.5 × 10^-4 μA/(μF·V) at a pressing density of 5.5 g/cm^3. Furthermore,the increase of sintering temperature has resulted in less specific capacity, lower leakage current coefficient of Ta anode sheets and more product loss.

quote

GB/T 7714-2015 [1] LIU Yong-gang, YI Jin-feng. The Influence of Forming Sintering Process on the Electrical Properties of Tantalum Capacitors with Solid Electrolyte[J]. Rare Metals and Cemented Carbides, 2008(4): 17-19.
MLA [1] LIU Yong-gang, and YI Jin-feng. "The Influence of Forming Sintering Process on the Electrical Properties of Tantalum Capacitors with Solid Electrolyte." Rare Metals and Cemented Carbides, no. 4, 2008, pp. 17-19.
APA [1] LIU Yong-gang, & YI Jin-feng. (2008). The Influence of Forming Sintering Process on the Electrical Properties of Tantalum Capacitors with Solid Electrolyte. Rare Metals and Cemented Carbides(4), 17-19.
IEEE [1] LIU Yong-gang and YI Jin-feng, "The Influence of Forming Sintering Process on the Electrical Properties of Tantalum Capacitors with Solid Electrolyte," Rare Metals and Cemented Carbides, no. 4, pp. 17-19, 2008. keywords: {tantalum powder;pressing density;sintering temperature;tantalum electrolytic capacitor;electrical property}